    • 3. 发明公开
    • Longitudinal magnetic recording medium
    • Langgestreckter磁铁Aufzeichnungsträger。
    • EP0435159A1
    • 1991-07-03
    • EP90124823.7
    • 1990-12-19
    • MITSUBISHI KASEI CORPORATION
    • Miyamoto, YukihiroYokoyama, Fumiaki
    • G11B5/712G11B5/704G11B5/706G11B5/66
    • G11B5/656G11B5/7305Y10S428/90Y10S428/928Y10T428/12465Y10T428/1275Y10T428/12854Y10T428/12944Y10T428/265Y10T428/31
    • A longitudinal magnetic recording medium comprising a non-magnetic substrate having a texture with a central line average roughness Ra in a circumferential direction of at least 20 Å and a magnetic alloy layer comprising cobalt and chromium as the main components, formed on the substrate, wherein the magnetic alloy layer has (i) a feature that when the orientation degree of the hcp crystal structure is represented by the diffraction ray intensity of electron diffraction by transmission electron diffractiometry, the intensity ratio of the electron diffraction ring in the Co (002) plane between the circumferential direction and the radial direction of the substrate is at least 3, and (ii) a segregation structure having low chromium concentration regions surrounded by high chromium concentration regions, the diameters of the defined low chromium concentration regions being within a range of from 80 to 500 Å, and the number of the surrounded low chromium concentration regions being from 600 to 1,500 regions/µm².
    • 一种纵向磁记录介质,其特征在于,在所述基板上形成有非磁性基板,所述非磁性基板的圆周方向的中心线平均粗糙度Ra为至少20nm,磁性合金层为主要成分, 磁性合金层具有(i)当通过透射电子衍射法测定电子衍射的衍射光强度来表示hcp晶体结构的取向度时,Co(002)面中的电子衍射环的强度比 在基板的圆周方向和径向方向之间至少为3,以及(ii)具有由高铬浓度区域包围的低铬浓度区域的偏析结构,所定义的低铬浓度区域的直径在 80至500安格姆,以及包围的低铬浓度区域的数量 为600〜1500个/亩2。