    • 2. 发明专利
    • Injection-molded material for automobile interior part, and molding thereof
    • 用于汽车内部部件的注射成型材料及其模制件
    • JP2011074327A
    • 2011-04-14
    • JP2009229985
    • 2009-10-01
    • Kao CorpPrime Polymer Co LtdSanyo Chem Ind LtdToyota Motor Corpトヨタ自動車株式会社三洋化成工業株式会社株式会社プライムポリマー花王株式会社
    • KICHISE YOSHIFUMISHINTAKU YUJISUGIMOTO YOSHIOMORI MASAHIROTAKENAKA AKIRAFUJITA MASAYOSHI
    • C08L67/04C08K5/103C08L23/02
    • PROBLEM TO BE SOLVED: To provide an injection-molded material containing polylactic acid which excels in heat resistance, and is suitably used as moldings, such as an automobile interior part.
      SOLUTION: The injection-molded material for an automobile interior part includes: polylactic acid; a high crystalline polylactic acid based resin containing a plasticizer and a crystal nucleating agent; a polyolefin; and a compatibilizer, wherein the plasticizer has two or more ester groups in the molecule, at least one sort of alcoholic components which composes the ester groups is a compound in which 0.5-5 mols of a 2-3C alkylene oxide is added on average based on one hydroxy group, the crystal nucleating agent is a mixture of a crystal nucleating agent (a): a compound which has a hydroxy group and an amide group in the molecule and a crystal nucleating agent (b): phenylphosphonic acid or a metal salt of its derivative, and the compatibilizer is a modified polyolefin which has at least one sort of reactive groups chosen from the group consisting of an acid anhydride group, a carboxyl group, a hydroxy group and an amino group and/or a copolymer of ethylenically unsaturated monomers.
      COPYRIGHT: (C)2011,JPO&INPIT
    • 要解决的问题:提供含有耐热性优异的聚乳酸的注射成型材料,适合用作汽车内部的模制品。 汽车内部部件的注射成型材料包括:聚乳酸; 含有增塑剂和结晶成核剂的高结晶性聚乳酸类树脂; 聚烯烃; 和增容剂,其中增塑剂在分子中具有两个或更多个酯基,构成酯基的至少一种醇组分是其中平均加入0.5-5摩尔2-3C环氧烷烃的化合物 在一个羟基上,晶体成核剂是结晶成核剂(a):分子中具有羟基和酰胺基的化合物和结晶成核剂(b)的混合物:苯基膦酸或金属盐 的增容剂,增容剂是具有至少一种选自酸酐基,羧基,羟基和氨基的反应性基团和/或烯属不饱和的共聚物的改性聚烯烃 单体。 版权所有(C)2011,JPO&INPIT
    • 3. 发明专利
    • Automotive interior part having excellent heat-resistant rigidity
    • 汽车内饰部件具有优异的耐热刚性
    • JP2012092159A
    • 2012-05-17
    • JP2010238186
    • 2010-10-25
    • Nippon A&L IncToyota Motor Corpトヨタ自動車株式会社日本エイアンドエル株式会社
    • YOSHIDA HARUICHIROKICHISE YOSHIFUMI
    • C08L77/00B60K37/00C08K7/02C08L21/00C08L25/08C08L51/00
    • PROBLEM TO BE SOLVED: To provide automotive interior parts, to which leather is attached, obtained by molding a fiber-containing thermoplastic resin composition and having not only excellent impact strength, chemical resistance, and dimensional stability but also excellent heat-resistant rigidity.SOLUTION: The automotive interior parts to which leather is attached are obtained by molding the fiber-containing thermoplastic resin composition. The fiber-containing thermoplastic resin composition is a thermoplastic resin composition containing: 40-60 pts.wt. of a rubber-enforced vinyl-based resin composition (D) comprising 40-70 pts.wt. of a graft copolymer (A), 10-20 pts.wt. of an unsaturated carboxylic acid-modified copolymer (B), and 10-50 pts.wt. of a copolymer (C); and 40-60 pts.wt. of a polyamide resin (E). The fiber-containing thermoplastic resin composition satisfies formula (1) and contains a fibrous filler satisfying formula (2). Formula (1): P=n/(n+k), wherein 0.5
    • 要解决的问题:为了提供通过模制含纤维的热塑性树脂组合物获得的汽车内饰件,其具有不仅具有优异的冲击强度,耐化学性和尺寸稳定性,而且具有优异的耐热性 刚性。

      解决方案:通过模制含纤维的热塑性树脂组合物获得附着有皮革的汽车内部部件。 含纤维的热塑性树脂组合物是含有40-60重量份的热塑性树脂组合物 的橡胶强化的乙烯基类树脂组合物(D),其包含40-70重量份 的接枝共聚物(A),10-20重量份 的不饱和羧酸改性共聚物(B)和10-50重量份 的共聚物(C); 和40-60重量 的聚酰胺树脂(E)。 含纤维热塑性树脂组合物满足公式(1),并且含有满足式(2)的纤维填料。 式(1):P = n /(n + k),其中0.5

    • 5. 发明专利
    • Polylactic acid resin composition and polylactic acid resin molded article
    • 聚酸树脂组合物和聚酰胺酸树脂模塑制品
    • JP2009256412A
    • 2009-11-05
    • JP2008104244
    • 2008-04-14
    • Takemoto Oil & Fat Co LtdToyota Motor Corpトヨタ自動車株式会社竹本油脂株式会社
    • KITA KENJIKICHISE YOSHIFUMIURAYAMA YUJIHATTA AKIONISHI HIRONORI
    • C08L67/04C08J5/00C08K5/20C08L101/16
    • PROBLEM TO BE SOLVED: To provide a polylactic acid resin composition in which a crystallization rate of a polylactic acid resin forming a stereo complex is sufficiently increased as well as a stereo complex crystal ratio is increased, and to provide a polylactic acid resin molded article by melt-molding and crystallizing the polylactic acid resin composition. SOLUTION: The polylactic acid resin composition contains, with respect to 100 pts.mass of the following polylactic acid resin, 0.05 to 30 pts.mass of a nitrogen-containing compound expressed by the formula. In the formula, R 1 represents an 8-22C aliphatic acyl group; and A 1 and A 2 each represents a hydrogen atom or 2-hydroxyethyl group, provided that, at least one of A 1 and A 2 is a 2-hydroxyethyl group. The polylactic resin comprises a polylactic acid blend that can generate a stereo complex crystal, and/or a polylactic acid stereo block copolymer. COPYRIGHT: (C)2010,JPO&INPIT
    • 待解决的问题提供一种聚合乳液树脂组合物,其中形成立体络合物的聚乳酸树脂的结晶速率以及立体络合物结晶比率增加,并且提供聚乳酸树脂 通过熔融成型并使聚乳酸树脂组合物结晶而成型。 &lt; P&gt;解决方案:聚乳酸树脂组合物相对于100重量份以下聚乳酸树脂含有0.05〜30重量份的由式表示的含氮化合物。 在该式中,R“SP”1表示8-22个脂肪族酰基; 并且A 1 和A 2 各自表示氢原子或2-羟乙基,条件是A 1 和A < SP> 2 是2-羟基乙基。 聚乳酸树脂包括可产生立体络合物晶体的聚乳酸共混物和/或聚乳酸立体嵌段共聚物。 版权所有(C)2010,JPO&INPIT