    • 1. 发明专利
    • Insolubilization material of heavy metals, and insolubilization method of heavy metals
    • 重金属的不合金材料和重金属的非金属化方法
    • JP2012082330A
    • 2012-04-26
    • JP2010230280
    • 2010-10-13
    • Taiheiyo Cement Corp太平洋セメント株式会社
    • YANAGIYA SHOHEIMATSUYAMA YUSUKESANO SUSUMU
    • C09K3/00B01J20/06B01J20/08B09B3/00B09C1/02B09C1/08C02F1/28C02F11/00
    • PROBLEM TO BE SOLVED: To provide an insolubilization material of heavy metals, which can inhibit diffusion to the periphery of heavy metals to not only a heavy metal in the form of a cation but also to heavy metals in the form of an anion; and to provide an insolubilization method of heavy metals using the same.SOLUTION: The insolubilization material of heavy metals includes, based on 100 parts by mass of a base material: 0.1-50 parts by mass of light burned magnesia and/or a light burned magnesia partial hydrate; and 0.1-50 parts by mass of a layered double hydroxide and/or a fired product of a layered double hydroxide. In addition, the insolubilization method of heavy metals comprises laying a material to be treated containing heavy metals on a heavy metals insolubilization layer which has laid the insolubilization material of heavy metals in the shape of a layer.
    • 要解决的问题:提供重金属的不溶性材料,其可以抑制向重金属的外围扩散到不仅以阳离子形式的重金属,而且还可以以阴离子形式的重金属 ; 并提供使用其的重金属的不溶解方法。 解决方案:重金属的不溶化材料包括:基于100质量份的基质材料:0.1-50质量份的轻烧氧化镁和/或轻烧的氧化镁部分水合物; 和0.1-50质量份层状双氢氧化物和/或层状双氢氧化物的烧制品。 此外,重金属的不溶化方法包括在重金属不溶化层上铺设含有重金属的待处理材料,该重金属不溶解层将重金属的不溶解材料铺设成层的形状。 版权所有(C)2012,JPO&INPIT
    • 2. 发明专利
    • Solidification material and processing method of contaminated soil
    • 污染土壤的固体材料和加工方法
    • JP2014088521A
    • 2014-05-15
    • JP2012240267
    • 2012-10-31
    • Taiheiyo Cement Corp太平洋セメント株式会社
    • MATSUYAMA YUSUKENOZAKI TAKAHITOYANAGIYA SHOHEISUGIYAMA AKINORI
    • C09K17/02B09B3/00B09C1/00C09K103/00G21F9/28G21F9/30
    • PROBLEM TO BE SOLVED: To provide a solidification material excellent in penetrability to contaminated soil, generating less dust when the contaminated soil is scraped off, and easy to control scraping thickness, and provide a processing method of contaminated soil using the solidification material.SOLUTION: There is provided a solidification material containing magnesium oxide of 50 mass% or more, and having 7 μm or less of a particle diameter dwith a cumulative volume of 20%, 22 μm or less of a particle diameter dwith the cumulative volume of 50%, and 40 μm or less of a particle diameter dwith the cumulative volume of 80%, in the cumulative distribution of a particle size of the solidification material. Also there is provided a processing method of contaminated soil for removing the solidified contaminated soil by adding 1.5 to 3.0 kg of a slurry of the solidification material having a water/solidification material ratio (mass ratio) of 2.5 to 4.5 per 1 mof the contaminated soil in terms of magnesium oxide to solidify the contaminated soil.
