    • 5. 发明授权
    • Method for producing antiglare film
    • 防眩膜的制造方法
    • US08932669B2
    • 2015-01-13
    • US13121386
    • 2009-09-29
    • Yuuki SaikiKazuhiro ShiojiriKazuhiro Oki
    • Yuuki SaikiKazuhiro ShiojiriKazuhiro Oki
    • B05D5/06G02B1/11B05D1/26B05D7/00
    • G02B1/111B05D1/265B05D7/5385B05D2201/02B05D2252/02
    • A method for producing an antiglare film includes: a step of preparing coating liquids comprising components capable of being unevenly distributed in an antiglare layer-forming coating liquid and a low-refractive index layer-forming coating liquid, respectively; a coating step of applying the low-refractive index layer-forming coating liquid as an upper layer and the antiglare layer-forming coating liquid as a lower layer on a support to form a coating layer; and a drying step of drying the coating layer and making the coating layer cause phase-separation so as to unevenly distribute the components and form an antiglare layer and a low-refractive index layer. By the production method, an antiglare film which suppresses reflection and glaring of external light in a display and whitening due to irregular reflection can be produced at a low cost.
    • 制造防眩膜的方法包括:分别制备包含能够分散在防眩层形成用涂布液和低折射率层形成用涂布液中的成分的涂布液的工序; 将作为上层的低折射率层形成用涂布液和防眩层形成用涂布液作为下层涂布在载体上以形成涂层的涂布步骤; 以及干燥步骤,使涂层干燥并使涂层引起相分离,从而不均匀地分配组分并形成防眩光层和低折射率层。 通过该制造方法,可以低成本地制造抑制显示器中的外部光的反射和眩光的抗眩光膜,并且由于不规则的反射而发白。
    • 7. 发明授权
    • Multilayer film and manufacturing method thereof
    • 多层膜及其制造方法
    • US08425984B2
    • 2013-04-23
    • US12918123
    • 2009-02-18
    • Kazuhiro OkiKazuhiro Shiojiri
    • Kazuhiro OkiKazuhiro Shiojiri
    • B05D3/02
    • B05D7/00G02B5/02G02F2201/38Y10T428/31504
    • According to a manufacturing method of a multilayer film according to one aspect of the present invention, at the step of applying a coating liquid prepared by dissolving a plurality of monomers or polymers in at least one solvent onto a substrate and subsequently drying the coating liquid, the solvent is allowed to penetrate into the substrate at a specified speed. This causes concentration distribution of the solvent within the coated layer in the thickness direction thereof, and thus a multilayer film separated into an upper layer and a lower layer can be formed by one coating. Accordingly, a multilayer film having a different function in each layer can be formed by one coating.
    • 根据本发明的一个方面的多层膜的制造方法,在将多种单体或聚合物在至少一种溶剂中溶解到基材上并随后干燥涂布液的步骤中, 允许溶剂以特定的速度渗透到基材中。 这使得涂层在其厚度方向上的溶剂的浓度分布,从而可以通过一次涂布形成分离成上层和下层的多层膜。 因此,可以通过一次涂布形成在各层中具有不同功能的多层膜。
    • 8. 发明申请
    • METHOD FOR PRODUCING ANTIGLARE FILM
    • 生产胶片的方法
    • US20110177240A1
    • 2011-07-21
    • US13121386
    • 2009-09-29
    • Yuuki SaikiKazuhiro ShiojiriKazuhiro Oki
    • Yuuki SaikiKazuhiro ShiojiriKazuhiro Oki
    • B05D5/06
    • G02B1/111B05D1/265B05D7/5385B05D2201/02B05D2252/02
    • A method for producing an antiglare film includes: a step of preparing coating liquids comprising components capable of being unevenly distributed in an antiglare layer-forming coating liquid and a low-refractive index layer-forming coating liquid, respectively; a coating step of applying the low-refractive index layer-forming coating liquid as an upper layer and the antiglare layer-forming coating liquid as a lower layer on a support to form a coating layer; and a drying step of drying the coating layer and making the coating layer cause phase-separation so as to unevenly distribute the components and form an antiglare layer and a low-refractive index layer. By the production method, an antiglare film which suppresses reflection and glaring of external light in a display and whitening due to irregular reflection can be produced at a low cost.
    • 制造防眩膜的方法包括:分别制备包含能够分散在防眩层形成用涂布液和低折射率层形成用涂布液中的成分的涂布液的工序; 将作为上层的低折射率层形成用涂布液和防眩层形成用涂布液作为下层涂布在载体上以形成涂层的涂布步骤; 以及干燥步骤,使涂层干燥并使涂层引起相分离,从而不均匀地分配组分并形成防眩光层和低折射率层。 通过该制造方法,可以低成本地制造抑制显示器中的外部光的反射和眩光的抗眩光膜,并且由于不规则的反射而发白。
    • 10. 发明授权
    • Anti-glare film manufacturing method
    • 防眩膜制造方法
    • US08936837B2
    • 2015-01-20
    • US13411064
    • 2012-03-02
    • Hideaki KagawaTakahiro NakazawaKazuhiro Oki
    • Hideaki KagawaTakahiro NakazawaKazuhiro Oki
    • C08F2/48G02B27/00G02B13/20G02B5/02B05D3/06B05D5/02B05D3/02
    • G02B5/0226B05D3/0209B05D3/067B05D5/02
    • The method includes: forming a coating film including particles and an ultraviolet curable resin on a film substrate; and curing the ultraviolet curable resin by ultraviolet irradiation to form an anti-glare layer constituted by the particles and the ultraviolet curable resin. A ratio of a thickness A of the anti-glare layer to a diameter B of the particles is in the range of 1.5 to 2.4. The ultraviolet irradiation is performed with two or more ultraviolet irradiation units, the first unit irradiation amount is 49 mJ/cm2 or less, the second and subsequent units irradiation amount is greater than 50 mJ/cm2, and the total irradiation amount is 100 mJ/cm2 or greater. The oxygen concentration at a position which is 1 mm above a surface of the coating film is 1 ppm to 2000 ppm. The first unit irradiation is performed above a roller with surface temperature of 10° C. to 24° C.
    • 该方法包括:在膜基材上形成包含颗粒和紫外线固化树脂的涂膜; 并通过紫外线照射固化紫外线固化树脂,以形成由该颗粒和紫外线固化树脂构成的防眩层。 抗眩光层的厚度A与颗粒的直径B之比为1.5〜2.4。 用两个以上的紫外线照射单元进行紫外线照射,第一单位照射量为49mJ / cm 2以下,第二次照射量和后续单位照射量大于50mJ / cm 2,总照射量为100mJ / cm2以上。 在涂膜表面1mm以上的位置的氧浓度为1ppm〜2000ppm。 在表面温度为10℃至24℃的辊上方进行第一单元照射。