    • Non-aqueous electrolyte battery and method of manufacturing the same
    • 非水电解质电池及其制造方法
    • US07261976B2
    • 2007-08-28
    • US10439807
    • 2003-05-16
    • Satoshi MizutaniHiroshi InoueTakatomo NishinoAtsuo Omaru
    • Satoshi MizutaniHiroshi InoueTakatomo NishinoAtsuo Omaru
    • H01M4/58H01M4/82
    • H01M4/133H01M4/0404H01M4/0452H01M4/134H01M4/1393H01M4/1395H01M4/364H01M10/052H01M10/0525H01M10/0585H01M2004/021Y10T29/49115
    • The battery comprises a positive electrode which has a positive electrode active material compound layer containing a positive electrode active material formed on a positive electrode current collector; a negative electrode which has at least one negative electrode thin film layer and at least one negative electrode active material compound layer, on a negative electrode current collector, and a non-aqueous electrolyte containing an electrolyte salt. The negative electrode thin film layer contains at least one Group 14 element, and is formed by a thin-film formation technology, and the negative electrode active material compound layer contains a binder and a negative electrode active material, which contains at least any one of Sn, Si, Sn compound, Si compound and carbonaceous material. With this negative electrode, the negative electrode thin film layer containing a high-capacity Group 14 element raises the battery capacity, and the negative electrode active material compound layer provides excellent charge/discharge cycle characteristics while suppressing degradation of the negative electrode even under repetitive charge/discharge.
    • 该电池包括正电极,该正极具有包含在正极集电体上形成的正极活性物质的正极活性物质化合物层; 在负极集电体上具有至少一个负极薄膜层和至少一个负极活性物质化合物层的负极和含有电解质盐的非水电解质。 负极薄膜层含有至少一个第14族元素,通过薄膜形成技术形成,负极活性物质化合物层含有粘合剂和负极活性物质,其含有至少任一种 Sn,Si,Sn化合物,Si化合物和碳质材料。 对于该负极,含有高容量组14元素的负极薄膜层提高了电池容量,负极活性物质化合物层即使在重复充电的同时也能够抑制负极的劣化的同时提供优异的充放电循环特性 /卸货。