    • 2. 发明专利
    • CONTINUOUS COLD ROLLING EQUIPMENT
    • JPH01309705A
    • 1989-12-14
    • JP14056688
    • 1988-06-09
    • KAWASAKI STEEL CO
    • KATSURA SHIGEFUMIKAWAI YOSHITONAKAHARA HISANAO
    • B21B27/10B21B45/02
    • PURPOSE:To prevent the dilution of a high-density rolling mill lubricant by roll cooling water and to prevent the degradation of lubricity by disposing nozzles for injecting the high-concn. rolling mill lubricant to the inlet side of a rolling mill and disposing jacket type coolers oppositely to the outer peripheral faces of rolling rolls to the outlet side of the rolling mill. CONSTITUTION:The pressurized cooling water sent to a water feed pipe 15 passes a pipe body 12 and is sent to a water feed header 20 and is further projected from slit nozzles 20a of the water feed header 20 so as to be forcibly passed in cooling water passages 19. This water enters the inside of a drain header 21 from a drain port 21a and is drained through a pipe body 13 and a drain pipe 16. The cooling water of the roll 2a is supplied while the water forms a water film with the outside peripheral face of the roll 2a in the hermetically sealed jacket type roll cooler 5 and, therefore, the roll cooling power is extremely high and the leakage of the cooling water from sealing parts 6a, 6b is obviated. The dilution of the high-concn. rolling mill lubricant by the cooling water is prevented.
    • 3. 发明专利
    • METHOD FOR SUPPLYING VAPORIZATION ROD STOCK INTO DRY PLATING BATH
    • JPH01176070A
    • 1989-07-12
    • JP33026987
    • 1987-12-28
    • KAWASAKI STEEL CO
    • KATSURA SHIGEFUMINAKAHARA HISANAONAGAMINE TSUNEOTAKAHASHI NORIOSUZUKI FUMIHITO
    • C23C14/24
    • PURPOSE:To continuously supply a rod stock and to prevent the falling of the end of the rod stock by providing a rugged surface on the ends of the rod stock and shrink-fitting the tail end of the preceding rod stock to the leading part of the succeeding rod stock with an electron beam. CONSTITUTION:After a push bar 8 in a vaporization rod stock fixing chamber 2 is advanced to the forward limit, the bar 8 is retreated to a fixation waiting position, and a gate valve 3 between a vapor-deposition chamber 4 and the fixing chamber 2 is closed. The rod stock having a recessed surface at the tail end is fixed by a rod stock fixing jig 13, and the recessed surface end is heated by an electron beam gun 14. The inside of the fixing chamber 2 is adjusted to atmospheric pressure, the rod stock is fixed from the outside, and the leading recessed surface is rapidly pushed into the projecting surface of the preceding rod. The inside of the fixing chamber is simultaneously evacuated, the valve 3 is opened, and then the leading projecting surface of the pushed-in rod stock is engaged with the tail-end recessed surface of the preceding rod slightly expanded by thermal expansion. A beam is then projected to join both rods, the rod stock is continuously pushed out, and normal operation is carried out.
    • 7. 发明专利
    • AIR LOCK FOR STRIP
    • JPS6324066A
    • 1988-02-01
    • JP16671886
    • 1986-07-17
    • KAWASAKI STEEL CO
    • TAKAHASHI NORIOSUZUKI FUMIHITONAKAHARA HISANAO
    • C23C14/56
    • PURPOSE:To always keep the inside of a vacuum chamber at a high vacuum by forming the air locks on the inlet and outlet sides of the vacuum deposition chamber in a continuous vacuum deposition device with plural differential pressure chambers, and providing the upper and lower seal rolls each furnished with a side seal roll in each differential pressure chamber. CONSTITUTION:A strip metal 4 is introduced into the vacuum chamber 1 through the air lock 2 on the inlet side consisting of plural differential pressure chambers 2a-2d, the vapor of a metal such as Al and Ti from a vapor deposition source 9 is deposited on the strip metal, and the strip metal is taken out through the air lock 3 on the outlet side consisting of differential pressure chambers 3d-3a. The upper and lower seal rolls 11 and 12 are provided on the inlet side of each differential pressure chamber of the air lock with the strip metal 4 in between to close the inlet side, and a couple of the upper and lower side seal rolls 19 and 20 being brought into contact with each other are fixed at both end parts of at least a set of the seal rolls through which the strip metal 4 is not passed. The same structure is provided to the air lock 3. Consequently, the penetration of air into the vacuum chamber 1 is prevented, the penetration of O2, CO2, and fine suspended matter into the vacuum chamber 1 is also prevented, and the deterioration in the quality of the deposited film is prevented.
