    • 1. 发明申请
    • PROCESS FOR MANUFACTURE OF A CARBOXY TERMINATED DENDRITIC POLYESTER
    • 羧酸封端聚酯的制备方法
    • WO2002066541A1
    • 2002-08-29
    • PCT/SE2002/000263
    • 2002-02-15
    • PERSTORP SPECIALTY CHEMICALS ABPETTERSSON, BoBJÖRNBERG, Håkan
    • PETTERSSON, BoBJÖRNBERG, Håkan
    • C08G83/00
    • C08G83/003C08G63/20C09D163/00C08L2666/18
    • A method for production of a carboxy terminated dendritic polyester is disclosed. Said process comprises ring opening addition of at least one anhydride of a di, tri or polyfunctional aromatic and/or cycloaliphatic carboxylic acid to at least one hydroxy functional dendritic polyester having a hydroxyl value of at least 50 mg KOH/g. Said ring opening addition is performed at a molar ratio said anhydride to hydroxyl groups of between 0.2 to 1 and 1 to 1 and at a reaction temperature of 130-150 °C. Yielded carboxy terminated dendritic polyester has a glass transition temperature of at least 35 °C. The invention relates in further aspects to a powder coating composition comprising the carboxy terminated dendritic polyester obtainable by said process and the use of said carboxy terminated dendritic polyester in a resin composition.
    • 公开了一种制备羧基封端的树枝状聚酯的方法。 所述方法包括向至少一种羟基值为至少50mg KOH / g的至少一种羟基官能树枝状聚酯开环加成二,三或多官能芳族和/或脂环族羧酸的至少一种酸酐。 所述开环加成以所述酸酐与羟基的摩尔比为0.2-1:1-1和130-150℃的反应温度进行。得到的羧基封端的树枝状聚酯具有至少35的玻璃化转变温度 本发明在另外的方面涉及一种粉末涂料组合物,其包含可通过所述方法获得的羧基封端的树枝状聚酯和所述羧基封端的树枝状聚酯在树脂组合物中的用途。
    • 3. 发明申请
    • AIR DRYING WATERBORNE RESIN COMPOSITION
    • 空气干燥水性树脂组合物
    • WO2004037928A1
    • 2004-05-06
    • PCT/SE2003/001605
    • 2003-10-16
    • PERSTORP SPECIALTY CHEMICALS ABHÄGGMAN, BoBJÖRNBERG, HåkanMIDELF, BirgerJAMES, David, B.
    • HÄGGMAN, BoBJÖRNBERG, HåkanMIDELF, BirgerJAMES, David, B.
    • C08L101/00
    • C08L101/005C09D201/005C08L2666/14
    • An air drying waterborne resin composition is disclosed. Said resin composition comprises at least one amphiphilic air drying dendritic polymer, at least one non-amphiphilic air drying alkyd resin, at least one drier initiating and/or promoting autoxidation, and water, and optionally at least one anionic and/or nonionic surfactant, and/or at least one coalescent agent. Said at least one amphiphilic air drying dendritic polymer is built up from a polyhydric dendritic core polymer having terminal hydroxyl groups and at least one unsaturated carboxylic acid and at least one adduct, obtainable by addition of a monoalkylated polyethylene glycol to a dicarboxylic acid or anhydride and/or a diisocyanate, each bonded to at least one terminal hydroxyl group in said polyhydric dendritic core polymer.
    • 公开了一种空气干燥水性树脂组合物。 所述树脂组合物包含至少一种两亲空气干燥树枝状聚合物,至少一种非两亲空气干燥醇酸树脂,至少一种引发和/或促进自动氧化的干燥剂,以及任选至少一种阴离子和/或非离子表面活性剂, 和/或至少一种聚结剂。 所述至少一种两亲空气干燥树枝状聚合物由具有末端羟基和至少一种不饱和羧酸的多元树枝状核聚合物和至少一种加合物构成,所述加成物可通过将二烷基化聚乙二醇加入到二羧酸或酸酐中而得到, /或二异氰酸酯,各自与所述多元树枝状核聚合物中的至少一个末端羟基键合。