    • Method for cleaning vulcanization mold
    • Verfahren zum Reinigen einer Vulkanisationsform
    • EP0790113A3
    • 1998-02-04
    • EP97102414.6
    • 1997-02-14
    • Bridgestone CorporationHoriike, Yasuhiro
    • Saitoh, ShinjiOhno, ShingoKato, NobukoHoriike, Yasuhiro
    • B29C33/72B08B7/00
    • B29C33/72B08B7/0035B29D2030/0663B29L2030/00
    • A cleaning method for realizing uniform ashing of residues at a high efficiency by uniformly injecting neutral active species directly toward the surfaces of vulcanization residues left on a vulcanization mold is described. The method includes setting a ring-shaped cavity in face-to-face reaction with the inner surfaces of a ring-shaped vulcanization mold (15) in a vacuum treating vessel(1), transmitting a microwave in the cavity (7), and emitting the microwave via a number of coupling slots formed in the outer side of the cavity (7) toward the inner surfaces (15s) of the vulcanization mold (15) whereupon a reaction gas is injected in the space of the treating vessel between the inner surfaces (15s) of the vulcanization mold and the cavity (7), so that a plasma including a major proportion of neutral active species generated from the reaction gas and the emitted microwave, and the elastomer residue is ashed by means of at least one gas selected from the plasma gas and a neutral active species-containing gas. A microwave generator useful for the method is also described.
    • 描述了通过将中性活性物质直接向残留在硫化模具上的硫化残余物的表面均匀地注入来实现高效残留物均匀灰化的清洁方法。 该方法包括在真空处理容器(1)中将环状空腔与环形硫化模具(15)的内表面进行面对面反应,在空腔(7)中传送微波,以及 通过形成在空腔(7)的外侧中的多个耦合槽朝向硫化模具(15)的内表面(15)发射微波,从而将反应气体注入处理容器的内部 硫化模具和空腔(7)的表面(15s),使得包含由反应气体和发射的微波产生的主要比例的中性活性物质的等离子体和弹性体残留物通过至少一种气体 选自等离子体气体和含中性活性物质的气体。 还描述了一种对该方法有用的微波发生器。
    • 3. 发明公开
    • Antireflection film
    • Entspiegelnde beschichtung
    • EP1154288A2
    • 2001-11-14
    • EP01303888.0
    • 2001-04-27
    • Bridgestone Corporation
    • Nishida, MitsuhiroOhno, ShingoYoshikawa, MasatoKato, Nobuko
    • G02B1/11
    • G02B1/111Y10T428/1059Y10T428/1064Y10T428/24942Y10T428/249939Y10T428/249953Y10T428/24998Y10T428/25
    • An antireflection film, which has excellent properties of preventing reflection and pollution, excellent marring resistance and chemical resistance and a low cost, comprises an organic film 4, a hard coating layer 3 formed on the organic film 4, a layer 2 having high index of refraction formed on the hard coating layer 3, and a surface layer 1 made of organic resin having excellent marring resistance and chemical resistance formed on the layer 2. Each of layers 1 through 3 is made of synthetic resin like acrylic resin. The high index of refraction of the layer 2 is brought by minute particles of metallic oxides having high indices of refraction included in the layer 2. Antistatic properties are given to either the layer 2 having high index of refraction or the hard coating layer 3 by doping electrically conductive minute particles.
    • 具有防止反射和污染,防恶劣性,耐化学性和低成本的优异性能的抗反射膜包括有机膜4,形成在有机膜4上的硬涂层3,具有高折射率的层2 形成在硬涂层3上的折射和在层2上形成的具有优异耐划伤性和耐化学性的由有机树脂制成的表面层1。层1至3中的每一个由合成树脂如丙烯酸树脂制成。 层2的​​高折射率由层2中包含的具有高折射率的金属氧化物的微小颗粒引起。抗静电性能被赋予具有高折射率的层2或通过掺杂的硬涂层3 导电微粒。
    • 6. 发明公开
    • Process for producing rubber-based composite material
    • Verfahren zur Herstellung von Verbundmaterialien auf Kautschukbasis
    • EP0872511A3
    • 1999-01-20
    • EP98106729.1
    • 1998-04-14
    • Bridgestone Corporation
    • Yoshikawa, MasatoKato, Nobuko
    • C08J5/12C08J3/24
    • C08J3/24C08J5/12C08J2321/00
    • A process for producing a rubber-based composite material including steps of laminating a rubber compound onto a substrate, with a bonding layer of metal or metal compound interposed therebetween, and subsequently vulcanizing the rubber compound, characterized in that vulcanization is carried out by controlling the composition of the rubber compound and the amount of metal in the bonding layer such that the following equation is established. x - 19 ≧ y ≧ 0.2 x - 12 wherein x is the amount (atom%) of metal in the bonding layer, and y is the slope (kgf·cm/min) of the vulcanization curve of the rubber compound. The rubber-based composite material retains good bond strength even when used in such a way that its bond interface is in contact with water. In addition, it has good adhesion to the substrate treated by conversion treatment.
    • 一种橡胶系复合材料的制造方法,其特征在于,包括以下步骤:将橡胶化合物层压到基材上,并且将金属或金属化合物的接合层插入其间,然后硫化所述橡胶化合物,其特征在于,通过控制 橡胶化合物的组成和接合层中的金属量,使得建立以下等式。 其中x是粘合层中金属的量(原子%),y是橡胶化合物的硫化曲线的斜率(kgf.cm / min)。 即使以这样的方式使用橡胶基复合材料,其粘合界面也与水接触。 此外,它对通过转化处理处理的基材具有良好的粘合性。
    • 9. 发明公开
    • Antireflection film
    • Entspiegelnde Beschichtung
    • EP1154288A3
    • 2004-07-28
    • EP01303888.0
    • 2001-04-27
    • Bridgestone Corporation
    • Nishida, MitsuhiroOhno, ShingoYoshikawa, MasatoKato, Nobuko
    • G02B1/11
    • G02B1/111Y10T428/1059Y10T428/1064Y10T428/24942Y10T428/249939Y10T428/249953Y10T428/24998Y10T428/25
    • An antireflection film, which has excellent properties of preventing reflection and pollution, excellent marring resistance and chemical resistance and a low cost, comprises an organic film 4, a hard coating layer 3 formed on the organic film 4, a layer 2 having high index of refraction formed on the hard coating layer 3, and a surface layer 1 made of organic resin having excellent marring resistance and chemical resistance formed on the layer 2. Each of layers 1 through 3 is made of synthetic resin like acrylic resin. The high index of refraction of the layer 2 is brought by minute particles of metallic oxides having high indices of refraction included in the layer 2. Antistatic properties are given to either the layer 2 having high index of refraction or the hard coating layer 3 by doping electrically conductive minute particles.
    • 具有防止反射和污染,防恶劣性,耐化学性和低成本的优异性能的抗反射膜包括有机膜4,形成在有机膜4上的硬涂层3,具有高折射率的层2 形成在硬涂层3上的折射和在层2上形成的具有优异耐划伤性和耐化学性的由有机树脂制成的表面层1。层1至3中的每一个由合成树脂如丙烯酸树脂制成。 层2的​​高折射率由层2中包含的具有高折射率的金属氧化物的微小颗粒引起。抗静电性能被赋予具有高折射率的层2或通过掺杂的硬涂层3 导电微粒。