会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 3. 发明专利
    • Low-chromium-containing stainless steel superior in corrosion resistance at welded part
    • 焊接部件耐腐蚀性低含铬不锈钢超导体
    • JP2011174122A
    • 2011-09-08
    • JP2010038030
    • 2010-02-24
    • Nippon Steel & Sumikin Stainless Steel Corp新日鐵住金ステンレス株式会社
    • TERAOKA SHINICHISAKAMOTO TOSHIHARUFUKAYA MASUHIRO
    • C22C38/00B21B3/02C21D8/02C21D9/46C22C38/50
    • C21D9/50C21D8/0205C21D8/0273C21D2211/005C21D2211/008C22C38/001C22C38/02C22C38/04C22C38/06C22C38/42C22C38/46C22C38/50
    • PROBLEM TO BE SOLVED: To provide the most suitable low-chromium-containing stainless steel which prevents the degradation of corrosion resistance at a welded part when the low-chromium-containing stainless steel that uses martensitic transformation has been repeatedly welded (multipath), is superior in grain-boundary corrosion resistance at the welded part even under a severe corrosive environment, at the same time, does not cause preferential corrosion at a portion adjacent to a bonded part in a heat-affected zone, and further is superior in manufacture efficiency. SOLUTION: The low-chromium-containing stainless steel includes, by mass%, 0.015-0.025% C, 0.008-0.014% N, 0.2-1.0% Si, 1.0-1.5 Mn, 0.04% or less P, 0.03% or less S, 10-13% Cr, 0.2-1.5% Ni, 0.005-0.1% Al, further Ti of 6×(C%+N%) or more but 0.25% or less, and the balance Fe with unavoidable impurities, while controlling the content of each element so as to satisfy expression (A): γp=420×C%+470×N%+23×Ni%+9×Cu%+7×Mn%-11.5×Cr%-11.5×Si%-12×Mo%-23×V%-47×Nb%-49×Ti%-52×Al%+189≥80% and expression (B): Ti%×N% COPYRIGHT: (C)2011,JPO&INPIT
    • 要解决的问题:为了提供最适合的低含铬不锈钢,当使用马氏体转变的低含铬不锈钢已被反复焊接时,可防止焊接部件的耐腐蚀性降低(多径 ),即使在严酷的腐蚀环境下,焊接部的晶界耐腐蚀性也优异,同时在热影响区附近的接合部附近也不会产生优先的腐蚀, 在制造效率。 解决方案:低铬含量的不锈钢以质量%计含有0.015-0.025%C,0.008-0.014%N,0.2-1.0%Si,1.0-1.5Mn,0.04%以下的P,0.03% 或更少的S,10-13%的Cr,0.2-1.5%的Ni,0.005-0.1%的Al,另外的Ti为6×(C%+ N%)或更高但是0.25%以下,余量为Fe,不可避免的杂质, 同时控制各元素的含量以满足表达式(A):γp= 420×C%+ 470×N%+ 23×Ni%+ 9×Cu%+ 7×Mn%-11.5×Cr%-11.5× Si%-12×Mo%-23×V%-47×Nb%-49×Ti%-52×Al%+189≥80%,(B):Ti%×N%<0.003; 并且在热影响区由于多路径焊接而具有优异的耐晶界腐蚀性,并且在与热影响区的接合部分相邻的部分具有优良的耐腐蚀性。 版权所有(C)2011,JPO&INPIT
    • 4. 发明专利
    • Martensitic stainless steel having excellent corrosion resistance
    • 具有优异耐腐蚀性的马氏体不锈钢
    • JP2010215995A
    • 2010-09-30
    • JP2009067136
    • 2009-03-19
    • Nippon Steel & Sumikin Stainless Steel Corp新日鐵住金ステンレス株式会社
    • TERAOKA SHINICHISAKAMOTO TOSHIHARU
    • C22C38/00C21D8/02C21D9/46C22C38/58
    • PROBLEM TO BE SOLVED: To provide a martensitic stainless steel sheet which has excellent corrosion resistance, at a low cost.
