    • 10. 发明授权
    • Piezoelectric element and process for production thereof
    • 压电元件及其制造方法
    • US06713123B2
    • 2004-03-30
    • US10428216
    • 2003-05-02
    • Toshikatsu KashiwayaMutsumi Kitagawa
    • Toshikatsu KashiwayaMutsumi Kitagawa
    • B05D500
    • H01L41/0805H01L41/083H01L41/0973H01L41/1875H01L41/314H01L41/43
    • A piezoelectric element includes: a ceramic substrate, an electrode and a piezoelectric portion made of a piezoelectric ceramic composition containing a Pb(Mg, Ni)1/3Nb2/3O3—PbZrO3—PbTiO3 ternary system solid solution composition being represented by the following general formula (1) as a main component: Pbx{(Mg1−yNiy)1/3×aNb2/3}bTicZrdO3 (1), wherein 0.95≦x≦1.05; 0.05≦y≦0.20; 0.90≦a≦1.10; b,c, and d are decimals falling in a range surrounded by (b, c, d)=(0.550, 0.425, 0.025), (0.550, 0.325, 0.125), (0.375, 0.325, 0.300), (0.100, 0.425, 0.475), (0.100, 0.475, 0.425) and (0.375, 0.425, 0.200) in the coordinates with coordinate axes of said b, c and d, and b+c+d=1.000. The electrode is electrically connected to the piezoelectric portion, and the piezoelectric portion is solidly attached to the ceramic substrate directly or via the electrode.
    • 压电元件包括​​:陶瓷基板,电极和由含有Pb(Mg,Ni)1 / 3Nb2 / 3O3-PbZrO3-PbTiO3三元体系固溶体组合物的压电陶瓷组合物制成的压电部件,由下列通式 (1)作为主要成分:Pbx {(Mg1-yNiy)1 / 3xaNb2 / 3} bTicZrdO3(1),其中0.95 <= x <= 1.05; 0.05 <= y <= 0.20; 0.90 <= a <= 1.10; (b,c,d)=(0.550,0.425,0.025),(0.550,0.325,0.125),(0.375,0.325,0.300),(0.100,0.425) ,0.475),(0.100,0.475,0.425)和(0.375,0.425,0.200)在坐标轴上的坐标,b + c + d = 1.000。 电极电连接到压电部分,并且压电部分直接或经由电极牢固地附接到陶瓷衬底。