    • 7. 发明申请
    • Method for producing coated article
    • 生产涂层制品的方法
    • US20060216423A1
    • 2006-09-28
    • US11384494
    • 2006-03-21
    • Yasuhito NaruseKenji HayashiManabu Hashigaya
    • Yasuhito NaruseKenji HayashiManabu Hashigaya
    • B05D3/02
    • B41C1/1008B41C1/1016B41C2201/02B41C2210/24
    • In the present invention, a coating liquid satisfies the liquid physical property conditions: (A) in the drying process, after the solid content concentration in the coating liquid is increased to 15% by mass or more by drying the coating film, or after the start of drying when the solid content concentration in the coating liquid is 15% by mass or more at the time of coating; (B) the shear viscosity of the coating liquid becomes 5 mPas or more for the shear rate of 103 sec−1 or less; (C) the value obtained through dividing by the average viscosity the first differential coefficient, the increase coefficient of the increase rate of the shear viscosity relative to the increase rate of the solid content concentration is 0.15 or more; and (D) the second differential coefficient, an additional increase coefficient of the increase coefficient relative to the solid content concentration is positive.
    • 在本发明中,涂布液在干燥工序中满足液体物性条件(A),通过干燥涂膜将涂布液中的固体成分浓度提高到15质量%以上 当涂布液中固体成分浓度为15质量%以上时开始干燥; (B)对于10 3秒-1以下的剪切速率,涂布液的剪切粘度为5mPa·s以上; (C)将平均粘度除以第一微分系数得到的值,剪切粘度的增加率相对于固体成分浓度的上升率的增加系数为0.15以上; 和(D)第二微分系数,增加系数相对于固体含量浓度的附加增加系数为正。
    • 10. 发明授权
    • Method for producing coated article
    • 生产涂层制品的方法
    • US07537805B2
    • 2009-05-26
    • US11384494
    • 2006-03-21
    • Yasuhito NaruseKenji HayashiManabu Hashigaya
    • Yasuhito NaruseKenji HayashiManabu Hashigaya
    • B05D1/00B05D7/00B05D3/00B41F1/18B41F23/04
    • B41C1/1008B41C1/1016B41C2201/02B41C2210/24
    • In the present invention, a coating liquid satisfies the liquid physical property conditions: (A) in the drying process, after the solid content concentration in the coating liquid is increased to 15% by mass or more by drying the coating film, or after the start of drying when the solid content concentration in the coating liquid is 15% by mass or more at the time of coating; (B) the shear viscosity of the coating liquid becomes 5 mPas or more for the shear rate of 103 sec−1 or less; (C) the value obtained through dividing by the average viscosity the first differential coefficient, the increase coefficient of the increase rate of the shear viscosity relative to the increase rate of the solid content concentration is 0.15 or more; and (D) the second differential coefficient, an additional increase coefficient of the increase coefficient relative to the solid content concentration is positive.
    • 在本发明中,涂布液在干燥工序中满足液体物性条件(A),通过干燥涂膜将涂布液中的固体成分浓度提高到15质量%以上 当涂布液中固体成分浓度为15质量%以上时开始干燥; (B)剪切速率为103秒-1以下时,涂布液的剪切粘度为5mPa·s以上; (C)将平均粘度除以第一微分系数得到的值,剪切粘度的增加率相对于固体成分浓度的上升率的增加系数为0.15以上; 和(D)第二微分系数,增加系数相对于固体含量浓度的附加增加系数为正。