    • 6. 发明授权
    • Charging member, process cartridge and electrophotographic apparatus
    • 充电部件,处理盒和电子照相设备
    • US08548359B2
    • 2013-10-01
    • US13555040
    • 2012-07-20
    • Tomohito TaniguchiMasataka KodamaTakehiko Aoyama
    • Tomohito TaniguchiMasataka KodamaTakehiko Aoyama
    • G03G15/02
    • G03G15/0233
    • A charging member is provided which can not easily cause vibration and can stably charge a photosensitive member, even where a high-frequency alternating-current voltage is applied thereto. It is a charging member having an electrically conductive substrate, an electrically conductive elastic layer and a surface layer, and the elastic layer has, in the order from the substrate side, a first rubber layer and a second rubber layer laminated to the first rubber layer, and, where the natural vibration frequency of the first rubber layer is represented by f1 and the natural vibration frequency of the second rubber layer is represented by f2, has a natural vibration frequency ratio, f2/f1, of from 2.35 or more to 10.0 or less.
    • 即使在施加高频交流电压的情况下,也能够容易地产生振动并且能够稳定地对感光体进行充电的充电部件。 是具有导电性基板,导电性弹性层和表面层的充电部件,弹性层从基板侧依次层叠有第一橡胶层和层叠到第一橡胶层的第二橡胶层 ,并且其中第一橡胶层的固有振动频率由f1表示,并且第二橡胶层的固有振动频率由f2表示,其固有振动频率比f2 / f1为2.35以上至10.0 或更少。
    • 7. 发明申请
    • CHARGING MEMBER, PROCESS CARTRIDGE, AND ELECTROPHOTOGRAPHIC APPARATUS
    • 充电会员,工艺盒和电子照相设备
    • US20110305481A1
    • 2011-12-15
    • US13217500
    • 2011-08-25
    • Tomohito TaniguchiSatoshi Koide
    • Tomohito TaniguchiSatoshi Koide
    • G03G21/18G03G15/02
    • G03G15/0233
    • An object of the present invention is to provide a charging member that brings out stable charging performance over a long period of time and also makes the surface of an electrophotographic photosensitive member not easily come to wear non-uniformly. It is a charging member having a conductive substrate and a conductive resin layer; the conductive resin layer containing a binder, conductive fine particles, and bowl-shaped resin particles each of which has an opening; the bowl-shaped resin particles being contained in the conductive resin layer in such a way as not to be exposed to the surface of the charging member; and the surface of the charging member having concavities derived from openings of the bowl-shaped resin particles and protrusions derived from edges of the openings of the bowl-shaped resin particles.
    • 本发明的一个目的是提供一种充电部件,其在长时间内产生稳定的充电性能,并且使得电子照相感光构件的表面不容易不均匀地磨损。 是具有导电性基板和导电性树脂层的充电部件, 含有粘合剂的导电树脂层,导电微粒和各具有开口的碗状树脂颗粒; 所述碗形树脂颗粒以不暴露于所述充电部件的表面的方式包含在所述导电树脂层中; 并且充电构件的表面具有源自碗状树脂颗粒的开口的凹部和源自碗状树脂颗粒的开口的边缘的突起。
    • 9. 发明授权
    • Charging member, process for its production, process cartridge
    • 充电器,其生产过程,处理盒
    • US08980423B2
    • 2015-03-17
    • US12723148
    • 2010-03-12
    • Tomohito TaniguchiTakumi FurukawaHidekazu MatsudaYusuke Yagisawa
    • Tomohito TaniguchiTakumi FurukawaHidekazu MatsudaYusuke Yagisawa
    • G03G5/04G03G15/02
    • G03G15/0233Y10T428/25
    • Concerned with a charging member in the conductive surface layer of which the conductive particles are so kept from agglomerating as to make charging performance not easily change even where the surface layer expands and contracts repeatedly in various environments. The charging member is a charging member having a conductive substrate and formed on the substrate a conductive elastic layer and a conductive surface layer. The elastic layer contains a polymer having a unit coming from ethylene oxide, and the surface layer contains a binder resin and graphitized particles. The binder resin contains a resin having in the molecule a urethane linkage or a siloxane linkage, or a urethane linkage and a siloxane linkage, and the graphitized particles have a graphite (002) plane lattice spacing of from 0.3362 nm or more to 0.3449 nm or less.
    • 涉及导电表面层中的导电表面层中的充电构件,其导电颗粒被保持凝聚,使得即使在各种环境中表面层膨胀和重复收缩的情况下,充电性能也不容易改变。 充电构件是具有导电基板的充电构件,并且在基板上形成导电弹性层和导电表面层。 弹性层含有具有来自环氧乙烷的单元的聚合物,表面层含有粘结剂树脂和石墨化颗粒。 粘结剂树脂含有在分子中具有氨基甲酸酯键或硅氧烷键或氨基甲酸酯键和硅氧烷键的树脂,并且石墨化颗粒的石墨(002)面晶格间距为0.3362nm以上至0.3449nm以下,或 减。
    • 10. 发明申请
    • CHARGING MEMBER, PROCESS FOR ITS PRODUCTION, PROCESS CARTRIDGE
    • 充值会员,其生产流程,流程盒
    • US20100166454A1
    • 2010-07-01
    • US12723148
    • 2010-03-12
    • Tomohito TaniguchiTakumi FurukawaHidekazu MatsudaYusuke Yagisawa
    • Tomohito TaniguchiTakumi FurukawaHidekazu MatsudaYusuke Yagisawa
    • G03G21/18G03G5/04G03G15/00
    • G03G15/0233Y10T428/25
    • Concerned with a charging member in the conductive surface layer of which the conductive particles are so kept from agglomerating as to make charging performance not easily change even where the surface layer expands and contracts repeatedly in various environments. The charging member is a charging member having a conductive substrate and formed on the substrate a conductive elastic layer and a conductive surface layer. The elastic layer contains a polymer having a unit coming from ethylene oxide, and the surface layer contains a binder resin and graphitized particles. The binder resin contains a resin having in the molecule a urethane linkage or a siloxane linkage, or a urethane linkage and a siloxane linkage, and the graphitized particles have a graphite (002) plane lattice spacing of from 0.3362 nm or more to 0.3449 nm or less.
    • 涉及导电表面层中的导电表面层中的充电构件,其导电颗粒被保持凝聚,使得即使在各种环境中表面层膨胀和重复收缩的情况下,充电性能也不容易改变。 充电构件是具有导电基板的充电构件,并且在基板上形成导电弹性层和导电表面层。 弹性层含有具有来自环氧乙烷的单元的聚合物,表面层含有粘结剂树脂和石墨化颗粒。 粘结剂树脂含有在分子中具有氨基甲酸酯键或硅氧烷键或氨基甲酸酯键和硅氧烷键的树脂,并且石墨化颗粒的石墨(002)面晶格间距为0.3362nm以上至0.3449nm以下,或 减。