热词
    • 4. 发明专利
    • Environmental load-reducing concrete composition
    • 环境负荷减少混凝土组合物
    • JP2011116612A
    • 2011-06-16
    • JP2009278074
    • 2009-12-07
    • Kajima Corp鹿島建設株式会社
    • KASAI HIROSHISHINTANI AKIRAYODA KAZUHISA
    • C04B28/08C04B14/02C04B28/04
    • PROBLEM TO BE SOLVED: To provide an environmental load-reducing concrete applicable on ground skeleton of a building material as an alternate material of a conventional common concrete and having large CO
      2 reduction effect.
      SOLUTION: The environmental load-reducing concrete composition is prepared by replacing cement of 75-100 mass% with blast furnace cement type B and replacing a part or total of coarse aggregate with hydrated lightweight aggregate to make the water content (unit quantity) of the lightweight aggregate to be ≥25 kg/m
      3 , in a common concrete composition in which cement component comprises portland cement, water/cement ratio is 40-65% and the compressive strength is 18-45 N/mm
      2 in 28 day material age.
      COPYRIGHT: (C)2011,JPO&INPIT
    • 要解决的问题:提供一种适用于建筑材料的地面骨架的环境负荷减少混凝土作为常规混凝土的替代材料,并具有较大的CO 2 还原效果。

      解决方案:通过用B型高炉水泥代替75-100质量%的水泥,用水合轻质骨料代替一部分或全部粗骨料,制成环境负荷减少的混凝土组成,使含水量(单位数量 )轻质骨料的含量≥25kg/ m 3 SP / 3>在普通混凝土组合物中,水泥组分包括硅酸盐水泥,水/水泥比为40-65%,抗压强度为18- 在第28天材料年龄中,45 N / mm 2 。 版权所有(C)2011,JPO&INPIT