会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 1. 发明授权
    • Method for making weldless magnesium/aluminum bonded components
    • 无镁镁合金部件的制造方法
    • US06450396B1
    • 2002-09-17
    • US09895371
    • 2001-07-02
    • Paul Edward Krajewski
    • Paul Edward Krajewski
    • B23K2000
    • B23K20/023B23K2103/10
    • A method of joining at least a portion of a first substrate with at least a portion of a second substrate. The first substrate includes at least 90 weight percent aluminum and a first set of additives wherein magnesium is the dominant constituent in the additives. The second substrate includes at least 85 weight percent magnesium and a second set of additives wherein aluminum is the dominant constituent of the second set of additives. The first and second substrates are heated to an elevated temperature ranging from about 440° C. to 500° C. Pressure is applied to the first and second substrates at least at one point of contact to bond the first and second substrates together.
    • 将第一基板的至少一部分与至少一部分第二基板接合的方法。 第一衬底包括至少90重量%的铝和第一组添加剂,其中镁是添加剂中的主要成分。 第二基材包括至少85重量%的镁和第二组添加剂,其中铝是第二组添加剂的主要成分。 将第一和第二基底加热到约440℃至500℃的升高温度。至少在一个接触点将压力施加到第一和第二基底上以将第一和第二基底结合在一起。
    • 3. 发明授权
    • High temperature isostatic pressure bonding of beryllium pressure vessels with an interior void
    • 具有内部空隙的铍压力容器的高温等压压接
    • US06264095B1
    • 2001-07-24
    • US09350349
    • 1999-07-14
    • Charles J. StoufferPatrick BourkeJames M. MarderLawrence H. Ryczek
    • Charles J. StoufferPatrick BourkeJames M. MarderLawrence H. Ryczek
    • B23K2000
    • B23K20/233B23K20/002B23K20/021
    • A process of bonding metal parts to one another to form seamless, hollow metal articles, particularly made from beryllium. Tooling is assembled to the parts, prior to hot pressing, to cause pressure to be applied to selective portions of the parts. The parts, assembled together with the tooling, are then subjected to hot isostatic pressing at a temperature of about 1700° F. to 1750° F., and at a pressure of about 2000 psi to 2500 psi, for around 3 hours. The tooling surrounding the metal parts functions to limit the amount of compression of the parts. Articles formed by this process are particularly useful in space flight applications because they are formed of a homogeneous material. Strength of the bond is enhanced because no filler metal is used. The absence of a filler metal also eliminates any thermal stress problems as a result of differences in coefficients of thermal expansion.
    • 将金属部件彼此粘合以形成无缝的中空金属制品,特别是由铍制成的方法。 在热压之前,将模具组装到部件上,以将压力施加到部件的选择性部分。 然后将与工具组装在一起的部件在约1700°F至1750°F的温度和约2000psi至2500psi的压力下进行约3小时的热等静压。 围绕金属部件的工具用于限制部件的压缩量。 通过该方法形成的物品在空间飞行应用中特别有用,因为它们由均匀的材料形成。 由于不使用填料金属,粘结强度提高。 不存在填充金属也消除了由于热膨胀系数差异导致的任何热应力问题。
    • 4. 发明授权
    • Rolled plate joining apparatus and continuous hot rolling apparatus equipped with the same
    • 轧制板接合装置和配备有其的连续热轧装置
    • US06189763B1
    • 2001-02-20
    • US09384592
    • 1999-08-27
    • Nobuhiro TazoeToshio IwanamiMasami OkiKouiti SakamotoSuguhiro FukushimaToshihiro Mori
    • Nobuhiro TazoeToshio IwanamiMasami OkiKouiti SakamotoSuguhiro FukushimaToshihiro Mori
    • B23K2000
    • B21B15/0085B21B1/024B21B1/224B21B1/26B21B1/46B21B15/0007B21B39/14B21B2015/0057B23Q11/10Y10T29/5184Y10T408/45Y10T408/46Y10T409/304032Y10T409/304144Y10T483/15Y10T483/1736Y10T483/174
    • There is provided a rolled plate joining apparatus equipped with a truck that can travel reversibly in the rolling direction, tailing end pinch rolls that are mounted on the truck and can be moved vertically with the tailing end of a preceding rolled plate pinched horizontally, leading end pinch rolls that are mounted on the truck and can pinch horizontally the leading end of a succeeding rolled plate, machining apparatuses for cutting one surface of the tailing end of the preceding rolled plate and the other surface of the leading end of the succeeding rolled plate, and a pressure welding apparatus for compressing the preceding rolled plate and the succeeding rolled plate with the machined surfaces of the preceding rolled plate and the succeeding rolled plate overlapped to reduce them approximately to the thickness of the rolled plates, including a tailing end centering apparatus placed between the tailing end pinch rolls and the pressure welding apparatus for pressing the opposite width ends of the tailing end of the rolled plate to align the center line of the rolled plate with the center line of the joining apparatus in the rolling direction and a leading end centering apparatus placed between the pressure welding apparatus and the leading end pinch rolls for pressing the opposite width ends of the leading end of the rolled plate to align the center line of the rolled plate with the center line of the joining apparatus in the rolling direction.
