会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 5. 发明申请
    • Acrylic resin, resin boards, transparent electrode boards for touch panels, touch panels, and processes for production of them
    • 丙烯酸树脂,树脂板,用于触摸面板的透明电极板,触摸面板及其制造方法
    • US20060041067A1
    • 2006-02-23
    • US10534525
    • 2003-11-10
    • Hideyuki SugamotoOsamu Kawai
    • Hideyuki SugamotoOsamu Kawai
    • C08L61/00C08K5/07
    • G06F3/045C08F220/18Y10T428/31855Y10T428/31909
    • A method of producing an acrylic resin plate, comprising a step of adding 0.001 to 1 part by weight of a polymerization initiator having 10 hours half life temperature of 80° C. or more and 0.015 to 0.2 parts by weight of cyclohexadiene or terpenoid-based compound into 100 parts by weight of a mixture composed of an alkyl methacrylate having a C1-4 alkyl group and a poly-functional (meth)acrylate to give a polymerizable mixture, and a step of polymerizing said polymerizable mixture; an acrylic resin comprising 3 to 30 wt % of an alkyl methacrylate unit having a C8-20 alkyl group, 2 to 35 wt % of a mono-ethylenically unsaturated monomer unit containing an alkyl methacrylate unit having a C1-4 alkyl group and 35 to 95 wt % of a poly-functional (meth)acrylate unit; an acrylic resin plate made of the resin and production process the same, and a transparent electrode plate for touch panel and a touch panel having them.
    • 一种丙烯酸树脂板的制造方法,其特征在于,包括将0.001〜1重量份的10分钟半衰期为80℃以上的聚合引发剂和0.015〜0.2重量份的环己二烯或萜类系 将100重量份由具有C1-4烷基的甲基丙烯酸烷基酯和多官能(甲基)丙烯酸酯组成的混合物混合,得到可聚合的混合物,以及使所述可聚合混合物聚合的步骤; 包含3至30重量%的具有C8-20烷基的甲基丙烯酸烷基酯单元,2至35重量%的含有具有C 1-4烷基的甲基丙烯酸烷基酯单元的单烯属不饱和单体单元和35至 95重量%的多官能(甲基)丙烯酸酯单元; 由树脂制成的丙烯酸树脂板和制造方法相同,以及用于触摸面板的透明电极板和具有它们的触摸面板。