      SOLUTION: The martensitic stainless steel having excellent corrosion resistance has a steel composition comprising, by mass, 0.03 to 0.25% C, 0.25 to 0.60% Si, ≤2.00% Mn, ≤0.035% P, ≤0.01% S, 11.0 to 15.5% Cr, ≤0.60% Ni, ≤0.80% Cu, 0.03 to 0.15% Sn, ≤0.060% V, ≤0.03% Al and 0.01 to 0.08% N, and the balance Fe with inevitable impurities, wherein the range of Sn and N satisfies a following inequality (A), and whose hardness is 300 to 600 HV by quenching or quenching and tempering: inequality (A) MCI=0.0016-(0.65Sn-0.059)
      2 +(N-0.050)
      2 ≥0.0 where, Sn and N are mass%.
      COPYRIGHT: (C)2010,JPO&INPIT
    • 要解决的问题:以低成本提供耐腐蚀性优异的马氏体不锈钢板。 解决方案:具有优异耐腐蚀性的马氏体不锈钢具有质量含有0.03-0.25%C,0.25-0.60%Si,≤2.00%Mn,≤0.035%P,≤0.01%S,11.0%的钢组成 至15.5%的Cr,≤0.60%的Ni,≤0.80%的Cu,0.03-0.15%的Sn,≤0.060%的V,≤0.03%的Al和0.01到0.08%的N,余量为Fe与不可避免的杂质,其中Sn的范围 并且N满足以下不等式(A),通过淬火或淬火回火,其硬度为300〜600HV:不等式(A)MCI = 0.0016-(0.65Sn-0.059) 2 + -0.050) 2 ≥0.0其中,Sn和N为质量%。 版权所有(C)2010,JPO&INPIT
    • 5. 发明专利
    • Martensitic stainless steel for disc brake
    • 用于碟形刹车的MARTENSITIC不锈钢
    • JP2010106315A
    • 2010-05-13
    • JP2008279238
    • 2008-10-30
    • Nippon Steel & Sumikin Stainless Steel Corp新日鐵住金ステンレス株式会社
    • TERAOKA SHINICHIITO TSUTOMUKOYAMA YUJI
    • C22C38/00C22C38/42C22C38/50
    • PROBLEM TO BE SOLVED: To provide such a component composition as to impart all of rust resistance, toughness, resistance to softening due to heat caused by braking and productivity, in a martensitic stainless steel for a disc brake in a two-wheeled vehicle to be used in as-quenched state.
      SOLUTION: The martensitic stainless steel for the disk brake comprises, by mass%, 0.025-0.055% C, 0.040-0.060% N, 0.25-0.45% Si, 1.0-1.5% Mn, 0.3% or less Ni, 11.5-13.5% Cr, 0.3-0.8% Cu, 0.001-0.010% Al and the balance Fe with unavoidable impurities, while satisfying the expressions: C+0.8×N: 0.055-0.080% and C/N=0.6-1.2, and while controlling γp expressed by the expression: γp=420[%C]+470[%N]+23[%Ni]+9[%Cu]+7[Mn]-11.5[%Cr]-11.5[%Si]-52[%AL]+189 to 85 to less than 100; and has a hardness of 32-38 by HRC after having been quenched.
      COPYRIGHT: (C)2010,JPO&INPIT
    • 要解决的问题:为了提供这样一种组成成分,用于赋予两轮盘式制动用马氏体不锈钢中所有的防锈性,韧性,由于制动产生的热而产生的软化的耐软化性和生产率 车辆在淬火状态下使用。 解决方案:用于盘式制动器的马氏体不锈钢以质量%计含有0.025-0.055%C,0.040-0.060%N,0.25-0.45%Si,1.0-1.5%Mn,0.3%或更少的Ni,11.5 -13.5%Cr,0.3-0.8%Cu,0.001-0.010%Al,余量为Fe和不可避免的杂质,同时满足以下表达式:C + 0.8×N:0.055-0.080%,C / N = 0.6-1.2,而 控制由以下表达式表示的γp:γp= 420 [%C] +470 [%N] +23 [%Ni] +9 [%Cu] +7 [Mn] -11.5 [%Cr] -11.5 [%Si] 52 [%AL] +189〜85〜小于100; 淬火后HRC的硬度为32-38。 版权所有(C)2010,JPO&INPIT
    • 9. 发明专利
    • Chromium-plated stainless steel sheet superior in corrosion resistance after having been worked
    • 镀铬不锈钢板耐腐蚀性高于工作时间
    • JP2010209458A
    • 2010-09-24
    • JP2009172590
    • 2009-07-24
    • Nippon Steel & Sumikin Stainless Steel Corp新日鐵住金ステンレス株式会社
    • SAKAMOTO TOSHIHARUTERAOKA SHINICHI
