    • 32. 发明专利
    • Method for designing press forming die, and die for press forming
    • 用于设计压制成型的方法和用于压制成型的模具
    • JP2013128956A
    • 2013-07-04
    • JP2011280464
    • 2011-12-21
    • Jfe Steel CorpJfeスチール株式会社
    • FUJII YUSUKESHINGU TOYOHISAYAMAZAKI YUJIHIGAI KAZUHIKO
    • B21D22/00
    • B21D22/02B21D22/00B21D37/20B21J13/02B30B12/00B30B15/02G01N2203/0067
    • PROBLEM TO BE SOLVED: To design a die in which predominantly bending cracks do not occur by predicting a shape of the die which is necessary for preventing the occurrence of predominantly bending crack during press forming.SOLUTION: The strain of a surface of a metal plate when a predominantly ductile crack occurs is obtained using the minimum radius Rof curvature of a press forming die and the critical strain εof a plane strain area in a forming limit diagram. By this means, a prediction expression [R/t≥(2R/t+(2R/t+1)ε)/2(1-(1+2R/t)ε)] is derived by which it can be determined that a predominantly bending crack does not occur if the obtained strain is equal to or less than the critical surface strain ε. Then, in order to prevent the occurrence of the predominantly bending crack, the minimum radius Rof curvature which is necessary for the die is predicted, and the die having the radius of curvature equal to or larger than the radius Rof curvature is designed.
    • 要解决的问题:设计一种模具,其中通过预测在压制成型期间防止主要弯曲裂纹发生所需的模具的形状,不会发生主要的弯曲裂纹。解决方案:金属板的表面的应变 当使用压制成型模具的最小半径Rof曲率和成形限制图中的平面应变面积的临界应变值获得主要是延性裂纹时。 通过这种方式,推导出可以确定的预测表达式[R /t≥(2R / t +(2R / t + 1)&egr))/ 2(1-(1 + 2R / t)&egr 如果获得的应变等于或小于临界表面应变,则不会发生主要弯曲的裂纹。 然后,为了防止主要弯曲裂纹的发生,预测了模具所需的最小半径Rof曲率,并且设计了具有等于或大于半径Rof曲率的曲率半径的模具。
    • 36. 发明专利
    • Reference position setting method for replica such as of model and centering jig used in this method
    • 在本方法中使用的模型和中心的替代的参考位置设置方法
    • JPS57127528A
    • 1982-08-07
    • JP1074381
    • 1981-01-29
    • Nissan Motor Co Ltd
    • SAIKI YASUMASAIKENO YOSHIYUKI
    • B21D37/20
    • B21D37/20
    • PURPOSE:To prevent occurrence of an error and make positioning at high accuracy by inserting a centering jig into an embedded bush installed in a replica. CONSTITUTION:Three holes P, Q, and R are made on a reference model and the first embedded bushes are installed in the holes P, Q, and R. Next, a connecting pin 9 is fitted to a hole 10a of the second embedded bush 7a allowing free detaching. Under this condition the connecting pin 9 is fitted to a hole 10 of the embedded bush 7 allowing free detaching. Consequently, the embedded bush 7a is arranged concentrically with the embedded bush 7. Under this state, a male mold model 2 as a replica is formed using synthetic reasin etc. After forming the model 2, this is separated from the reference model and a centering jig 11 is inserted into the hole 10a of the embedded bush 7a. Using this centering jig, criteria of measurement are picked up by the needle of a layout machine.
    • 目的:通过将定心夹具插入安装在复制品中的嵌入式衬套中,防止发生错误并进行高精度定位。 构成:在参考模型上制作三个孔P,Q和R,第一个嵌入式衬套安装在孔P,Q和R中。接下来,连接销9装配到第二嵌入衬套 7a允许自由分离。 在这种情况下,连接销9装配到嵌入式衬套7的孔10中,允许自由分离。 因此,嵌入式衬套7a与嵌入式衬套7同心地配置。在该状态下,使用合成再固化剂等形成作为副本的阳模型2.在形成模型2之后,将其与参考模型分离,并且定心 夹具11插入到嵌入式衬套7a的孔10a中。 使用该定心夹具,测量标准由布局机的针拾取。
    • 40. 发明专利
    • ダイヤモンドライクカーボン層積層体およびその製造方法
    • 类似钻石的碳层层压板及其制造方法
    • JP2016128599A
    • 2016-07-14
    • JP2015003517
    • 2015-01-09
    • 株式会社神戸製鋼所
    • 伊藤 弘高
    • C23C16/27B32B15/04B23B27/14B23B27/20B21D37/01B21D37/20C23C14/06
    • B21D37/01B21D37/20B23B27/14B23B27/20B32B15/04C23C14/06C23C16/27
    • 【課題】DLC層が高い密着性を示し、特には厳しい環境で使用する場合やDLC層を厚くした場合であっても高い密着性を示し、かつ中間層の構造が複雑でなく生産性よく形成できるダイヤモンドライクカーボン層積層体を提供する。 【解決手段】基材上に、ダイヤモンドライクカーボン層が、中間層を介して形成された積層体であって、前記中間層は、前記基材上に設けられた第1層と、該第1層上に設けられた第2層とからなり、前記基材は金属からなり、前記第1層はCrからなり、前記第2層はCrと炭素とからなり、前記基材側から前記ダイヤモンドライクカーボン層側に向かって炭素が増加するとともにCrが減少する組成傾斜構造を有し、かつ該第2層のダイヤモンドライクカーボン層と接する面の、Crと炭素の合計に対する炭素の割合が80原子%以下であることを特徴とするダイヤモンドライクカーボン層積層体。 【選択図】なし
    • 要解决的问题:提供类金刚石碳层层叠体,其中类金刚石碳层(DLC层)对基材表现出高粘合性,特别是甚至当在恶劣环境中使用或增加DLC厚度时 由于中间层的结构不复杂,所以表现出高粘附性并且可以以高生产率形成。解决方案:类金刚石碳层层压体是层叠层,其中在基底上形成类金刚石碳层,通过 中间层。 中间层包括形成在基底上的第一层和形成在第一层上的第二层。 基板由金属制成。 第一层是由Cr制成。 第二层由Cr和碳制成,并且具有组成梯度结构,其中碳含量增加并且Cr的含量从衬底侧朝向类金刚石碳层侧减小。 与金刚石状碳层接触的第二层的表面中的碳与Cr和碳的总量的比例为80原子%以下。选择图:无