    • 10. 发明授权
    • Hydrothermal activation of acid zeolites with alumina
    • 用氧化铝水热激活酸性沸石
    • US4468475A
    • 1984-08-28
    • US512511
    • 1983-07-11
    • Guenter H. Kuehl
    • Guenter H. Kuehl
    • B01J29/40B01J29/28B01J37/26
    • B01J29/40B01J2229/26B01J2229/42
    • In the process for activating high-silica zeolite catalyst with alumina activating agent wherein a crystalline zeolite catalyst having a silica:alumina ratio greater than 70 and a constraint index of 1 to 12 is contacted with the activating agent at elevated temperature, the improvement which comprises: hydrothermally treating an intimate mixture of zeolite catalyst and an effective amount of activating agent in contact with an aqueous liquid phase under reaction conditions to increase the cracking activity of the catalyst.The activated catalyst product may be produced by hydrothermal treatment of a composite mixture of zeolite and hydrated alumina binder material. The preferred zeolites are acid ZSM-5 type crystalline materials having a silica:alumina ratio of at least 2000:1.
    • 在氧化铝活化剂活化高硅石沸石催化剂的方法中,其中二氧化硅:氧化铝比大于70且约束指数为1至12的结晶沸石催化剂在升高的温度下与活化剂接触,其改进包括 :在反应条件下水热处理沸石催化剂和水性液相接触的有效量的活化剂的紧密混合物,以增加催化剂的裂解活性。 活化的催化剂产物可以通过水热处理沸石和水合氧化铝粘结剂材料的复合混合物来制备。 优选的沸石是二氧化硅:氧化铝比至少为2000:1的酸性ZSM-5型结晶材料。