    • 1. 发明专利
    • Diaphragm, manufacturing method thereof, and speaker device
    • 透镜,其制造方法和扬声器装置
    • JP2005223807A
    • 2005-08-18
    • JP2004031840
    • 2004-02-09
    • Mogami Denki CorpPioneer Electronic CorpTohoku Pioneer Corpパイオニア株式会社最上電機株式会社東北パイオニア株式会社
    • KAWADA KAZUHARUSEKIKAWA HIDEOAIZAWA SHINICHI
    • D21J3/02H04R7/02H04R7/14H04R9/06H04R31/00
    • PROBLEM TO BE SOLVED: To provide a diaphragm which is easily manufactured and has satisfactory characteristics.
      SOLUTION: At least any one kind of fiber material of wooden pulp, chemical fiber and inorganic fiber, a foaming agent and a fine fiber-like binding material of high beating degree are blended as necessary to prepare a paper making material and make paper. A molded object after paper making is attached in the inside of the die of a drying apparatus having a gap corresponding to the shape of a diaphragm 400, and the object is heated and dried so that one part of a vibrating portion 420 becomes thick, thereby forming a foaming thick portion 421 and a non-foaming portion 422. By improvement in bending rigidity by thickness by foaming and improvement in strength by tangling of fibers by fine fiber-like binding material, the diaphragm can be partially reinforced in a state of even weight by preventing increase in weight without reinforcement such as lamination of a different sheet-like member or impregnation of a composite resin, and frequency characteristic is flattened and satisfactory acoustic characteristic can be obtained.
      COPYRIGHT: (C)2005,JPO&NCIPI
    • 要解决的问题:提供容易制造且具有令人满意的特性的隔膜。 解决方案:根据需要,可以混合至少任意一种木浆,化纤,无机纤维的纤维材料,发泡剂和高打浆度的细纤维状粘结材料,以制备造纸材料并制成 纸。 造纸后的成型体被安装在具有对应于隔膜400的形状的间隙的干燥装置的管芯的内部,并且被加热干燥,使得振动部分420的一部分变厚 形成发泡厚部421和非发泡部422.通过发泡的弯曲刚度提高,通过细纤维状粘结材料使纤维的缠结提高强度,隔膜可以部分地被加强成均匀的状态 通过防止增加重量而不增加诸如不同片状构件的层压或复合树脂的浸渍的重量,并且频率特性变平坦,并且可以获得令人满意的声学特性。 版权所有(C)2005,JPO&NCIPI
    • 2. 发明专利
    • Diaphragm, manufacturing method thereof, and speaker device
    • 透镜,其制造方法和扬声器装置
    • JP2005223806A
    • 2005-08-18
    • JP2004031838
    • 2004-02-09
    • Mogami Denki CorpPioneer Electronic CorpTohoku Pioneer Corpパイオニア株式会社最上電機株式会社東北パイオニア株式会社
    • KAWADA KAZUHARUTAKAHASHI SHINOBUAIZAWA SHINICHI
    • H04R7/02H04R7/12H04R7/16H04R31/00
    • PROBLEM TO BE SOLVED: To provide a diaphragm which is easily manufactured and has satisfactory characteristics.
      SOLUTION: At least any one kind of fiber material of wooden pulp, chemical fiber and inorganic fiber, a foaming agent and a fine fiber-like binding material of high beating degree are blended as necessary to prepare a paper making material and make paper. A molded object after paper making is attached in the inside of a die of a drying apparatus having a gap corresponding to the shape of a diaphragm 400, and the object is heated and dried to be foamed so that an edge 430 becomes thick. By improvement in rigidity by thickness by foaming and tangling between fibers by the fine fiber-like binding agent, the strength of the edge 430 can be improved without increasing the minimum resonant frequency without reinforcement such as lamination of a different sheet-like member or impregnation of a composite resin, and a satisfactory acoustic characteristic can be obtained.
      COPYRIGHT: (C)2005,JPO&NCIPI
    • 要解决的问题:提供容易制造且具有令人满意的特性的隔膜。 解决方案:根据需要,可以混合至少任意一种木浆,化纤,无机纤维的纤维材料,发泡剂和高打浆度的细纤维状粘结材料,以制备造纸材料并制成 纸。 造纸后的成型体被安装在具有对应于隔膜400的形状的间隙的干燥装置的管芯的内部,并且将物体加热干燥以发生边缘430变厚。 通过由细纤维状粘结剂通过发泡和纤维之间的缠​​结改善厚度的刚性,可以提高边缘430的强度,而不会增加无增强的最小共振频率,例如不同的片状部件的层压或浸渍 的复合树脂,并且可以获得令人满意的声学特性。 版权所有(C)2005,JPO&NCIPI