    • C25D5/26
    • PROBLEM TO BE SOLVED: To provide a chromium-plated stainless steel sheet superior in corrosion resistance after having been worked. SOLUTION: The chromium-plated stainless steel sheet superior in corrosion resistance after having been worked has a corrosion prevention layer containing an outer layer of a hydration chromium oxide layer and an inner layer of a metallic chromium layer, on the surface of a substrate of a stainless steel sheet containing 10.5-30.0 mass% Cr. The corrosion prevention layer has a thickness of 0.01-0.10 μm, and preferably has such corrosion resistance that a cathode current density measured in a 3.5% NaCl solution at 30°C, which is in a state of being opened to the atmospheric air, is 2.5 μA/cm 2 or less in such a condition that the electric potential is -0.6 V with respect to a silver/silver chloride standard electrode. COPYRIGHT: (C)2010,JPO&INPIT
    • 要解决的问题:提供加工后耐腐蚀性优异的镀铬不锈钢板。 解决方案:加工后的耐腐蚀性优异的镀铬不锈钢板在其表面上具有包含水合氧化铬层外层和金属铬层内层的防腐蚀层 含有10.5〜30.0质量%Cr的不锈钢板的基材。 防腐蚀层的厚度为0.01-0.10μm,优选具有这样的耐腐蚀性,即在处于大气中的状态下在30℃的3.5%NaCl溶液中测量的阴极电流密度为 在相对于银/氯化银标准电极的电位为-0.6V的条件下,为2.5μA/ cm 2 / SP以下。 版权所有(C)2010,JPO&INPIT
    • 10. 发明专利
    • Mo SAVING TYPE FERRITIC STAINLESS STEEL FOR AUTOMOTIVE EXHAUST SYSTEM MEMBER HAVING EXCELLENT CORROSION RESISTANCE AFTER HEATING
    • 用于汽车排气系统的Mo保存型不锈钢在加热后具有优异的耐腐蚀性
    • JP2010116619A
    • 2010-05-27
    • JP2008292091
    • 2008-11-14
    • Nippon Steel & Sumikin Stainless Steel Corp新日鐵住金ステンレス株式会社
    • SAKAMOTO TOSHIHARUTERAOKA SHINICHIHIRAIDE NOBUHIKO
    • C22C38/00C22C38/28C22C38/60F01N13/16
    • PROBLEM TO BE SOLVED: To provide an Mo saving type ferritic stainless steel for an automotive exhaust system member which can obtain corrosion resistance after heating and workability equal to or above those of SUS436J1L (17Cr-0.5Mo series) without comprising Mo. SOLUTION: The Mo saving type ferritic stainless steel for an automotive exhaust system member having excellent corrosion resistance after heating has a composition comprising, by mass, ≤0.015% C, 0.10 to 0.50% Si, 0.05 to 0.50% Mn, ≤0.050% P, ≤0.0100% S, ≤0.015% N, 0.010 to 0.100% Al and 16.5 to 22.5% Cr, further comprising one or two kinds selected from 0.03 to 0.30% Ti and 0.03 to 0.30% Nb, further comprising one or more kinds selected from 0.05 to 1.00% Sn and 0.05 to 1.00% Sb, and, if required, further comprising one or more kinds selected from 0.05 to 0.50% Cu, 0.05 to 0.50% Ni and 0.0005 to 0.0050% B. COPYRIGHT: (C)2010,JPO&INPIT
    • 要解决的问题:提供一种用于汽车排气系统构件的Mo节约型铁素体不锈钢,其可以获得等于或高于不含Mo的SUS436J1L(17Cr-0.5Mo系列)的加热后的耐腐蚀性。 &lt; P&gt;解决方案:加热后耐腐蚀性优异的汽车用排气系统部件用Mo型铁素体系不锈钢,其组成为:质量%≤0.15%,Si:0.10〜0.50%,Mn:0.05〜0.50% 0.050%P,≤0.0100%S,≤0.015%N,0.010〜0.100%Al和16.5〜22.5%Cr,还含有选自0.03〜0.30%Ti和0.03〜0.30%Nb中的一种或两种,还包含一种或 选自0.05〜1.00%的Sn和0.05〜1.00%的Sb的多种,如果需要,还可以含有选自0.05〜0.50%的Cu,0.05〜0.50%的Ni和0.0005〜0.0050%的一种或多种。 版权所有(C)2010,JPO&INPIT