    • 1. 发明公开
    • LEATHER WITH SELF-CLEANING PROPERTIES AND RESISTANCE TO HEAT/FIRE AND METHOD OF OBTAINING THEREOF
    • 具有自洁性能及抗革产热的/ Fire和方法
    • EP3173493A1
    • 2017-05-31
    • EP16464008.8
    • 2016-09-06
    • Institutul National de Cercetare-Dezvoltare Pentru Textile si Pielarie (INCDTP) Sucursala Institul de Cercetare Pielarie Incaltaminte (ICPI)
    • GAIDÃU, Carmen CorneliaIGNAT, Madalina CameliaPITICESCU, Roxana MioaraPITICESCU, Radu RobertPOPESCU, Laura MadalinaIONESCU, Marcel
    • C14C11/00C14C13/00C14C9/00
    • C14C11/003C14C9/00C14C13/00
    • The invention relates to leather for furniture and automotive upholstery and protective footwear, surface finished with titanium dioxide nano particles doped with 10% silica with an average particle size of 46 nm and with self-cleaning properties and improved resistance to heat transmission and combustion. The process for obtaining leather with self-cleaning properties and resistance to heat/fire consists in applying the base coat containing 0.05-10% titanium dioxide nano particles (% relative to the amount of binder) doped with 10% of silica which are dispersed in an equal amount of polyethylene glycol 600 and, according to another variant, 0.01-15% sodium polyacrylate, by mechanical stirring for 10 minutes, followed by sonication for 5 minutes, with pigment paste based on macro titanium dioxide, water and acrylic binder. This composition is applied by spraying in successive coats with intermediate drying and final pressing at 110°C and 20 kgf, followed by fixation with nitrocellulose lacquer in successive coats, with intermediate drying and final pressing in the same conditions. Self-cleaning properties are provided through photocatalytic degradation of organic dirt under the influence of ultraviolet and visible light and resistance to heat transfer and combustion.
    • 本发明涉及皮革的家具和汽车内饰和防护鞋,表面掺杂有10%的二氧化硅上的46纳米的平均颗粒尺寸,并与自清洁性能和改善的热传递和燃烧性二氧化钛纳米颗粒结束。 用于获得皮革具有自洁性,耐热性/火besteht申请(相对于粘合剂的量%)掺杂有分散在二氧化硅的10%的底涂层含有0.05〜10%的二氧化钛纳米粒子的制造方法 ,聚丙烯酸酯,基于宏二氧化钛,水和丙烯酸类粘合剂等量聚乙二醇600和,雅鼎的另一种变型0.01-15%钠,由10分钟的机械搅拌,随后超声处理5分钟,用颜料糊。 该组合物通过喷涂在连续的外套与中间干燥和最终压制在110℃和20千克力,接着用在连续涂层硝基漆固定,与中间干燥和最终在相同条件下加压的应用。 自清洁性能通过的有机污垢光催化降解的紫外线和可见光和耐热传递和燃烧的影响下提供。
    • 5. 发明公开
    • COLLAGEN POLYDISPERSIONS FOR THE TREATMENT OF CEREAL SEEDS AND PROCESS THEREOF
    • 用于处理谷物种子的胶原多分散物及其加工
    • EP3170393A1
    • 2017-05-24
    • EP15464007.2
    • 2015-11-24
    • Institutul National de Cercetare-Dezvoltare Pentru Textile si Pielarie (INCDTP) Sucursala Institul de Cercetare Pielarie Incaltaminte (ICPI)
    • Niculescu, Mihaela-DoinaGaidau, Carmen CorneliaEpure, Doru-GabrielGîdea, MihaiStepan, Emil
    • A01N25/04A01N61/00A23J1/10C12P21/06
    • A23J1/10A01N63/02C12P21/06A01N25/00A01N25/04
    • The invention relates to a product based on collagen polydispersions used for cereal seed treatment in order to stimulate growth, reduce the intake of pesticides and the process of manufacturing thereof.
      Extraction of collagen polydispersions from leather waste occurs in two phases carried out through a compact process in the first phase through alkaline hydrolysis of chrome tanned leather waste, with 8-12% calcium oxide, or thermal hydrolysis of rawhide waste, at a solid/liquid ratio of 1/4, at a temperature of 70.....85°C, stirring for a period of 3.....5 hours and static until the next day without thermal input, followed by enzymatic hydrolysis with enzymatic preparation Alcalase 2.4L in concentration of 2.5.....4.5 enzyme units/total nitrogen gram, at a temperature of 63°C ± 2°C continuously stirring for 3.....5 hours for tanned leather waste, and static until the next day without thermal input in the case of extraction from rawhide waste. This process enables protein mass recovery in a proportion of 85.....95% and cleavage of peptide chains, yielding collagen polydispersions containing free amino acids, with average molecular weight of 4000-6000 Da for systemic cereal seed treatment, with effects on stimulating germination and increasing resistance to insect and fungal attacks.
    • 本发明涉及用于谷物种子处理的基于胶原多分散体的产品,以刺激生长,减少农药的摄入量及其制造过程。 皮革废料中胶原多分散体的萃取分两个阶段进行,第一阶段通过一个紧凑的过程,通过碱性水解铬鞣制的皮革废料,8-12%的氧化钙或生皮废料的热水解,固/液 比例为1/4,温度为70 ..... 85°C,搅拌3 ..... 5小时,静止至第二天无热输入,然后用酶制剂进行酶水解 碱性蛋白酶2.4L浓度为2.5 ..... 4.5酶单位/总氮克,在63℃±2℃的温度下持续搅拌3 ........ 5小时,鞣制皮革废物,静止至 第二天在没有热量输入的情况下从生皮废物中提取。 该过程使得蛋白质质量回收率可达85%-95%,肽链断裂,产生含有游离氨基酸的胶原多分散体,平均分子量为4000-6000Da,用于全身谷物种子处理,对 刺激发芽并增加对昆虫和真菌攻击的抵抗力。