    • 本发明提供了一种装有卡车的轧制板接合装置,其能够在轧制方向上可逆地移动,拖尾端夹送辊安装在卡车上,并且可以在先前的轧制板的拖尾端水平地夹紧的状态下垂直移动, 夹持辊安装在卡车上,可以水平地夹紧后续轧制板的前端,用于切割前一轧制板的尾端的一个表面和后续轧制板的前端的另一个表面的加工装置, 以及用于压缩先前的轧制板和随后的轧制板的压力焊接装置,其中前轧制板和随后的轧制板的加工表面重叠,以将它们大致减小到轧制板的厚度,包括设置在尾部定中心装置 在后端夹送辊和用于按压相对的wi的压力焊接装置之间 轧制板的后端的第二端部,使轧制板的中心线与轧制方向的接合装置的中心线对准,并且将前端定心装置配置在压接装置与前端夹送辊之间, 将轧制板的前端的相对的宽度端压入轧制板的中心线与轧制方向的中心线对准。
    • 6. 发明授权
    • Terminal pressure-welding apparatus
    • 端子压焊设备
    • US06513695B2
    • 2003-02-04
    • US09781997
    • 2001-02-14
    • Nobuaki Yamakawa
    • Nobuaki Yamakawa
    • B23K2000
    • B23K20/02B23K2101/38
    • A terminal pressure-welding apparatus is provided, which includes: a first pattern; a second pattern facing the first pattern, one of the first and second patterns is provided approachably and disapproachably with respect to the other thereof; a mounting portion to mount the other of the first and second patterns; a displacing member carrying the one of the first and second patterns and being movable relatively to the other of the first and second patterns; and a stopping means to check an abutment of the first pattern and the second pattern, wherein a terminal metal fitting and an end portion of an electric wire are placed between the first and second patterns, and the terminal metal fitting and the end portion are pressure-welded by making the first and second patterns approach each other. The stopping means has a projecting portion projecting from the mounting portion toward the displacing member in order to abut against an end plane of the displacing member thereby to check the abutment of the first and second patterns. The projecting portion has an abutting plane to abut against the end plane, an adjusting means of a distance between the abutting plane and the mounting portion, and a fixing means to secure the projecting portion to the mounting portion for keeping the distance.
    • 提供端子压焊装置,其包括:第一图案; 面向第一图案的第二图案,第一图案和第二图案中的一个相对于另一图案可接近地和不可预见地提供; 安装所述第一和第二图案中的另一个的安装部分; 移动构件承载第一和第二图案中的一个并且可相对于第一和第二图案中的另一个移动; 以及止动装置,用于检查第一图案和第二图案的邻接部,其中端子金属配件和电线的端部被放置在第一和第二图案之间,并且端子金属配件和端部是压力 通过使第一和第二模式彼此接近而被焊接。 止动装置具有从安装部朝向位移构件突出的突出部分,以便抵靠位移构件的端面,从而检查第一和第二图案的邻接。 突出部分具有邻接端面的抵接平面,邻接平面和安装部分之间的距离的调节装置,以及用于将突出部分固定到安装部分以保持距离的固定装置。
    • 7. 发明授权
    • Metal sandwich structure with integral hardpoint
    • 金属夹层结构具有整体硬度
    • US06419146B1
    • 2002-07-16
    • US09610665
    • 2000-07-05
    • Frederick W. BuldhauptJohn R. FischerMatthew G. KistnerJeffrey D. Will
    • Frederick W. BuldhauptJohn R. FischerMatthew G. KistnerJeffrey D. Will
    • B23K2000
    • B64C1/12B21D26/055B21D47/00B23K26/037B23K26/123B23K26/206B23K26/244B23K26/26B23K26/28B23K26/38B23K2101/02B64C2001/0081Y10T29/18Y10T29/49371Y10T428/1234Y10T428/12347Y10T428/12361Y10T428/12375
    • A superplastically formed, diffusion bonded sandwich structure having integral metal hardpoints, made by joining two superplastic metal core sheets together into a core pack by welding or diffusion bonding along a pattern of lines which form junction lines between the core sheets when the pack is inflated by gas pressure at superplastic temperatures. Face sheets are laid under and over the core pack and metal inserts are interposed between the face sheets and the core. All of the sheets in the pack are sealed together around an outside peripheral edge to create a gas tight envelope. The pack is heated to superplastic temperatures in a cavity in a die, and the top and bottom face sheets are diffusion bonded to top and bottom surfaces of the metal insert by application of heat and pressure from top and bottom inner surfaces of the die cavity. While at superplastic temperatures, the pack is inflated by gas pressure against inside surfaces of a die to form an expanded metal sandwich structure having integral webs and integral hardpoints formed by the metal insert. After forming, the gas pressure is reduced to near atmospheric, the die is opened and the part is removed from the die.
    • 一种具有整体金属硬点的超塑性扩散粘结夹层结构,其通过沿着线形图案通过焊接或扩散接合将两个超塑性金属芯片连接在一起,制成芯组件,该芯线在芯片片材之间形成连接线时, 超塑性气体压力。 将面片放置在芯组件的下面和后面,金属插入件插入在面片和芯之间。 包装中的所有片材围绕外围边缘密封在一起以形成气密封壳。 将包装件加热到模具中的空腔中的超塑性温度,并且通过从模腔的顶部和底部内表面施加热和压力将顶部和底部面板扩散结合到金属插入件的顶部和底部表面。 当在超塑性温度下,该组件通过气压对模具的内表面进行充气,以形成具有整体网状物和由该金属插入件形成的整体硬点的多孔金属夹层结构。 成型后,将气体压力降低至接近大气压,打开模具,将模具从模具中取出。