    • 9. 发明专利
    • IRON LOSS REDUCTION METHOD FOR SINGLE DIRECTIONAL GRAIN ORIENTED SILICON STEEL PLATE
    • JPS61296703A
    • 1986-12-27
    • JP13786885
    • 1985-06-26
    • KAWASAKI STEEL CO
    • IGUCHI MASAONAKAHARA HISANAOITO ISAO
    • H01F1/18H01F1/16
    • PURPOSE:To avoid loss of effect caused through high temperature hysteresis such as strain relief anneal by a method wherein a grain oriented silicon steel plate which is finished to have mirror surface is rolled into a loose coil in which the plate surfaces are separated from each other and subjected to a depressurized CVD process to form a very thin tension film on the steel plate surface. CONSTITUTION:A grain oriented silicon steel plate is rolled into a loose coil 9 and the coil 9 is inserted into a vacuum furnace 1 and the vacuum rate in the furnace is made to be 10 -10 Torr by the operation of a vacuum pump through a vacuum passage 8. After that, while H2 gas is being introduced through a gas introduction passage 4, in order to improve circulation of the gas in the furnace, the gas is extracted through a gas exhaust passage 10 and the inside of the furnace is always under the depressurized condition (normal operating pressure is 1-500 Torr) and the gas flow through the gaps between the steel plates of the loose coil 9 is kept smooth. Then, after a heater 3 is operated and the coil temperature reaches 600 deg.C-1,000 deg.C and kept at that, a mixture gas such as TiCl4 and N2, TiCl4 and CH4 or TiCl4 and CH4 and N2 is introduced through the gas introduction passage 4 and a very thin tension film is formed on the steel plate surface by a depressurized CVD method in 5min-100hr.
    • 10. 发明专利
    • DIE REPLACING DEVICE OF O-PRESS
    • JPS609523A
    • 1985-01-18
    • JP11770683
    • 1983-06-28
    • KAWASAKI STEEL CO
    • NAKAHARA HISANAOYOSHIMURA HIROYUKIMINE YOSHISUKEMIURA KAZUHIKOMIZUTANI NAOKI
    • B21D5/01B21D37/04B21D37/14
    • PURPOSE:To easily carry in and out old and new master dies and to improve the efficiency of die replacing operation by providing a dolly capable of mounting the master dies to the inlet and outlet sides of an O-press and providing a master-die preparing table to the side-part of the O-press. CONSTITUTION:Rolls for transporting dies in the inside of an O-press 8 are raised to hold old master dies 1A, 2A into a transportable state. A closing stand 21 and an exit-side table 9 are retreated to form an entrance-exit space of dollys 22A, 22B at the inlet and exit sides of the O-press 8. The dolly 22A at the inlet side of O-press 8 is traveled to a press-line center. The old master dies 1A, 2A are transferred to the line inlet side and are loaded onto the dolly 22A, which is traveled along a rail 23A and is adjoined to an old die preparing table 29 to load the dies 1A, 2A onto a table 29. In this way, all of the dies 1A, 2A are loaded from the O-press 8 to the table 29. Next, new master dies 1B, 2B are transferred from a new master-die preparing table 30 to insert them into the press 8 from the exit side, reversely to the operation mentioned above, for repacing the dies by the dolly 22B.