    • 要解决的问题:提供一种对污染土壤渗透性优异的固化材料,在污染污垢被刮掉时产生较少的灰尘,易于控制刮除厚度,并提供使用固化材料的污染土壤的加工方法。 提供含有50质量%以上的氧化镁和7μm以下的粒径d的累积体积为20%,22μm以下的累积体积为50%的粒径d的凝固材料, 在凝固材料的粒径的累积分布中,累积体积为80%的粒径d为40μm以下。 还提供了一种污染土壤的处理方法,通过加入1.5至3.0kg每1摩尔的水/固化材料比(质量比)为2.5至4.5的固化材料的浆液,以将污染的土壤去除固化的污染土壤 以氧化镁为固化污染土壤。
    • 3. 发明专利
    • Method for removing heavy metal in wastewater
    • 在废水中去除重金属的方法
    • JP2011206692A
    • 2011-10-20
    • JP2010077295
    • 2010-03-30
    • Taiheiyo Cement Corp太平洋セメント株式会社
    • YANAGIYA SHOHEIHAYASHI HIROSHIMATSUYAMA YUSUKE
    • C02F1/28B01J20/04
    • PROBLEM TO BE SOLVED: To provide a method for removing a heavy metal in wastewater by using a heavy metal adsorbent excellent in filterability and heavy metal adsorbing performance.SOLUTION: In the method for removing a heavy metal in wastewater, the heavy metal adsorbent includes 100 pts.wt. of hydrotalcite, and 10-1,000 pts.wt. of a partial hydrate of light burned magnesia obtained by hydrating part of the light burned magnesia obtained by firing magnesium carbonate, magnesium hydroxide, or a mineral containing magnesium carbonate or magnesium hydroxide at 550-1,400°C. The heavy metal adsorbent is added to the wastewater in which the heavy metal is dissolved, and the mixture is stirred and then subjected to solid-liquid separation to recover the heavy metal adsorbent.
    • 要解决的问题:提供通过使用过滤性和重金属吸附性能优异的重金属吸附剂来除去废水中的重金属的方法。解决方案:在废水中除去重金属的方法中,重金属吸附剂包括100 重量份 的水滑石和10-1,000重量份 通过在550-1,400℃煅烧碳酸镁,氢氧化镁或含有碳酸镁或氢氧化镁的矿物而获得的部分轻烧氧化镁而获得的轻烧氧化镁的部分水合物。 将重金属吸附剂加入其中溶解重金属的废水中,搅拌混合物,然后进行固液分离以回收重金属吸附剂。
    • 5. 发明专利
    • Material for treating heavy metal or the like
    • 用于处理重金属或类似物的材料
    • JP2012177051A
    • 2012-09-13
    • JP2011041585
    • 2011-02-28
    • Taiheiyo Cement Corp太平洋セメント株式会社
    • YANAGIYA SHOHEIMATSUYAMA YUSUKESANO SUSUMUMORIYA MASAHIKOTAKANO HIROYUKI
    • C09K3/00B01J20/04B09B3/00B09C1/02B09C1/08C02F1/28C02F11/00
    • PROBLEM TO BE SOLVED: To provide a treating material which is excellent in elution suppressing effect such as a heavy metal or the like with a small addition, even if a contaminant of extremely high concentration is treated, and is capable of adjusting the pH of a treated product to 5.8-8.6.SOLUTION: A material for treating the heavy metal or the like contains 5-50 parts mass magnesias (B), which satisfy all of the following conditions (B1)-(B3), based on 100 parts mass of at least one water-soluble salt selected from metal sulfate and metal chloride. The condition (B1) is that the magnesia contains partially the magnesium hydroxide produced by partially hydrating a fired material, which is obtained by firing a solid material based on magnesium carbonate and/or magnesium hydroxide at 650-1,000°C and contains magnesium oxide; the condition (B2) is that the magnesia has 1.5-12.0 mass% ignition loss rate when measured at 1,000°C; and the condition (B3) is that the magnesia has ≤3.0 mass% calcium content in terms of CaO.
