    • 1. 发明专利
    • Method of manufacturing modified coal and manufacturing method of coke
    • 制造改性煤的方法和焦炭的制造方法
    • JP2009013222A
    • 2009-01-22
    • JP2007173968
    • 2007-07-02
    • Jfe Chemical CorpJfe Techno Research CorpJfeケミカル株式会社Jfeテクノリサーチ株式会社
    • MIYAZAWA KUNIOMOROTOMI HIDETOSHIITAGAKI SHOZOTAKENAKA JOICHI
    • C10B57/08
    • PROBLEM TO BE SOLVED: To provide a method of reforming low-grade coal containing a large amount of oxygen atoms without generating a large amount of water, and to provide a method of manufacturing coke for iron-making by using the same.
      SOLUTION: A method of manufacturing modified coal by treating low-grade coal with heavy oils comprises: a catalyst-carrying step of causing low-grade coal containing a large amount of oxygen atoms to carry a metal and/or a metal compound; a porosification step of drying the low-grade coal carrying the catalyst and subsequently porosifying the low-grade coal by heating it at a temperature of 300-1,200°C in an inert atmosphere or in a slightly oxidizing atmosphere; and a modifying step of heating the porous low-grade coal after the porosification step together with heavy oils at a temperature of 300-500°C in an inert atmosphere or in a reducing atmosphere, thereby causing decomposate of heavy oils to adhere to the surface of the porous low-grade coal.
      COPYRIGHT: (C)2009,JPO&INPIT
    • 要解决的问题:提供一种重整含有大量氧原子的低等级煤而不产生大量水的方法,并提供一种通过使用该方法制造用于制铁的焦炭的方法。 解决方案:通过用重油处理低等级煤来制造改性煤的方法包括:催化剂携带步骤,使含有大量氧原子的低等级煤携带金属和/或金属化合物 ; 干燥含有催化剂的低级煤的孔化步骤,然后在惰性气氛或轻微氧化气氛中在300-1200℃的温度下加热低品位煤; 以及在惰性气氛或还原气氛中,在300-500℃的温度下,与粗油加热多孔低等级煤的改性步骤,其中重油分解粘附在表面上 的多孔低品位煤。 版权所有(C)2009,JPO&INPIT
    • 3. 发明专利
    • Method of manufacturing modified coal and manufacturing method of coke
    • 制造改性煤的方法和焦炭的制造方法
    • JP2009013221A
    • 2009-01-22
    • JP2007173965
    • 2007-07-02
    • Jfe Techno Research CorpJfeテクノリサーチ株式会社
    • MIYAZAWA KUNIOMOROTOMI HIDETOSHIITAGAKI SHOZO
    • C10B57/08C10B57/04C10B57/06
    • PROBLEM TO BE SOLVED: To provide a method of reforming low-grade coal containing a large amount of oxygen atoms without generating a large amount of water, and to provide a method of manufacturing coke for iron-making by using the same.
      SOLUTION: A method of manufacturing modified coal by treating low-grade coal with heavy oils comprises: a deoxidization step of subjecting low-grade coal containing a large amount of oxygen atoms to a heating treatment, thereby decreasing the oxygen content down to ≤15 mass%; and a modifying step of heating the low-grade coal after deoxidization together with heavy oils at a temperature of 300-500°C, thereby causing the decomposition product of heavy oils to adhere to the surface of the low-grade coal.
