    • Phase difference plate manufacturing method, phase difference plate, and liquid crystal display device
    • 相差板制造方法,相差板和液晶显示装置
    • US09321227B2
    • 2016-04-26
    • US13820667
    • 2011-08-31
    • Taku HatanoKenichi Harai
    • Taku HatanoKenichi Harai
    • B29D11/00G02B5/30G02F1/1335G02F1/13363
    • B29D11/00644B29D11/00788B29L2009/00G02B5/3083G02F1/133528G02F1/13363G02F1/133634G02F2001/13356G02F2001/133638
    • A step of forming a layered body including a resin layer (a) containing a resin A having positive intrinsic birefringence and a resin layer (b) containing a resin B having negative intrinsic birefringence, the resin layer (b) being provided on one side of the resin layer (a); a first stretching step of stretching the layered body in one direction at a temperature T1; and a second stretching step of, after the first stretching step, stretching the layered body in another direction that is approximately orthogonal to the previous stretching direction at a temperature T2 which is lower than the temperature T1 to obtain a phase difference plate are performed. By these steps, a phase difference plate wherein a slow axis of the resin layer (a) after the stretching treatment and a slow axis of the resin layer (b) after the stretching treatment are approximately parallel to each other, and in-plane retardation Rea and NZ coefficient NZa in the resin layer (a) after the stretching treatment, and in-plane retardation Reb and NZ coefficient NZb in the resin layer (b) after the stretching treatment satisfy specific relationship is obtained.
    • 形成包含含有具有正的固有双折射的树脂A的树脂层(a)和含有具有负的固有双折射的树脂B的树脂层(b)的层叠体的步骤,树脂层(b)设置在 树脂层(a); 第一拉伸步骤,在一个方向上以T1的温度拉伸层叠体; 以及第二拉伸步骤,在第一拉伸步骤之后,进行层叠体在与先前的拉伸方向近似正交的方向上,在低于温度T1的温度T2下拉伸,以获得相位差板。 通过这些工序,拉伸处理后的树脂层(a)的慢轴和拉伸处理后的树脂层(b)的慢轴大致平行的相位差板,面内延迟 拉伸处理后的树脂层(a)中的Rea和NZ系数NZa以及拉伸处理后的树脂层(b)中的面内相位差Reb和NZ系数NZb满足特定的关系。
    • 2. 发明授权
    • Wave plate, method for producing same, and liquid crystal display device
    • 波片,其制造方法和液晶显示装置
    • US09079350B2
    • 2015-07-14
    • US13389967
    • 2010-07-28
    • Taku HatanoKenichi Harai
    • Taku HatanoKenichi Harai
    • G02F1/1335B29C55/02B29C55/14G02B5/30G02F1/13363
    • B29C55/023B29C55/143B29K2995/0034G02B5/3083G02F1/13363
    • A phase difference plate is manufactured by a method including a step of forming a multilayer body by co-extruding or co-casting a resin A having a positive intrinsic birefringence value and a resin B having a negative intrinsic birefringence value, the multilayer body including a layer “a” containing the resin A and a layer “b” containing the resin B; a step of stretching the multilayer body at a temperature T1 in one direction; and a step of subsequently stretching the multilayer body at temperature T2 lower than the temperature T1 in a direction that is approximately orthogonal to the previous stretching direction. The resulting phase difference plate has specific in-plane retardation Rea of the layer “a”, retardation Rta in the thickness direction thereof, in-plane retardation Reb of the layer “b”, and retardation Rtb in the thickness direction thereof.
