热词
    • 8. 发明专利
    • Sliding member, method for manufacturing the same and sliding method
    • 滑动构件,其制造方法和滑动方法
    • JP2010215952A
    • 2010-09-30
    • JP2009062601
    • 2009-03-16
    • Nagoya UnivToyota Motor Corpトヨタ自動車株式会社国立大学法人名古屋大学
    • FUWA YOSHIOUMEHARA TOKUJINOOIYAMA TAKAYUKIKAMIYA MASATOHATANO TAKUYA
    • C23C14/58
    • PROBLEM TO BE SOLVED: To provide a sliding member which reduces the initial coefficient of friction of the carbon nitride coating film and also can enhance its initial affinity, and to provide a method for manufacturing the same.
      SOLUTION: This manufacturing method includes the steps of: forming the carbon nitride coating film CN on a surface of a substrate W; and irradiating the surface of the carbon nitride coating film CN with ultraviolet rays. The surface layer contains more graphite structures by being irradiated with ultraviolet rays, compared to the other part of carbon nitride which has not been irradiated with ultraviolet rays, and accordingly the sliding member can acquire enhanced initial affinity. In addition, because only the surface layer is graphitized, the strength of the carbon nitride coating film CN itself is secured.
      COPYRIGHT: (C)2010,JPO&INPIT
    • 要解决的问题:提供一种降低碳氮化物涂膜的初始摩擦系数的滑动构件,并且还可以提高其初始亲合力,并提供其制造方法。 解决方案:该制造方法包括以下步骤:在衬底W的表面上形成氮化碳涂覆膜CN; 并用紫外线照射氮化碳涂膜CN的表面。 与没有被紫外线照射的碳氮化物的其他部分相比,通过照射紫外线而表面层含有更多的石墨结构,因此滑动部件可以获得增强的初始亲和力。 此外,由于只有表面层被石墨化,所以确保了氮化碳涂膜CN本身的强度。 版权所有(C)2010,JPO&INPIT