    • 1. 发明授权
    • Substrates provided with a microstructured surface, methods for the production thereof, and their use
    • 具有微结构表面的基板,其制造方法及其用途
    • US06649266B1
    • 2003-11-18
    • US09959023
    • 2001-10-15
    • Frank GrossMartin MennigPeter W. OliveiraHelmut SchmidtStefan Sepeur
    • Frank GrossMartin MennigPeter W. OliveiraHelmut SchmidtStefan Sepeur
    • B32B1700
    • C09K3/18B05D1/40B05D5/08B08B17/06B08B17/065B29C59/026B29C2059/023Y10T428/31Y10T428/315Y10T428/31612Y10T428/31663
    • Substrates provided with a microstructured surface have a surface layer which (a) comprises a composition comprising condensates of one or more hydrolysable compounds of at least one element M from main groups III to V and/or transition groups II to IV of the Periodic Table of the Elements, at least some of these compounds containing not only hydrolysable groups A but also non-hydrolysable, carbon-containing groups B and the total molar ratio of groups A to groups B in the parent monomeric starting compounds being from 10:1 to 1:2, from 0.1 to 100 mol % of the groups B being groups B′ containing on average from 5 to 30 fluorine atoms which are attached to one or more aliphatic carbon atoms distanced from M by at least two atoms, and (b) has a microstructuring of such kind that the contact angle with respect to water or hexadecane is at least 5° higher than the contact angle of a corresponding smooth surface. The substrates provided with a microstructured surface are particularly suitable as transparent or translucent easy-to-clean systems.
    • 提供有微结构化表面的底物具有表面层,其表面层包含一种组合物,该组合物包含至少一种元素M的主要组III至V的一种或多种可水解化合物的缩合物和/或周期表的转变基团II至IV的组合物 元素,这些化合物中的至少一些化合物不仅含有可水解基团A,而且含有不可水解的含碳基团B,并且母体单体起始化合物中基团A与基团B的总摩尔比为10:1至1 2,0.1〜100摩尔%的基团B为含有平均5〜30个氟原子的基团B',其通过至少两个原子与一个或多个与M离开的一个或多个脂族碳原子连接,(b)具有 这种微结构化使得相对于水或十六烷的接触角比相应的光滑表面的接触角高至少5°。具有微结构化表面的基底特别合适 作为透明或半透明的易于清洁的系统。
    • 9. 发明授权
    • Method for producing thermoshaped substrates coated with a sol-gel lacquer
    • 制备涂有溶胶 - 凝胶漆的热固性基材的方法
    • US06482525B1
    • 2002-11-19
    • US09763521
    • 2001-02-23
    • Reiner KasemannNora KunzeHelmut SchmidtStefan Sepeur
    • Reiner KasemannNora KunzeHelmut SchmidtStefan Sepeur
    • B32B904
    • C08J7/047C08J2483/00C09D4/00Y10T428/31663C08G77/00
    • What is described is a method for producing a thermally shaped substrate coated with a sol-gel coating material, in which the sol-gel coating material comprises one or more hydrolyzable silanes, which may have been hydrolyzed to form a precondensate, and, if desired, a crosslinking agent, at least some of the hydrolyzable silanes containing on a non-hydrolyzable substituent a functional group by way of which crosslinking is possible, and in which A) the sol-gel coating material is applied to a thermally shapable substrate, B) the applied sol-gel coating material is partially precrosslinked and/or dried, C) the substrate coated with the sol-gel coating material is subsequently shaped thermally, and D) during and/or after the thermal shaping the sol-gel coating material is cured completely by means of thermal or photochemical crosslinking.
    • 描述的是制备涂覆有溶胶 - 凝胶涂层材料的热定形基材的方法,其中溶胶 - 凝胶涂层材料包含一种或多种可水解的硅烷,其可以被水解形成预缩合物,如果需要 交联剂,至少一些在不可水解取代基上含有官能团的可水解硅烷,其中交联是可能的,其中A)将溶胶 - 凝胶涂料施加到可热成形的基材上,B) 所施加的溶胶 - 凝胶涂层材料被部分预先交联和/或干燥,C)涂覆有溶胶 - 凝胶涂层材料的基材随后被热成型,并且D)在热成型期间和/或之后,溶胶 - 凝胶涂层材料被固化 完全通过热或光化学交联。
    • 10. 发明授权
    • Process of preserving paper
    • 保存纸张的过程
    • US6071475A
    • 2000-06-06
    • US068905
    • 1998-05-21
    • Helmut SchmidtReiner KasemannStefan SepeurHelmut Duddeck
    • Helmut SchmidtReiner KasemannStefan SepeurHelmut Duddeck
    • D21H25/18
    • D21H25/18
    • A process is disclosed for preserving paper involving the following steps:(a) a plurality of paper layers in contact with one another at least in regions is simultaneously brought into contact with a preservative fluid containing polycondensates based on one or more hydrolytic polycondensation-capable compounds of elements M of main groups III-V and sub-groups II-IV of the Periodic Table; in said polycondensates, at least one organic group (G) with at least two carbon atoms and for each carbon atom at least one atom selected from hydrogen or fluorine and without polar substituents is bound, either directly via one of the carbon atoms or via a connecting group A, to at least 0.1% of the central atoms M; and(b) the paper thus treated with the preservative fluid is dried and/or hardened.
    • PCT No.PCT / EP96 / 05176 Sec。 371日期1998年5月21日 102(e)日期1998年5月21日PCT 1996年11月22日PCT公布。 出版物WO97 / 19224 日期1997年5月29日公开了一种用于保存纸的方法,涉及以下步骤:(a)至少在区域中彼此接触的多个纸层同时与含有缩聚物的防腐液接触,所述防缩液基于一种或多种水解 主要III-V族和元素周期表Ⅱ-Ⅳ族元素M的缩聚能力化合物; 在所述缩聚物中,至少一个具有至少两个碳原子的有机基团(G)和对于每个碳原子,至少一个选自氢或氟并且没有极性取代基的原子直接通过碳原子之一或经由 将A族连接至至少0.1%的中心原子M; 和(b)用防腐剂流体处理的纸被干燥和/或硬化。