    • 6. 发明授权
    • Hot-rolled steel sheet and method for forming hot-rolled steel sheet
having low yield ratio, high strength and excellent toughness
    • 热轧钢板和成品率低,强度高,韧性优异的热轧钢板的制造方法
    • US5948183A
    • 1999-09-07
    • US947388
    • 1997-10-08
    • Susumu OkadaMasahiko MoritaFumimaru Kawabata
    • Susumu OkadaMasahiko MoritaFumimaru Kawabata
    • C21D8/02C22C38/02C22C38/04C22C38/12C22C38/14
    • C22C38/04C21D8/0226C22C38/02C22C38/12C22C38/14C21D2211/002C21D2211/005
    • The present invention provides a hot-rolled steel sheet having a low yield ratio, a high specific strength, and excellent toughness. The hot-rolled steel sheet comprises: 0.005 to less than 0.030 weight percent of carbon, 1.5 weight percent or less of silicon, 1.5 weight percent or less of manganese, 0.020 weight percent or less of phosphorus, 0.015 weight percent or less of sulfur, 0.005 to 0.10 weight percent of aluminum, 0.0100 weight percent or less of nitrogen, 0.0002 to 0.0100 weight percent of boron, at least one element selected from the group consisting of 0.20 weight percent or less of titanium and 0.25 weight percent or less of niobium in an amount to satisfy (Ti+Nb/2)/C.gtoreq.4, and balance iron and incidental impurities. The metal structure is selected from the group consisting of ferrite and bainitic ferrite. The amount of carbon dissolved in grains ranges from 1.0 to 4.0 ppm. The present invention also provides a method for producing a hot-rolled steel sheet. The method includes hot-rolling a steel slab containing the above components, cooling at a rate of between 5 to not more than 20.degree. C./sec., and then coiling at a temperature ranging from over 550.degree. C. to 700.degree. C.
    • 本发明提供一种低屈服比,高比强度,优异的韧性的热轧钢板。 该热轧钢板包括:0.005〜小于0.030重量%的碳,1.5重量%以下的硅,1.5重量%以下的锰,0.020重量%以下的磷,0.015重量%以下的硫, 0.005〜0.10重量%的铝,0.0100重量%以下的氮,0.0002〜0.0100重量%的硼,至少一种选自钛的0.20重量%以下和0.25重量%以下的铌的元素 满足(Ti + Nb / 2)/ C> / = 4的量,并平衡铁和杂质。 金属结构选自铁素体和贝氏体铁素体。 溶解在谷物中的碳的量为1.0至4.0ppm。 本发明还提供一种热轧钢板的制造方法。 该方法包括对含有上述成分的钢板进行热轧,以不超过20℃/秒的速度冷却,然后在550℃〜700℃的温度下卷取 。
    • 8. 发明申请
    • IMAGE SENSING APPARATUS HAVING ELECTRONIC ZOOM FUNCTION, AND CONTROL METHOD THEREFOR
    • 具有电子变焦功能的图像感应装置及其控制方法
    • US20070296837A1
    • 2007-12-27
    • US11754448
    • 2007-05-29
    • Masahiko Morita
    • Masahiko Morita
    • H04N5/262
    • H04N5/3454H04N5/232H04N5/23245H04N5/23296H04N5/2628
    • In an image sensing apparatus having an image sensing element that senses an object and outputs image data and an electronic zoom function, either a first processing mode or a second processing mode is set and an angle of view is designated. In the first processing mode, the image sensing element is driven by switching reading regions and reading methods of image data from the image sensing element based on the designated angle of view and the image data is read, processed, and the angle of view determined by the switched reading region is changed to the designated angle of view. In the second processing mode, the reading region and the reading method of the image data are fixed and the image data output from the image sensing element is processed, and the angle of view determined by the fixed reading region changed to the designated angle of view.
    • 在具有感测对象的图像感测元件并输出图像数据和电子变焦功能的图像感测装置中,设置第一处理模式或第二处理模式,并且指定视角。 在第一处理模式中,通过基于指定的视角切换读取区域和从图像感测元件读取图像数据的方法来驱动图像感测元件,并且读取,处理图像数据,并且由 切换读取区域改变为指定的视角。 在第二处理模式中,图像数据的读取区域和读取方法是固定的,并且处理从图像感测元件输出的图像数据,并且由固定读取区域确定的视角改变为指定的视角 。