    • Bolt material excellent in stress, corrosion, cracking resistance
    • 螺栓材料在应力,腐蚀,抗裂性方面优秀
    • JPS59136443A
    • 1984-08-06
    • JP13564283
    • 1983-07-25
    • Hitachi LtdHitachi Metals Ltd
    • HATSUTORI SHIGEOWATANABE RIKIZOUMORI YASUHIKOMASAOKA ISAOSASAKI RIYOUICHIITOU HISAO
    • C22C19/05
    • PURPOSE: To enhance the stress corrosion cracking resistance of a bolt under a high temp. water environment, by preparing the bolt used under a gap and stress acting condition in the high temp. water environment from an Ni-alloy.
      CONSTITUTION: The bolt used under a gap and stress acting condition in a high temp. water environment within a boiling water type or pressure water type nuclear reactor is fabricated from an Ni-alloy containing, on a wt. basis, 15W 25% Cr, 1W8% Mo, 0.4W2% Al, 0.7W3% Ti, 0.7W4.5% Nb, less than 40% Fe and more than 40% Ni. In this case, contained Al, Ti and Nb are contained in the range shown by the relation of 3.5%≤2Al+Ti+0.5Nb≤5.5%. This Ni- alloy contains one or more of a γ'-phase and a γ"-phase in the austenite phase base of the structure thereof and suitable for a bolt material showing excellent stress corrosion cracking resistance used in a high temp. water environment.
      COPYRIGHT: (C)1984,JPO&Japio
    • 目的:提高高温下螺栓的抗应力腐蚀开裂性能。 水环境,通过准备在高温下在间隙下使用的螺栓和应力作用条件。 来自Ni合金的水环境。 构成:在高温下在间隙和应力作用条件下使用的螺栓。 沸水型或压水型核反应堆内的水环境由Ni合金制成, 基础为15-25%Cr,1-8%Mo,0.4-2%Al,0.7-3%Ti,0.7-4.5%Nb,小于40%Fe和超过40%的Ni。 在这种情况下,包含的Al,Ti和Nb的含量在3.5%<= 2Al + Ti + 0.5Nb <= 5.5%的关系所示的范围内。 该镍合金在其结构的奥氏体相中含有一个或多个γ'相和γ“相,并且适用于在高温下使用的具有优异的应力腐蚀开裂性的螺栓材料。 水环境。