    • 7. 发明专利
    • METHOD AND DEVICE FOR REPAIRING BOTTOM SIDE WALL OF BLAST FURNACE
    • JPH11293310A
    • 1999-10-26
    • JP10124598
    • 1998-04-13
    • NIPPON STEEL CORP
    • NAKAMURA YUKIHIROYAMADA JUNJINAKAMURA HITOSHISUZUKI TOSHIFUMI
    • C21B7/06C21B7/14F27D1/16
    • PROBLEM TO BE SOLVED: To prolong the operational period of a blast furnace by press-fitting a plastic shapeless refractory after iron tapping or during blowing-off from a repair hole pierced in a hearth side wall at a position higher than a tap hole in the vicinity of the tap hole to execute the sufficiently curable repair at the wear parts of the side wall at the tap hole part. SOLUTION: A repair hole 3 is pierced in a blast furnace hearth side wall part 2. The repair hole 3 is pierced from an external side wall of the hearth to an internal side wall of the hearth at a position higher than a tap hole 1 in the vicinity of the tap hole 1. When wear parts of the side wall of a furnace bottom in the vicinity of the tap hole 1 where the hot metal is fluidized strongly in the blast furnace, a relatively soft plastic shapeless refractory is press-fitted from the repair hole 3 at the timing when the hot metal level after iron tapping or during blowing-off at the tap hole 1 is sufficiently lowered. A first filled part 4 is formed up to the vicinity of the tap hole 1 with the press-fitted refractory and then, a second filled part 5 is formed up to the upper part of the top hole 1. The wear parts of the side wall of the tap hole part are sufficiently repaired in this way, the iron tapping time is secured and the erosion of bricks is suppressed.