    • 1. 发明授权
    • Polymerisation process
    • 聚合过程
    • US07915356B2
    • 2011-03-29
    • US12296216
    • 2007-04-06
    • Vincenzo ArcellaValeri KapeliouchkoStefano FerreroAniello Gargiulo
    • Vincenzo ArcellaValeri KapeliouchkoStefano FerreroAniello Gargiulo
    • C08F2/18C08F2/00C08J5/00B01J19/18
    • C08F2/01B01F7/00975B01F7/166B01F7/1665C08F14/18C08F14/26Y10S526/918C08F2/02
    • A fluoropolymer [polymer (F)], a polymerisation process for its manufacture, and a molding process using such fluoropolymer [polymer (F)].The polymerisation process comprises polymerising at least one fluorinated monomer in a polymerization medium, in which the polymerization medium is mixed by means of a stirring system comprising at least two counter-rotating impellers. Surprisingly and advantageously, the polymerization occurs without fouling or deposit formation on the reactor walls, and moreover, occurs with improved homogeneity, without composition, pressure or temperature gradients, thus enabling obtaining homogeneous polymer composition with no risk of local overheating.A polymer (F) obtained from such process has improved morphology (percentage of organized structures, i.e. of particles of regular shape) and, hence, has good free flowing properties which make it suitable for being processed by compression molding with no need of intermediate milling or grinding process or other size reduction process.
    • 含氟聚合物[聚合物(F)],其制造的聚合方法和使用这种含氟聚合物[聚合物(F)]的成型方法。 聚合方法包括在聚合介质中聚合至少一种氟化单体,其中聚合介质通过包括至少两个反向旋转叶轮的搅拌系统混合。 令人惊奇和有利地,聚合反应发生在反应器壁上没有结垢或沉积物形成,此外,在没有组成,压力或温度梯度的情况下,具有改进的均匀性发生,从而能够获得均匀的聚合物组合物,而没有局部过热的风险。 从这种方法获得的聚合物(F)具有改善的形态(有组织的结构的百分比,即规则形状的颗粒的百分比),因此具有良好的自由流动性,使其适于通过压缩加工而不需要中间研磨 或研磨过程或其他尺寸缩小过程。
    • 2. 发明申请
    • Polymerization Process
    • 聚合过程
    • US20090108501A1
    • 2009-04-30
    • US12296216
    • 2007-04-06
    • Vincenzo ArcellaValeri KapeliouchkoStefano FerreroAniello Gargiulo
    • Vincenzo ArcellaValeri KapeliouchkoStefano FerreroAniello Gargiulo
    • C08J5/00C08F2/00
    • C08F2/01B01F7/00975B01F7/166B01F7/1665C08F14/18C08F14/26Y10S526/918C08F2/02
    • A fluoropolymer [polymer (F)], a polymerisation process for its manufacture, and a moulding process using such fluoropolymer [polymer (F)].The polymerisation process comprises polymerising at least one fluorinated monomer in a polymerization medium, in which the polymerization medium is mixed by means of a stirring system comprising at least two counter-rotating impellers. Surprisingly and advantageously, the polymerization occurs without fouling or deposit formation on the reactor walls, and moreover, occurs with improved homogeneity, without composition, pressure or temperature gradients, thus enabling obtaining homogeneous polymer composition with no risk of local overheating.A polymer (F) obtained from such process has improved morphology (percentage of organized structures, i.e. of particles of regular shape) and, hence, has good free flowing properties which make it suitable for being processed by compression moulding with no need of intermediate milling or grinding process or other size reduction process.
    • 含氟聚合物[聚合物(F)],其制造的聚合方法和使用这种含氟聚合物[聚合物(F)]的成型方法。 聚合方法包括在聚合介质中聚合至少一种氟化单体,其中聚合介质通过包括至少两个反向旋转叶轮的搅拌系统混合。 令人惊奇和有利地,聚合反应发生在反应器壁上没有结垢或沉积物形成,此外,在没有组成,压力或温度梯度的情况下,具有改进的均匀性发生,从而能够获得均匀的聚合物组合物,而没有局部过热的风险。 从这种方法获得的聚合物(F)具有改善的形态(有组织的结构的百分比,即规则形状的颗粒的百分比),因此具有良好的自由流动性,使其适于通过压缩加工而不需要中间研磨 或研磨过程或其他尺寸缩小过程。
    • 7. 发明申请
    • Solar cell module
    • 太阳能电池组件
    • US20100116927A1
    • 2010-05-13
    • US12594525
    • 2008-04-04
    • Paolo TonioloPadmanabhan SrinivasanAlessio MarraniGiambattista BesanaVincenzo Arcella
    • Paolo TonioloPadmanabhan SrinivasanAlessio MarraniGiambattista BesanaVincenzo Arcella
    • B64C39/00H01L31/0203H01L31/18B64C11/00H01L31/042
    • H02S50/15B32B27/322H01L31/048H01L31/0481Y02E10/50
    • The present invention pertains to a solar cell module comprising at least one photovoltaic element encapsulated between a front layer on its light receiving surface side and a back layer, said front layer comprising at least one layer comprising a tetrafluoroethylene (TFE) polymer [polymer (F)], said polymer (F) comprising: recurring units derived from TFE; and from 15 to 25% wt of recurring units derived from at least one perfluoromonomer [monomer (CM)] chosen among: (i) perfluoroalkylvinylethers complying with formula CF2═CFORf1, in which Rf1 is a C1-C6 perfluoroalkyl, e.g. —CF3, —C2F5, —C3F7; and/or (ii) perfluoro-oxyalkylvinylethers complying with formula CF2═CFOX0, in which X0 is a C1-C12 perfluorooxyalkyl having one or more ether groups, like perfluoro-2-propoxy-propyl; and (iii) mixtures thereof. Still objects of the invention are a process for the manufacture of the solar cell module as above defined and its use for producing current to external sources, e.g. for powering a fixed-wing aircraft.
    • 本发明涉及太阳能电池模块,其包括封装在其光接收表面侧的前层和背层之间的至少一个光伏元件,所述前层包括至少一层包含四氟乙烯(TFE)聚合物[聚合物(F )],所述聚合物(F)包含:衍生自TFE的重复单元; 和15至25重量%的衍生自至少一种全氟单体[单体(CM)]的重复单元,其选自:(i)符合式CF2 = CFORf1的全氟烷基乙烯基醚,其中Rf1为C1-C6全氟烷基,例如 -CF 3,-C 2 F 5,-C 3 F 7; 和/或(ii)符合式CF 2 = CFOX 0的全氟 - 烷氧基乙烯基醚,其中X 0是具有一个或多个醚基的C 1 -C 12全氟氧烷基,如全氟-2-丙氧基 - 丙基; 和(iii)它们的混合物。 本发明的另一目的是制造如上所述的太阳能电池组件的方法及其用于产生电流至外部源的用途,例如, 为固定翼飞机提供动力。