    • PROBLEM TO BE SOLVED: To provide a laminate having flexibility, high mechanical strength, and high fuel barrier properties which cannot be attained by a conventional laminate structure.
      SOLUTION: In the laminate, a fluororesin layer (A), a fluororesin non-containing resin layer (B) and an elastomer layer (C) are bonded in this order. The invention also relates to the laminate in which the elastomer layer (C), the fluororesin non-containing resin layer (B), the fluororesin layer (A), the fluororesin non-containing resin layer (B), and the elastomer layer (C) are bonded in this order.
      COPYRIGHT: (C)2011,JPO&INPIT
    • 要解决的问题:提供一种具有柔性,高机械强度和高燃料阻挡性能的层压板,其通过常规层压结构不能实现。 解决方案:在层压体中,氟树脂层(A),含氟树脂不含树脂层(B)和弹性体层(C)按此顺序键合。 本发明还涉及弹性体层(C),含氟树脂不含树脂层(B),氟树脂层(A),氟树脂非含树脂层(B)和弹性体层( C)按顺序键合。 版权所有(C)2011,JPO&INPIT
    • 6. 发明专利
    • Wiper blade rubber
    • 刮水器橡胶
    • JP2014028602A
    • 2014-02-13
    • JP2012170567
    • 2012-07-31
    • Daikin Ind Ltdダイキン工業株式会社
    • MASUI TOSHIAKIYANAGIGUCHI TOMIHIKOINABA TSUYOSHI
    • B60S1/38C08K3/22C08K5/3462C08L9/02
    • PROBLEM TO BE SOLVED: To provide wiper blade rubber having excellent low friction property and wiping-out performance.SOLUTION: Wiper blade rubber comprises a lip section wiping a wiping-out surface. The lip section includes a rubber section (A) and a fluororesin layer (B) provided on the rubber section (A). The fluororesin layer (B) is provided on a surface of the lip section and the rubber section (A) is formed of a rubber composition for vulcanization. The fluororesin layer (B) is formed of a fluorine polymer composition and has a thickness of 50 μm or less. The fluorine polymer composition contains a fluorine polymer (b1) having a copolymerization unit derived from chlorotrifluoroethylene. The rubber section (A) is vulcanized and adhered to the fluororesin layer (B).
    • 要解决的问题:提供具有优异的低摩擦性能和擦拭性能的刮水片橡胶。解决方案:刮水片橡胶包括擦拭擦拭表面的唇部。 唇部包括设置在橡胶部分(A)上的橡胶部分(A)和氟树脂层(B)。 氟树脂层(B)设置在唇部的表面上,橡胶部(A)由硫化用橡胶组合物形成。 氟树脂层(B)由氟聚合物组合物形成,厚度为50μm以下。 氟聚合物组合物含有具有来源于三氟氯乙烯的共聚单元的氟聚合物(b1)。 将橡胶部(A)硫化并粘附在氟树脂层(B)上。
    • 8. 发明专利
    • Laminate
    • 层压板
    • JP2012081682A
    • 2012-04-26
    • JP2010231266
    • 2010-10-14
    • Daikin Industries LtdDaiso Co Ltdダイキン工業株式会社ダイソー株式会社
    • MASUI TOSHIAKIINABA TSUYOSHIKUWASHIMA MASAMIHAMAGUCHI KOSHIROKITAGAWA NORIKI
    • B32B25/08B32B1/08B32B27/30B32B27/38C08G59/40F16L11/12
    • PROBLEM TO BE SOLVED: To provide a vulcanizing laminate in which a rubber layer and a fluororesin layer are bonded firmly without using an adhesive and moreover without carrying out surface treatment to each of the rubber layer and the fluororesin layer.SOLUTION: The laminate includes a rubber layer (A) and a fluororesin layer (B) which is laminated on the rubber layer (A). The rubber layer (A) is a layer formed from a rubber composition for vulcanizing. The rubber composition for vulcanizing contains epichlorohydrin rubber (a1), strong base compound (a2) which has an amidine frame in a molecule, and epoxy resin (a3). The fluororesin layer (B) is a layer formed by fluoropolymer composition. The fluoropolymer composition contains fluoropolymer (b1) which has a copolymer unit originating from chlorotrifluoroethylene.
    • 待解决的问题:提供一种硫化层压体,其中橡胶层和氟树脂层牢固地粘合而不使用粘合剂,而且不对橡胶层和氟树脂层进行表面处理。 解决方案:层压体包括层压在橡胶层(A)上的橡胶层(A)和氟树脂层(B)。 橡胶层(A)是由用于硫化的橡胶组合物形成的层。 用于硫化的橡胶组合物包含表氯醇橡胶(a1),在分子中具有脒框架的强碱化合物(a2)和环氧树脂(a3)。 氟树脂层(B)是由氟聚合物组合物形成的层。 氟聚合物组合物含有含有源自三氟氯乙烯的共聚物单元的含氟聚合物(b1)。 版权所有(C)2012,JPO&INPIT
    • 9. 发明专利
    • Laminate
    • 层压板
    • JP2012061644A
    • 2012-03-29
    • JP2010206138
    • 2010-09-14
    • Daikin Industries LtdDaiso Co Ltdダイキン工業株式会社ダイソー株式会社
    • HAMAGUCHI KOSHIROKITAGAWA NORIKIMASUI TOSHIAKIINABA TSUYOSHIKUWASHIMA MASAMITAEDA MAYUKO
    • B32B25/08B32B1/08C08G65/24C08K3/22C08K3/36C08K5/42C08L63/00C08L71/03F16L11/04
    • PROBLEM TO BE SOLVED: To provide a vulcanized laminate with a rubber layer and a fluororesin layer firmly bonded together without treating their surfaces and using an adhesive.SOLUTION: This laminate includes the rubber layer (A) and the fluororesin layer (B) laminated on the former. In addition, the rubber layer (A) is formed of a rubber composition for vulcanization, and contains epichlorohydrin rubber (a1), at least one kind of a chemical compound (a2) selected from a group composed of p-toluenesulfonate of 1,8-diazabicyclo(5.4.0)undecene-7 or 1,5-diazabicyclo(4.3.0)-nonene-5, a phenol salt, phenol resinate, orthophthalate, formate and octylate, a magnesium oxide (a3), silica (a4) and epoxy resin (a5). The fluororesin layer (B) contains a fluoropolymer (b1) with a copolymerization unit derived from chlorotrifluoroethylene.
    • 要解决的问题:提供具有橡胶层和氟树脂层的硫化层压板,其不用处理它们的表面并使用粘合剂牢固地结合在一起。 解决方案:该层压体包括层压在前者上的橡胶层(A)和氟树脂层(B)。 另外,橡胶层(A)由硫化用橡胶组合物形成,并含有表氯醇橡胶(a1),选自由对甲苯磺酸盐组成的组中的至少一种化合物(a2) 苯酚盐,苯酚树脂酸盐,邻苯二甲酸盐,甲酸盐和辛酸盐,氧化镁(a3),二氧化硅(a4),二氧化硅(a4),二氯甲烷 和环氧树脂(a5)。 氟树脂层(B)含有具有来自三氟氯乙烯的共聚单元的含氟聚合物(b1)。 版权所有(C)2012,JPO&INPIT