    • 4. 发明专利
    • Weld fume collecting apparatus
    • 焊接FUME收集设备
    • JP2005288473A
    • 2005-10-20
    • JP2004106448
    • 2004-03-31
    • Jfe Koken CorpJfe工建株式会社
    • YAHAGI ISAMUMURAKAMI TADANOBUINOUE HIROAKITAMAOKI HIROYUKI
    • B23K9/32B23K37/02
    • PROBLEM TO BE SOLVED: To surely collect produced weld fumes regardless of the direction of a welding torch.
      SOLUTION: The weld fume collecting apparatus 10 collects weld fumes caused accompanying welding which is performed while a truck with a welding torch attached runs along a guide rail 3 installed on a workpiece 1. A surface facing the workpiece 1 is opened in the apparatus to mount a collection box 11 surrounding the periphery of the welding torch on the truck. Then, in the collection box 11, there is installed a connecting part 17 which is communicated with the inside of the collection box and is connected to a means for sucking the weld fumes.
      COPYRIGHT: (C)2006,JPO&NCIPI
    • 要解决的问题:无论焊枪的方向如何,都要确保收集产生的焊接烟雾。 解决方案:焊接烟气收集装置10收集随着焊接附带的焊接引起的焊接烟雾,当焊枪附着的卡车沿着安装在工件1上的导轨3运行时。面向工件1的表面在 用于将收集箱11安装在卡车上的焊炬周边周围的装置。 然后,在收集箱11中安装有与收集箱内部连通的连接部17,并与吸附焊接烟雾的装置连接。 版权所有(C)2006,JPO&NCIPI
    • 5. 发明专利
    • Horizontal welding method
    • 水平焊接方法
    • JP2007021571A
    • 2007-02-01
    • JP2005211255
    • 2005-07-21
    • Jfe Koken CorpJfe工建株式会社
    • YAHAGI ISAMUMURAKAMI TADANOBU
    • B23K9/02B23K9/23B23K103/04
    • PROBLEM TO BE SOLVED: To stably form a finish bead of high quality in which ruggedness on the surface is reduced in horizontal welding, and to efficiently perform the welding by reducing a welding operational time.
      SOLUTION: When a finish bead is formed, from the side of an upper plate 2 on the surfaces of beads 5a to 5d stacked at passes (a) to (d), a bead 5e and a bead 5f are successively formed, the sagging lower parts of the preceding beads are remelted, and further, the height of excess metal is reduced by the action of gravity, thus the number of passes upon the formation of the finish bead is reduced. Further, since the excess metal of the finish bead is reduced, and the depth of the trough in the superposed parts of the bead 5e and the bead f is reduced, the finish bead can be made flat, and welding of high quality can be performed. In this way, a repolishing operation for the finish bead can be remarkably reduced.