    • A retardation film composed of a laminated film which comprises a layer A composed of a material having a positive intrinsic birefringence and a layer B composed of a material having a negative intrinsic birefringence; the retardation film has a stretching temperature Tα which causes delaying of a phase after the stretching to a phase before the stretching and a stretching temperature Tβ which causes hastening of a phase after the stretching to a phase before the stretching, in cases of uniaxially stretching in a direction of an X axis by draw ratio of 1.25, in which the phase is of linearly polarized light ΨX in relation to linearly polarized light ΨY, the X axis is an uniaxially stretching direction; and the retardation film satisfies 0.92 ≦R40/Re ≦1.08, wherein Re (nm) and R40 (nm) are retardation values of light having a wavelength of 550 nm.
    • 由包含由具有正的本征双折射的材料构成的层A和由具有负的固有双折射的材料构成的层B的层压膜构成的延迟膜; 延迟膜具有拉伸温度Tα,其使拉伸后的相位延迟到拉伸前的相位和拉伸温度T&bgr; 在拉伸后的相位拉伸至拉伸前的相位的情况下,在相对于线偏振光的相位为线偏振光ΨX的情况下,在X轴方向上以1.25的拉伸比进行单轴拉伸的情况下, ΨY,X轴是单轴拉伸方向; 并且相位差膜满足0.92≦̸ R40 / Re≦̸ 1.08,其中Re(nm)和R40(nm)是波长为550nm的光的延迟值。
    • 10. 发明授权
    • Phase difference plate manufacturing method, phase difference plate, and liquid crystal display device
    • 相差板制造方法,相差板和液晶显示装置
    • US09321227B2
    • 2016-04-26
    • US13820667
    • 2011-08-31
    • Taku HatanoKenichi Harai
    • Taku HatanoKenichi Harai
    • B29D11/00G02B5/30G02F1/1335G02F1/13363
    • B29D11/00644B29D11/00788B29L2009/00G02B5/3083G02F1/133528G02F1/13363G02F1/133634G02F2001/13356G02F2001/133638
    • A step of forming a layered body including a resin layer (a) containing a resin A having positive intrinsic birefringence and a resin layer (b) containing a resin B having negative intrinsic birefringence, the resin layer (b) being provided on one side of the resin layer (a); a first stretching step of stretching the layered body in one direction at a temperature T1; and a second stretching step of, after the first stretching step, stretching the layered body in another direction that is approximately orthogonal to the previous stretching direction at a temperature T2 which is lower than the temperature T1 to obtain a phase difference plate are performed. By these steps, a phase difference plate wherein a slow axis of the resin layer (a) after the stretching treatment and a slow axis of the resin layer (b) after the stretching treatment are approximately parallel to each other, and in-plane retardation Rea and NZ coefficient NZa in the resin layer (a) after the stretching treatment, and in-plane retardation Reb and NZ coefficient NZb in the resin layer (b) after the stretching treatment satisfy specific relationship is obtained.