    • 通过包括通过共挤出或共铸具有正本征双折射值的树脂A和具有负的固有双折射值的树脂B来形成多层体的步骤的方法制造相差板,所述多层体包括 含有树脂A的层“a”和含有树脂B的层“b” 在一个方向上在温度T1下拉伸多层体的步骤; 以及在大致正交于前述拉伸方向的方向上随后在低于温度T1的温度T2下拉伸多层体的步骤。 所得到的相位差板具有层“a”的具体的面内相位差Rea,厚度方向的延迟量Rta,层“b”的面内相位差Reb,厚度方向的延迟量Rtb。
    • 3. 发明申请
    • PHASE DIFFERENCE PLATE MANUFACTURING METHOD, PHASE DIFFERENCE PLATE, AND LIQUID CRYSTAL DISPLAY DEVICE
    • 相差板制造方法,相位差板和液晶显示装置
    • US20130169910A1
    • 2013-07-04
    • US13820667
    • 2011-08-31
    • Taku HatanoKenichi Harai
    • Taku HatanoKenichi Harai
    • G02F1/1335
    • B29D11/00644B29D11/00788B29L2009/00G02B5/3083G02F1/133528G02F1/13363G02F1/133634G02F2001/13356G02F2001/133638
    • A step of forming a layered body including a resin layer (a) containing a resin A having positive intrinsic birefringence and a resin layer (b) containing a resin B having negative intrinsic birefringence, the resin layer (b) being provided on one side of the resin layer (a); a first stretching step of stretching the layered body in one direction at a temperature T1; and a second stretching step of, after the first stretching step, stretching the layered body in another direction that is approximately orthogonal to the previous stretching direction at a temperature T2 which is lower than the temperature T1 to obtain a phase difference plate are performed. By these steps, a phase difference plate wherein a slow axis of the resin layer (a) after the stretching treatment and a slow axis of the resin layer (b) after the stretching treatment are approximately parallel to each other, and in-plane retardation Rea and NZ coefficient NZa in the resin layer (a) after the stretching treatment, and in-plane retardation Reb and NZ coefficient NZb in the resin layer (b) after the stretching treatment satisfy specific relationship is obtained.
    • 形成包含含有具有正的固有双折射的树脂A的树脂层(a)和含有具有负的固有双折射的树脂B的树脂层(b)的层叠体的步骤,树脂层(b)设置在 树脂层(a); 第一拉伸步骤,在一个方向上以T1的温度拉伸层叠体; 以及第二拉伸步骤,在第一拉伸步骤之后,进行层叠体在与先前的拉伸方向近似正交的方向上,在低于温度T1的温度T2下拉伸,以获得相位差板。 通过这些工序,拉伸处理后的树脂层(a)的慢轴和拉伸处理后的树脂层(b)的慢轴大致平行的相位差板,面内延迟 拉伸处理后的树脂层(a)中的Rea和NZ系数NZa以及拉伸处理后的树脂层(b)中的面内相位差Reb和NZ系数NZb满足特定的关系。
    • 4. 发明申请
    • WAVE PLATE, METHOD FOR PRODUCING SAME, AND LIQUID CRYSTAL DISPLAY DEVICE
    • 波片,其制造方法和液晶显示装置
    • US20120140154A1
    • 2012-06-07
    • US13389967
    • 2010-07-28
    • Taku HatanoKenichi Harai
    • Taku HatanoKenichi Harai
    • G02F1/1335B29D11/00G02B27/28
    • B29C55/023B29C55/143B29K2995/0034G02B5/3083G02F1/13363
    • A phase difference plate is manufactured by a method including a step of forming a multilayer body by co-extruding or co-casting a resin A having a positive intrinsic birefringence value and a resin B having a negative intrinsic birefringence value, the multilayer body including a layer “a” containing the resin A and a layer “b” containing the resin B; a step of stretching the multilayer body at a temperature T1 in one direction; and a step of subsequently stretching the multilayer body at temperature T2 lower than the temperature T1 in a direction that is approximately orthogonal to the previous stretching direction. The resulting phase difference plate has specific in-plane retardation Rea of the layer “a”, retardation Rta in the thickness direction thereof, in-plane retardation Reb of the layer “b”, and retardation Rtb in the thickness direction thereof.
    • 通过包括通过共挤出或共铸具有正本征双折射值的树脂A和具有负的固有双折射值的树脂B来形成多层体的步骤的方法制造相差板,所述多层体包括 含有树脂A的层“a”和含有树脂B的层“b” 在一个方向上在温度T1下拉伸多层体的步骤; 以及在大致正交于前述拉伸方向的方向上随后在低于温度T1的温度T2下拉伸多层体的步骤。 所得到的相位差板具有层“a”的具体的面内延迟Rea,其厚度方向的延迟值Rta,层“b”的面内相位差Reb和厚度方向的延迟量Rtb。