      COPYRIGHT: (C)2009,JPO&INPIT
    • 要解决的问题:提供一种重整含有大量氧原子的低等级煤而不产生大量水的方法,并提供一种通过使用该方法制造用于制铁的焦炭的方法。 解决方案:通过用重油处理低等级煤制造改性煤的方法包括:将含有大量氧原子的低品位煤进行加热处理的脱氧步骤,从而将氧含量降低到 ≤15质量% 以及在300-500℃的温度下,与重油一起在脱氧后加热低等级煤,由此使重质油分解产物附着在低等级煤的表面上的改性工序。 版权所有(C)2009,JPO&INPIT
    • 5. 发明专利
    • Method for producing benzene compound and method for processing plastic material
    • 苯乙烯化合物的生产方法和加工塑料的方法
    • JP2007291039A
    • 2007-11-08
    • JP2006122990
    • 2006-04-27
    • Jfe Chemical CorpJfeケミカル株式会社
    • TAKENAKA JOICHIMIYAZAWA KUNIO
    • C07C4/06B01D3/00C07B61/00C07C7/04C07C15/04C07C15/06C08J11/08C08J11/16C10G1/10
    • Y02P20/52Y02W30/701Y02W30/705
    • PROBLEM TO BE SOLVED: To provide a method for producing benzene compounds free from side chain or benzene compounds having short side chain from polystyrene and other plastic materials by a hydrocracking method in high yield. SOLUTION: The method for producing benzene compounds comprises a dissolution step to heat and mix polystyrene and a solvent to obtain a polystyrene solution, a hydrocracking step to react the polystyrene solution obtained by the dissolution step with hydrogen in the presence of a catalyst to perform hydrocracking reaction, and a distillation step to distill the hydrocracking reaction product produced by the hydrocracking step to obtain benzene compounds, provided that at least a part of the light fraction having a boiling point of 130-140°C and obtained by the distillation step is returned to the dissolution step. COPYRIGHT: (C)2008,JPO&INPIT
    • 待解决的问题:提供一种通过加氢裂化方法以高产率生产不含侧链的苯化合物或具有短链侧链的苯化合物的方法。 解决方案:苯化合物的制造方法包括将聚苯乙烯和溶剂加热混合以获得聚苯乙烯溶液的溶解步骤,加氢裂化步骤,使通过溶解步骤获得的聚苯乙烯溶液与氢在催化剂存在下反应 进行加氢裂化反应,以及蒸馏步骤,蒸馏通过加氢裂化步骤产生的加氢裂化反应产物,得到苯化合物,条件是至少部分沸点为130-140℃的轻馏分并通过蒸馏得到 步骤返回到溶解步骤。 版权所有(C)2008,JPO&INPIT
    • 6. 发明专利
    • Method for producing activated carbon
    • 生产活性炭的方法
    • JP2007182358A
    • 2007-07-19
    • JP2006002668
    • 2006-01-10
    • Jfe Chemical CorpJfeケミカル株式会社
    • SHIODE TETSUOMIYAZAWA KUNIO
    • C01B31/12
    • PROBLEM TO BE SOLVED: To provide a method for producing activated carbon with which smooth operation of a production unit, improvement in safety of an operator and prevention of environmental pollution are achieved in the production of activated carbon.
      SOLUTION: This production method employs two or more activation units and conducts operation processes as follows: charging a carbon material into a first activation unit and starting operation of the first activation unit; then charging a carbon material into a second activation unit and starting operation of the second activation unit; further starting a third to an Nth activation units, respectively, by serially setting back the timing of charging the carbon material; thereafter drying up the inside of the first activation unit which is finished its operation, and charging the carbon material and starting again operation of the first activation unit.
      COPYRIGHT: (C)2007,JPO&INPIT
    • 要解决的问题:提供一种生产活性炭的生产活性炭的生产方法,在生产活性炭时可以实现操作者的安全性和防止环境污染。 解决方案:该生产方法采用两个或更多个激活单元并进行如下操作过程:将碳材料装入第一激活单元并启动第一激活单元的操作; 然后将碳材料装入第二激活单元并启动第二激活单元的操作; 分别通过串联地设置碳材料的充电时间来进一步开始第三到第N激活单元; 然后干燥完成其操作的第一激活单元的内部,并且对碳材料充电并再次开始第一激活单元的操作。 版权所有(C)2007,JPO&INPIT
    • 7. 发明专利
    • Method of manufacture activated carbon
    • 制备活性炭的方法
    • JP2007131461A
    • 2007-05-31
    • JP2005323032
    • 2005-11-08
    • Jfe Chemical CorpJfeケミカル株式会社
    • NONAKA TOSHIHARUNAGAYAMA KATSUHIROUEHARA KENICHIMIYAZAWA KUNIO
    • C01B32/336
    • PROBLEM TO BE SOLVED: To provide a method of manufacturing activated carbon by which the activated carbon is always uniformly activated thereby the activated carbon having a large and uniform surface area is manufactured.
      SOLUTION: The method of manufacturing activated carbon comprises the steps of: mixing 89-98.9 mass% powder of a phenolic resin, 1-10 mass% pitch and 0.1-1 mass% polyvinyl alcohol; granulating the obtained mixture; carbonizing the granulated mixture; and activating the carbonized mixture. It is preferable to disintegrate the activated carbon obtained after activation and classify the disintegrated activated carbon.
      COPYRIGHT: (C)2007,JPO&INPIT
    • 要解决的问题:为了提供活性炭的制造方法,通过该方法,活性炭总是均匀地活化,从而制造具有大而均匀的表面积的活性炭。 解决方案:制造活性炭的方法包括以下步骤:将89-98.9质量%酚醛树脂粉末,1-10质量%沥青和0.1-1质量%聚乙烯醇混合; 对所得混合物进行造粒; 将造粒混合物碳化; 并活化碳化混合物。 活化后得到的活性炭优选分解,分解活性炭。 版权所有(C)2007,JPO&INPIT