    • 3. 发明授权
    • Spring steel and method for manufacturing the same
    • 弹簧钢及其制造方法
    • US08608874B2
    • 2013-12-17
    • US13638375
    • 2011-02-28
    • Minoru HonjoKazukuni HaseHideto Kimura
    • Minoru HonjoKazukuni HaseHideto Kimura
    • C22C38/22C22C38/04C21D9/02
    • F16F1/021C21D1/25C21D8/06C21D9/02C21D2211/008C22C38/04C22C38/22C22C38/34
    • Disclosed is high strength spring steel that can limit the depth of pitting occurring when corroded and therefore possesses high strength as well as excellent pitting corrosion resistance and corrosion fatigue property, with a composition containing: C: greater than 0.35 mass % and less than 0.50 mass %; Si: greater than L75 mass % and less than or equal to 3.00 mass %; Mn: 0.2 mass % to 1.0 mass %; Cr: 0.01 mass % to 0.04 mass %; P: 0.025 mass % or less; S: 0.025 mass % or less; Mo: 0.1 mass % to 1.0 mass %; and 0: 0.0015 mass % or less, under a condition that a PC value calculated by PC=4.2×([C]+[Mn])+0.1×(1/[Si]+1/[Mo])+20.3×[Cr]+0.001×(1/[N]) is greater than 3.3 and equal to or less than 8.0. Also disclosed is a preferred method for manufacturing the same.
    • 公开了一种高强度弹簧钢,其可以限制腐蚀发生的点蚀深度,因此具有高强度以及优异的耐点腐蚀性和耐腐蚀疲劳性能,组合物含有:C:大于0.35质量%且小于0.50质量% %; Si:大于L75质量%且小于等于3.00质量%; Mn:0.2质量%〜1.0质量% Cr:0.01质量%〜0.04质量% P:0.025质量%以下; S:0.025质量%以下; Mo:0.1质量%〜1.0质量% 在[PC] = 4.2×([C] + [Mn])+ 0.1×(1 / [Si] + 1 / [Mo])+ 20.3× [Cr] + 0.001×(1 / [N])大于3.3且等于或小于8.0。 还公开了其制造方法。