    • An optical recording medium affording a maximum Kerr effect enhancement, yet exhibiting a good signal-to-noise ratio, includes, for example, a substrate, an interference layer, a tracking guide layer, and a recording layer which are successively formed one above the other in the stated order. The interference layer is made of a light transmissive material and has a refractive index that is larger than that of the substrate. The interference layer has a first portion etched to a predetermined depth (d) and a second portion having a predetermined thickness (D). The tracking guide layer is formed on the second portion of the interference layer in a predetermined pattern, e.g. spirally or coaxially, for obtaining a tracking signal for use in tracking servo. The thickness of the interference layer defined by D minus d is set substantially equal to (.lambda./4n)+M(.lambda./2n) where .lambda. is a wavelength of light for reading the information, n is a refractive index of the interference layer, and M is an integer.
    • 提供最大克尔效应增强但呈现出良好的信噪比的光记录介质包括例如基板,干涉层,跟踪引导层和记录层,它们依次形成在 其他按照规定的顺序。 干涉层由透光材料制成,折射率大于基板的折射率。 干涉层具有蚀刻到预定深度(d)的第一部分和具有预定厚度(D)的第二部分。 跟踪引导层以预定的图案形成在干涉层的第二部分上,例如, 螺旋或同轴,用于获得用于跟踪伺服的跟踪信号。 由D减去d定义的干涉层的厚度基本上等于(λ/ 4n)+ M(λ/ 2n),其中λ是用于读取信息的光的波长,n是干涉层的折射率, M是整数。
    • 4. 发明授权
    • Manufacturing method of ink jet head
    • 喷墨头的制造方法
    • US07845070B2
    • 2010-12-07
    • US11644247
    • 2006-12-22
    • Yumiko Ohashi
    • Yumiko Ohashi
    • H05K3/36B23P17/00B21D53/76
    • B41J2/1609B41J2/1623B41J2/1626B41J2/1631B41J2/1632B41J2/1634B41J2002/14362B41J2002/14459Y10T29/49126Y10T29/49401
    • A manufacturing method of an ink jet head has: a step of forming a flow path hole on each of first plates to be flow path plates; a step of laminating one or plurality of said flow path plates on which said flow path hole is formed and a second plate to be a nozzle plate to each other; a step of laminating a protective film to said second plate; a step of laminating said plurality of flow path plates on which said flow path holes are formed to each other; a step of forming a nozzle hole on a region where the protective film is laminated, in said second plate to which the protective film is laminated; and a step of removing said protective film from said nozzle plate, after the step of laminating said plurality of flow path plates and said nozzle plate to each other.
    • 喷墨头的制造方法具有以下步骤:在每个第一板上形成作为流路板的流路孔; 将形成有所述流路孔的一个或多个所述流路板与形成喷嘴板的第二板层压的工序; 将保护膜层压到所述第二板的步骤; 将形成有所述流路孔的所述多个流路板彼此层压的步骤; 在层叠有保护膜的区域上形成喷嘴孔的步骤; 以及在将所述多个流路板和所述喷嘴板彼此层压的步骤之后,从所述喷嘴板移除所述保护膜的步骤。
    • 7. 发明授权
    • Manufacturing method for orifice plate
    • 孔板制造方法
    • US5277783A
    • 1994-01-11
    • US874009
    • 1992-04-27
    • Yumiko OhashiHideo Maruyama
    • Yumiko OhashiHideo Maruyama
    • B41J2/16C25D1/08
    • C25D1/08B41J2/162B41J2/1625
    • The present invention relates to a manufacturing method for an orifice plate to be used for an ink jet printer or the like. First, a master having a predetermined pattern firmly provided on a substrate is prepared. An electroformed film is then formed on the master by an electroforming method. Finally, the electroformed film is separated from the substrate. In this case, the mask pattern is firmly provided on the substrate, and a mechanical strength of the mask pattern itself is large. Furthermore, the mask pattern is insoluble to an alkali aqueous solution. Thus, the master can be reused, and it can be strongly washed. Accordingly, the master has a durability to repeated usage, thereby contributing to an improvement in the quality of the orifice plate to be manufactured and a reduction in the manufacturing cost.
    • 本发明涉及一种用于喷墨打印机等的孔板的制造方法。 首先,准备具有牢固地设置在基板上的预定图案的母版。 然后通过电铸方法在母板上形成电铸薄膜。 最后,将电铸薄膜与基材分离。 在这种情况下,掩模图案牢固地设置在基板上,并且掩模图案本身的机械强度大。 此外,掩模图案不溶于碱性水溶液。 因此,主人可以重复使用,可以强力洗涤。 因此,主机具有重复使用的耐久性,从而有助于提高待制造的孔板的质量和降低制造成本。
    • 9. 发明申请
    • Manufacturing method of ink jet head
    • 喷墨头的制造方法
    • US20070144001A1
    • 2007-06-28
    • US11644247
    • 2006-12-22
    • Yumiko Ohashi
    • Yumiko Ohashi
    • B21D53/76
    • B41J2/1609B41J2/1623B41J2/1626B41J2/1631B41J2/1632B41J2/1634B41J2002/14362B41J2002/14459Y10T29/49126Y10T29/49401
    • A manufacturing method of an ink jet head has: a step of forming a flow path hole on each of first plates to be flow path plates; a step of laminating one or plurality of said flow path plates on which said flow path hole is formed and a second plate to be a nozzle plate to each other; a step of laminating a protective film to said second plate; a step of laminating said plurality of flow path plates on which said flow path holes are formed to each other; a step of forming a nozzle hole on a region where the protective film is laminated, in said second plate to which the protective film is laminated; and a step of removing said protective film from said nozzle plate, after the step of laminating said plurality of flow path plates and said nozzle plate to each other.
    • 喷墨头的制造方法具有以下步骤:在每个第一板上形成作为流路板的流路孔; 将形成有所述流路孔的一个或多个所述流路板与形成喷嘴板的第二板层压的工序; 将保护膜层压到所述第二板的步骤; 将形成有所述流路孔的所述多个流路板彼此层压的步骤; 在层叠有保护膜的区域上形成喷嘴孔的步骤; 以及在将所述多个流路板和所述喷嘴板彼此层压的步骤之后,从所述喷嘴板移除所述保护膜的步骤。