    • Hard anodize of cold spray aluminum layer
    • 冷喷涂铝层的硬阳极氧化
    • EP2204473A2
    • 2010-07-07
    • EP09252862.9
    • 2009-12-22
    • United Technologies Corporation
    • Bogue, WilliamLomasney, Gary M.Derosa, Robert J.Bunting, Billie W.Parkos, Joseph
    • C23C24/04C25D11/08C25D11/16C25D11/24
    • C23C24/04C23C28/322C23C28/345C25D11/08C25D11/16C25D11/24C25D11/30F01D5/288F05D2230/31F05D2230/90F05D2300/121
    • A process for repairing components (60) includes the steps of providing a component (60) having an affected area (44) on a surface (45) of a component (60) to be repaired; depositing a repair material over the affected area (44) on the surface (45) of the component (60) so that the repair material plastically deforms without melting and bonds to the affected area (44) upon impact with the affected area (44) and thereby covers the affected area (44); providing a sulfuric acid based anodizing solution; anodizing a deposited repair material on the surface (45) of said component (60) in the sulfuric acid based anodizing solution; consuming only a portion of the deposited repair material to form a hard anodized coating layer upon the deposited repair material to form a hard anodized coated component (60); providing a corrosion resistant sealant solution; and contacting a hard anodized coated component with the corrosion resistant sealant solution to form a corrosion resistant sealant coating on the hard anodized coated component (60).
    • 用于修复部件(60)的方法包括以下步骤:在待修复的部件(60)的表面(45)上提供具有受影响区域(44)的部件(60) 将修复材料沉积在部件(60)的表面(45)上的受影响区域(44)上,使得修复材料在没有熔化的情况下塑性变形并且在与受影响区域(44)撞击时结合到受影响区域(44) 从而覆盖受影响的区域(44); 提供硫酸基阳极氧化溶液; 在所述硫酸基阳极氧化溶液中将沉积的修复材料阳极氧化在所述部件(60)的表面(45)上; 仅消耗一部分沉积的修复材料以在沉积的修复材料上形成硬质阳极氧化涂层以形成硬质阳极氧化涂层组件(60); 提供耐腐蚀密封剂溶液; 以及使硬质阳极氧化涂层部件与耐腐蚀密封剂溶液接触以在硬质阳极氧化涂层部件(60)上形成耐腐蚀密封剂涂层。