    • A method is provided for producing large cubic boron nitride crystals having the size of 0,1 carat or larger. The method involves providing a reaction vessel which contains CBN seed material, a CBN source separated from the seed material by a mass of solvent/catalyst for CBN synthesis which is capable of melting under CBN synthesis conditions, the separation of seed material and source material being such that under the operating conditions of CBN synthesis a temperature gadient is created between the seed material and the source material with the seed material being located at a point near the minimum value of temperature of the temperature gradient and the source material being located at a point near the maximum value of temperature of the temperature gradient, placing that reaction vessel in the reaction zone of a high temperature/high pressure apparatus and subjecting the contents of the reaction vessel to conditions of temperature and pressure in the CBN stable region of the boron nitride phase diagram for a period of at least several hours.
    • 提供了一种生产尺寸为0.1克拉或更大的大立方氮化硼晶体的方法。 该方法包括提供包含CBN种子材料的反应容器,通过用于CBN合成的溶剂/催化剂的质量与种子材料分离的CBN源,其能够在CBN合成条件下熔化,种子材料和源材料的分离为 使得在CBN合成的操作条件下,在种子材料和源材料之间产生温度gad子,其中种子材料位于温度梯度的最小温度值附近的点处,并且源材料位于一点 接近温度梯度温度的最大值,将该反应容器置于高温/高压设备的反应区中,并将反应容器的内容物置于氮化硼的CBN稳定区域中的温度和压力条件下 相图至少持续几个小时。
    • 4. 发明公开
    • Cubic boron nitride manufacture
    • Herstellung von kubischem Bornitrid。
    • EP0255327A2
    • 1988-02-03
    • EP87306632.8
    • 1987-07-28
    • DE BEERS INDUSTRIAL DIAMOND DIVISION (PROPRIETARY) LIMITED
    • Hedges, Lesley KayRobertson, Stuart HedleyDavies, Geoffrey John
    • C30B29/38C30B9/00
    • C30B9/00B01J3/062B01J2203/0645B01J2203/066B01J2203/068C30B29/403Y10T117/1096
    • A method is provided for producing large cubic boron nitride crystals having the size of 0,1 carat or larger. The method involves providing a reaction vessel which contains CBN seed material, a CBN source separated from the seed material by a mass of solvent/catalyst for CBN synthesis which is capable of melting under CBN synthesis conditions, the separation of seed material and source material being such that under the operating conditions of CBN synthesis a temperature gadient is created between the seed material and the source material with the seed material being located at a point near the minimum value of temperature of the temperature gradient and the source material being located at a point near the maximum value of temperature of the temperature gradient, placing that reaction vessel in the reaction zone of a high temperature/high pressure apparatus and subjecting the contents of the reaction vessel to conditions of temperature and pressure in the CBN stable region of the boron nitride phase diagram for a period of at least several hours.
    • 提供了一种用于生产尺寸为0.1克拉或更大的大型立方氮化硼晶体的方法。 该方法包括提供一种包含CBN种子材料的反应容器,通过大量用于CBN合成的溶剂/催化剂与种子材料分离的CBN源,其能够在CBN合成条件下熔化,种子材料和源材料的分离 使得在CBN合成的操作条件下,在种子材料和源材料之间产生温度启动子,种子材料位于接近温度梯度的最低温度值的点,并且源材料位于一点 接近温度梯度的最大温度值,将反应容器置于高温/高压装置的反应区中,并使反应容器中的内容物在氮化硼的CBN稳定区域中进行温度和压力条件 相图至少数小时。