    • 4. 发明授权
    • Rubber-modified styrenic resin composition and molded article thereof
    • 橡胶改性苯乙烯树脂组合物及其成型品
    • US06660806B1
    • 2003-12-09
    • US09458959
    • 1999-12-10
    • Shuji YoshimiHayato KiharaTakahiro Ishii
    • Shuji YoshimiHayato KiharaTakahiro Ishii
    • C08F27901
    • C08L51/04C08L23/08C08L83/04C08L2666/04C08L2666/02
    • A rubber-modified styrenic resin composition comprising (A) 100 wt. parts of a rubber-modified styrenic resin which contains 10 to 35 wt. % of soft component particles having an average particle size of 0.1 to 0.5 &mgr;m, where said soft component particles have a single occlusion structure comprising a core part which consists of a single continuous phase of a styrenic resin and a shell part which comprises a rubber polymer and occludes said core part, and (B) 0.1 to 10 wt. parts of a polymer having a solubility parameter (SP) of 8.45 to 8.70 and having no aromatic vinyl compound unit therein. This composition has excellent plane impact strength and gloss properties, as well as moldability and other physical properties, and satisfies properties required for exterior materials, wrapping materials and molded foam articles.
    • 橡胶改性苯乙烯树脂组合物,其包含(A)100重量% 橡胶改性苯乙烯树脂的一部分,其含有10〜35重量% %的平均粒径为0.1〜0.5μm的软组分颗粒,其中所述软组分颗粒具有包含由单一连续相的苯乙烯树脂组成的核心部分和包含橡胶聚合物的壳部分的单一闭塞结构 并封闭所述核心部分,(B)0.1〜10wt。 部分溶解度参数(SP)为8.45〜8.70的聚合物,其中没有芳族乙烯基化合物单元。 该组合物具有优异的平面冲击强度和光泽性能,以及成型性等物理性能,并且满足外部材料,包装材料和模塑泡沫制品所需的性能。
    • 5. 发明授权
    • Styrenic resin composition and injection- and extrusion-molded articles
    • 苯乙烯树脂组合物和注射和挤出成型制品
    • US5534580A
    • 1996-07-09
    • US334330
    • 1994-11-04
    • Shinichi MitsuiHayato KiharaShuji Yoshimi
    • Shinichi MitsuiHayato KiharaShuji Yoshimi
    • C08K3/00C08L25/02C08L25/04C08K3/32
    • C08K3/0033C08L25/04C08L2205/02C08L25/02
    • Disclosed are a styrenic resin composition comprising (a) a styrenic resin having a weight average molecular weight of 100,000 to 2,000,000 and (b) a finely divided particulate inorganic or organic substance, the inorganic substance having a refractive index of 1.5-2.0 and an average particle diameter of 0.1-20 .mu.m, and the organic substance having a refractive index of 1.5-2.0 and an average particle diameter of 0.1-20 .mu.m and not having a glass transition temperature in a temperature range of 90.degree. C. or below, said particulate inorganic or organic substance accounting for 0.002 to 1 weight % based on the styrenic resin composition, as well as an injection-molded article prepared by molding the styrenic resin composition, and an extrusion-molded article comprising the styrenic resin composition in an amount of at least 50 weight %.
    • 公开了一种苯乙烯树脂组合物,其包含(a)重均分子量为100,000至2,000,000的苯乙烯树脂和(b)细碎的无机或有机物质,所述无机物质的折射率为1.5-2.0,平均 粒径为0.1-20μm,有机物折射率为1.5-2.0,平均粒径为0.1-20μm,玻璃化转变温度在90℃以下的温度范围内 所述颗粒状无机或有机物质相对于苯乙烯类树脂组合物为0.002〜1重量%,以及通过将苯乙烯系树脂组合物成型而制备的注射成型品,以及含有苯乙烯系树脂组合物的挤出成型品 至少50重量%。
    • 9. 发明授权
    • Rubber-modified styrenci resin composition and molded article thereof
    • 橡胶改性苯乙烯树脂组合物及其成型体
    • US6020428A
    • 2000-02-01
    • US656014
    • 1996-05-24
    • Shuji YoshimiHayato KiharaTakahiro Ishii
    • Shuji YoshimiHayato KiharaTakahiro Ishii
    • C08L23/08C08L51/04C08L83/04C08L25/04
    • C08L51/04C08L23/08C08L83/04
    • A rubber-modified styrenic resin composition comprising (A) 100 wt. parts of a rubber-modified styrenic resin which contains 10 to 35 wt. % of soft component particles having an average particle size of 0.1 to 0.5 .mu.m, where said soft component particles have a single occlusion structure comprising a core part which consists of a single continuous phase of a styrenic resin and a shell part which comprises a rubber polymer and occludes said core part, and (B) 0.1 to 10 wt. parts of a polymer having a solubility parameter (SP) of 8.45 to 8.70 and having no aromatic vinyl compound unit therein. This composition has excellent plane impact strength and gloss properties as well as moldability and other physical properties, and satisfies properties required for exterior materials, wrapping materials and molded foam articles.
    • 橡胶改性苯乙烯树脂组合物,其包含(A)100重量% 橡胶改性苯乙烯树脂的一部分,其含有10〜35重量% %的平均粒度为0.1〜0.5μm的软成分颗粒,其中所述软组分颗粒具有单一的闭塞结构,其包括由单一连续相的苯乙烯树脂组成的芯部分和包含橡胶的壳部分 聚合物并封闭所述核心部分,和(B)0.1至10wt。 部分溶解度参数(SP)为8.45〜8.70的聚合物,其中没有芳族乙烯基化合物单元。 该组合物具有优异的平面冲击强度和光泽性以及成型性等物理性能,并且满足外部材料,包装材料和模塑泡沫制品所需的性能。