会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 1. 发明授权
    • Hydroprocessing with self-promoted molybdenum and tungsten sulfide
catalyst
    • 用自身促进的钼和硫化钨催化剂进行加氢处理
    • US4705619A
    • 1987-11-10
    • US7765
    • 1987-01-28
    • Larry E. McCandlishTeh C. Ho
    • Larry E. McCandlishTeh C. Ho
    • B01J37/08C10G45/04C10G45/08C10G45/50C10G47/04C10G47/12
    • C10G45/04B01J37/086
    • Hydrocarbon feeds are upgraded by contacting same, at elevated temperature and in the presence of hydrogen, with a self-promoted catalyst prepared by heating one or more water soluble catalyst precursors in a non-oxidizing atmosphere in the presence of sulfur at a temperature of at least about 200.degree. C. The precursors will be one or more compounds of the formula ML(Mo.sub.y W.sub.1-y O.sub.4) wherein M is one or more promoter metals selected from the group consisting essentially of Mn, Fe, Co, Ni, Cu, Zn and mixtures thereof, wherein O.ltoreq.y.ltoreq.1 and wherein L is a nitrogen containing, neutral multidentate, chelating ligand. In a preferred embodiment the ligand L will comprise one or more chelating alkyl di or triamines and the non-oxidizing atmosphere and to form the catalyst will comprise H.sub.2 S.
    • 通过在升高的温度和在氢的存在下使其接触来提高烃进料与通过在硫的存在下在非氧化性气氛中在一定温度下加热一种或多种水溶性催化剂前体而制备的自促进催化剂 至少约200℃。前体将是一种或多种式ML(MoyW1-yO4)的化合物,其中M是一种或多种选自基本上由Mn,Fe,Co,Ni,Cu,Zn和 其混合物,其中O y为1,并且其中L为含氮中性多齿螯合配体。 在优选的实施方案中,配体L将包含一种或多种螯合烷基二或三胺,并且非氧化性气氛和形成催化剂将包含H 2 S。
    • 3. 发明授权
    • Hydrotreating with self-promoted molybdenum and tungsten sulfide catalyst
    • 用自身促进的钼和硫化钨催化剂加氢处理
    • US4663023A
    • 1987-05-05
    • US687579
    • 1984-12-28
    • Larry E. McCandlishTeh C. Ho
    • Larry E. McCandlishTeh C. Ho
    • C10G45/08B01J27/00B01J31/00B01J37/08C10G45/04C10G45/50C10G47/04C10G47/12
    • C10G45/04B01J37/086
    • Hydrocarbon feeds are upgraded by contacting same, at elevated temperature and in the presence of hydrogen, with a self-promoted catalyst prepared by heating one or more water soluble catalyst precursors in a non-oxidizing atmosphere in the presence of sulfur at a temperature of at least about 200.degree. C. The precursors will be one or more compounds of the formula ML(Mo.sub.y W.sub.1-y O.sub.4) wherein M is one or more promoter metals selected from the group consisting essentially of Mn, Fe, Co, Ni, Cu, Zn and mixtures thereof, wherein O.ltoreq.y.ltoreq.1 and wherein L is a nitrogen containing, neutral multidentate, chelating ligand. In a preferred embodiment the ligand L will comprise one or more chelating alkyl di or triamines and the non-oxidizing atmosphere and to form the catalyst will comprise H.sub.2 S.
    • 通过在升高的温度和在氢的存在下使其接触来提高烃进料与通过在硫的存在下在非氧化性气氛中在一定温度下加热一种或多种水溶性催化剂前体而制备的自促进催化剂 至少约200℃。前体将是一种或多种式ML(MoyW1-yO4)的化合物,其中M是一种或多种选自基本上由Mn,Fe,Co,Ni,Cu,Zn和 其混合物,其中O y为1,并且其中L为含氮中性多齿螯合配体。 在优选的实施方案中,配体L将包含一种或多种螯合烷基二或三胺,并且非氧化性气氛和形成催化剂将包含H 2 S。