    • IMPROVED EXPANDABLE AND EXPANDED ALKENYL AROMATIC POLYMER PARTICLES AND METHODS OF MAKING THE SAME
    • 改进的可膨胀和膨胀的亚苄基芳族聚合物颗粒及其制备方法
    • WO1990002151A1
    • 1990-03-08
    • PCT/US1989002576
    • 1989-06-13
    • THE DOW CHEMICAL COMPANY
    • THE DOW CHEMICAL COMPANYTUSIM, Martin, H.
    • C08J09/16
    • C08J9/0023C08J2325/00
    • The present invention relates to expandable and expanded alkenyl aromatic polymer particles having the ability to use a decreased amount of blowing agent to produce an expanded alkenyl aromatic polymer particle of an equivalent bulk density or the same amount of blowing agent to produce an expanded alkenyl aromatic polymer particle having a decreased bulk density by including a density modifier in the expandable alkenyl aromatic polymer particle in an amount of about 0.005 to 0.5 weight percent by weight of the total mixture. Also included as part of the invention are methods of making the expandable and expanded alkenyl aromatic polymer particles wherein the expandable and expanded alkenyl aromatic polymer particles have a density modifier included in an amount of about 0.005 percent to about 0.5 weight percent by weight of the total mixture.
    • 本发明涉及可膨胀和膨胀的链烯基芳族聚合物颗粒,其具有使用减少量的发泡剂以产生等效堆积密度的膨胀的烯基芳族聚合物颗粒或相同量的发泡剂以产生膨胀的链烯基芳族聚合物 通过在可膨胀的链烯基芳族聚合物颗粒中包含以总混合物的重量计为约0.005至0.5重量%的量的密度调节剂来减小堆积密度的颗粒。 作为本发明的一部分还包括制备可膨胀和膨胀的链烯基芳族聚合物颗粒的方法,其中可膨胀和膨化的链烯基芳族聚合物颗粒具有包含的密度调节剂,其量为总重量的约0.005重量%至约0.5重量% 混合物。
    • 2. 发明申请
    • ETHYLENE POLYMER FOAMS BLOWN WITH 1,1-DIFLUOROETHANE AND METHOD OF MAKING SAME
    • 用1,1-二氟乙烯吹制的乙烯聚合物粉末及其制备方法
    • WO1994025255A1
    • 1994-11-10
    • PCT/US1994003309
    • 1994-03-25
    • THE DOW CHEMICAL COMPANY
    • THE DOW CHEMICAL COMPANYTUSIM, Martin, H.PARK, Chung, P.MALONE, Bruce, A.
    • B29C67/22
    • C08J9/149C08J2323/02
    • Disclosed are processes for making olefin polymer foam structures with 1,1-difluoroethane (HFC-152a). One foam structure is comprised of an ethylene polymer material, and is blown with a mixture of isobutane and 1,1-difluoroethane. Another foam structure has a cross section of 2 or more inches (5 or more centimeters) in one dimension and 18 or more inches (46 or more centimeters) in the other dimension, and is blown with 75 mole percent or more HFC-152a. Another foam structure is in coalesced strand form with a density of 16 to 48 kilograms per cubic meter, and is blown with a first blowing agent of 20 to 90 mole percent 1,1-difluoroethane and 80 to 10 mole percent of a second blowing agent selected from isobutane, n-butane, and propane.
    • 公开了制备具有1,1-二氟乙烷(HFC-152a)的烯烃聚合物泡沫结构的方法。 一种泡沫结构由乙烯聚合物材料组成,并用异丁烷和1,1-二氟乙烷的混合物吹制。 另一种泡沫结构在一个维度上具有2或更多英寸(5厘米或更多厘米)的横截面,在另一个尺寸上具有18英寸(46厘米或更多厘米)的横截面,并且用75摩尔%或更多的HFC-152a吹制。 另一种泡沫结构是聚结的链形式,密度为16至48千克/立方米,并且用20至90摩尔%的1,1-二氟乙烷的第一发泡剂和80至10摩尔%的第二发泡剂 选自异丁烷,正丁烷和丙烷。