    • 2. 发明申请
    • METHOD FOR FORMING MULTILAYER COATING FILM
    • 形成多层涂膜的方法
    • US20100129662A1
    • 2010-05-27
    • US12452808
    • 2008-07-18
    • Junya OgawaKoji KanagawaShuichi NakaharaTadashi IidaHiroyuki NaganoYoshizumi MatsunoYasushi Nakao
    • Junya OgawaKoji KanagawaShuichi NakaharaTadashi IidaHiroyuki NaganoYoshizumi MatsunoYasushi Nakao
    • B05D3/02B32B27/38
    • B05D7/574B05D3/0254B05D7/572B05D2202/10Y10T428/31511
    • This invention provides a method for forming multilayer coating film excelling in smoothness and distinctness of image, by 3-coat-1-bake system in which a step of applying onto a coating object a water-based intermediate paint (X) to form an intermediate coating film; a step of adjusting the solid content of the intermediate coating film to 70-100 mass %; a step of applying onto the intermediate coating film a water-based base coating paint (Y) containing 30-55 mass parts of alcoholic solvent having a boiling point of 170-250° C., to form a base coating film; a step of adjusting the solid content of the base coating film to 70-100 mass %; a step of applying a clear paint (Z) comprising 40-60 mass parts of carboxyl-containing compound and 60-40 mass parts of polyepoxide onto the base coating film to form a clear coating film; and heating the intermediate coating film, base coating film and clear coating film at 100-120° C. for 3-10 minutes and thereafter further heating them at 130-160° C. for 10-30 minutes; are successively carried out.
    • 本发明提供了一种形成多层涂膜的方法,其通过3-涂层1烘烤系统的平滑度和清晰度,其中涂布在涂料上的步骤为水性中间涂料(X)以形成中间体 涂膜; 将中间涂膜的固体成分调整为70〜100质量%的工序; 向中间涂膜施加含有30-55质量份沸点为170-250℃的醇溶剂的水性底涂层(Y)的步骤,以形成基底涂膜; 调整基底涂膜的固体成分为70〜100质量%的工序。 将包含40-60质量份含羧基化合物和60-40质量份聚环氧化物的透明涂料(Z)施加到基底涂膜上以形成透明涂膜的步骤; 并在100-120℃下加热中间涂膜,底涂层和透明涂膜3-10分钟,然后在130-160℃下进一步加热10-30分钟; 相继进行。
    • 3. 发明授权
    • Method for forming multilayer coating film
    • 多层涂膜形成方法
    • US08906465B2
    • 2014-12-09
    • US12452808
    • 2008-07-18
    • Junya OgawaKoji KanagawaShuichi NakaharaTadashi IidaHiroyuki NaganoYoshizumi MatsunoYasushi Nakao
    • Junya OgawaKoji KanagawaShuichi NakaharaTadashi IidaHiroyuki NaganoYoshizumi MatsunoYasushi Nakao
    • B05D5/00B05D3/02B05D7/00B05D1/02
    • B05D7/574B05D3/0254B05D7/572B05D2202/10Y10T428/31511
    • This invention provides a method for forming multilayer coating film excelling in smoothness and distinctness of image, by 3-coat-1-bake system in which a step of applying onto a coating object a water-based intermediate paint (X) to form an intermediate coating film; a step of adjusting the solid content of the intermediate coating film to 70-100 mass %; a step of applying onto the intermediate coating film a water-based base coating paint (Y) containing 30-55 mass parts of alcoholic solvent having a boiling point of 170-250° C., to form a base coating film; a step of adjusting the solid content of the base coating film to 70-100 mass %; a step of applying a clear paint (Z) comprising 40-60 mass parts of carboxyl-containing compound and 60-40 mass parts of polyepoxide onto the base coating film to form a clear coating film; and heating the intermediate coating film, base coating film and clear coating film at 100-120° C. for 3-10 minutes and thereafter further heating them at 130-160° C. for 10-30 minutes; are successively carried out.
    • 本发明提供了一种形成多层涂膜的方法,其通过3-涂层1烘烤系统的平滑度和清晰度,其中涂布在涂料上的步骤为水性中间涂料(X)以形成中间体 涂膜; 将中间涂膜的固体成分调整为70〜100质量%的工序; 向中间涂膜施加含有30-55质量份沸点为170-250℃的醇溶剂的水性底涂层(Y)的步骤,以形成基底涂膜; 调整基底涂膜的固体成分为70〜100质量%的工序。 将包含40-60质量份含羧基化合物和60-40质量份聚环氧化物的透明涂料(Z)施加到基底涂膜上以形成透明涂膜的步骤; 并在100-120℃下加热中间涂膜,底涂层和透明涂膜3-10分钟,然后在130-160℃下进一步加热10-30分钟; 相继进行。