    • 待解决的问题:即使处理浓度极高的污染物,即使加入少量的重金属等,也能够提供洗脱抑制效果好的处理材料,能够调整 处理产品的pH值为5.8-8.6。 解决方案:用于处理重金属等的材料含有5-50份质量的氧化镁(B),其满足以下所有条件(B1) - (B3),基于100质量份的至少一种 选自金属硫酸盐和金属氯化物的水溶性盐。 条件(B1)是氧化镁部分含有通过部分水化烧制材料产生的氢氧化镁,其通过在650-1,000℃下煅烧基于碳酸镁和/或氢氧化镁的固体材料并含有氧化镁而获得; 条件(B2)是在1,000℃下测定时,氧化镁具有1.5-12.0质量%的灼烧损失率; 条件(B3)是以CaO计,钙含量≤3.0质量%。 版权所有(C)2012,JPO&INPIT
    • 6. 发明专利
    • 改良土の配合設計方法、セメント系固化材の製造方法、およびセメント系固化材
    • 水泥改性土组合物设计方法,水泥基固结材料和水泥基固结材料的制造方法
    • JP2014218856A
    • 2014-11-20
    • JP2013099781
    • 2013-05-10
    • 太平洋セメント株式会社Taiheiyo Cement Corp
    • YANAGIYA SHOHEIMATSUYAMA YUSUKESAKAMAKI KATSUYUKISUGIYAMA AKINORISUGAYA HIDEYUKI
    • E02D3/12C04B7/14C09K17/02C09K17/06C09K17/10
    • Y02P40/143
    • 【課題】改良土の最適な配合を容易に設計できる方法等を提供する。【解決手段】対象土の含水比、対象土中のビチューメン、フミン酸、フルボ酸、アロフェン、およびアロフェンを除く非晶質相の含有率に基づき算出した対象土の特性値と、改良土の目標強度に基づき、エーライト、石膏、および高炉スラグの配合量を算出して改良土の配合設計を行う、改良土の配合設計方法と、該改良土の配合設計方法により求めたエーライト、石膏、および高炉スラグの配合量に基づき、少なくとも、セメントクリンカー、および石膏を混合してセメント系固化材を製造するセメント系固化材の製造方法と、該固化材の製造方法を用いて製造してなるセメント系固化材である。【選択図】図2
    • 要解决的问题:提供能够容易地设计水泥改良土壤最佳混合的方法等。解决方案:提供了一种基于目标土壤特征值计算的水泥改良土壤组成设计方法 基于目标土壤,沥青,腐殖酸,富里酸,水杨醛和目标土壤中不含Allophane的非晶相含水量与水泥改良土壤的目标强度的比例,通过计算阿利石,石膏的混合量 和高炉渣; 基于通过水泥改良土壤的组成设计方法获得的阿利特,石膏和高炉矿渣的混合量,至少混合水泥熟料和石膏来制造水泥基固化材料的制造方法; 以及使用固化材料的制造方法制造的水泥基固化材料。
    • 7. 发明专利
    • 浚渫土の処理方法
    • JP2019001901A
    • 2019-01-10
    • JP2017117354
    • 2017-06-15
    • TAIHEIYO CEMENT CORPHYUUENSU KK
    • INOE KAZUSHIGEYANAGIYA SHOHEISHIDARA MORIYOSHI
    • C09K17/12E02F7/00
    • 【課題】固化処理後の改良された浚渫土からの有機物の溶出を抑制することができ、かつ、固化処理土の強度を確保しながら、固化処理土の過度の硬化および強アルカリ性化を防ぐことができる浚渫土の処理方法を提供する。【解決手段】浚渫土からの有機物の溶出を抑制するための浚渫土の処理方法であって、上記浚渫土中の有機物の含有率を測定する有機物量測定工程と、上記有機物の含有率が、予め定めた特定の値以下である場合、上記浚渫土にケイ酸カルシウム含有粉粒状物を添加して混合し、かつ、オゾン処理を行わずに、改良された浚渫土を得て、上記有機物の含有率が、上記予め定めた特定の値を超える場合、上記浚渫土にケイ酸カルシウム含有粉粒状物を添加して混合し、次いで、水を加えて含水比を高めた後に、オゾン処理を行って、改良された浚渫土を得る浚渫土改良工程、を含む浚渫土の処理方法。【選択図】なし