    • STRENGTHENED IRON CATALYST FOR SLURRY REACTORS
    • 加强型浆料反应器用铁催化剂
    • WO2009032701A2
    • 2009-03-12
    • PCT/US2008/074484
    • 2008-08-27
    • RENTECH, INC.BENHAM, Charles, B.FRAENKEL, DanBLEY, Richard, A.TAYLOR, Jesse, W.DEMIREL, BelmaROLFE, Sara, L.WRIGHT, Harold, A.
    • DEMIREL, BelmaROLFE, Sara, L.WRIGHT, Harold, A.
    • B01J23/78C07C27/06
    • B01J23/78B01J21/005B01J21/08B01J37/03C10G2/331C10G2300/70
    • A method of strengthening a precipitated unsupported iron catalyst by: preparing a precipitated unsupported iron catalyst containing copper and potassium; adding a solution comprising a structural promoter to the previously prepared catalyst; drying the mixture; and calcining the dried catalyst. A method for preparing an iron catalyst, the method comprising: precipitating a catalyst precursor comprising iron phases selected from hydroxides, oxides, and carbonates; adding a promoter to the catalyst precursor to yield a promoted precursor; drying the promoted precursor to yield dried catalyst; and calcining the dried catalyst, wherein the catalyst further comprises copper and potassium. A method of preparing a strengthened precipitated iron catalyst comprising: co-precipitating iron, copper, magnesium, and aluminum; washing the precipitate; alkalizing the precipitate; and drying the precipitate to yield a dried catalyst precursor. The dried catalyst precursor may be calcined and treated with a gas comprising carbon monoxide.
    • 通过以下步骤强化沉淀的无载体铁催化剂的方法:制备沉淀的含铜和钾的无载体铁催化剂; 将包含结构助催化剂的溶液加入到先前制备的催化剂中; 干燥混合物; 并煅烧干燥的催化剂。 一种制备铁催化剂的方法,所述方法包括:使包含选自氢氧化物,氧化物和碳酸盐的铁相的催化剂前体沉淀; 向催化剂前体添加促进剂以产生促进的前体; 干燥促进的前体以产生干燥的催化剂; 并煅烧该干燥的催化剂,其中该催化剂还包含铜和钾。 一种制备强化沉淀铁催化剂的方法,包括:共沉淀铁,铜,镁和铝; 洗涤沉淀物; 碱化沉淀物; 并干燥沉淀物得到干燥的催化剂前体。 干燥的催化剂前体可以煅烧并用包含一氧化碳的气体处理。