    • Alkoxylated/cationically modified amide-containing polymers
    • 烷氧基化/阳离子改性含酰胺的聚合物
    • US4970290A
    • 1990-11-13
    • US163220
    • 1988-02-26
    • Dodd W. Fong
    • Dodd W. Fong
    • C08F8/32C08F8/44
    • C08F8/44C08F2800/10
    • Pendant amide-containing polymers may be modified in such a way to achieve substituted pendant amide groups described by the structure: ##STR1## wherein: R is chosen from the group consisting of hydrogen and lower alkyl (C.sub.1 -C.sub.4) groups,R.sup.1 is a multivalent hydrocarbonaceous bridging group containing from 1-20 carbon atoms,X is a tertiary amine or a quaternary ammonium salt functional group,Y is chosen from the group consisting of --OR'", and ##STR2## and mixtures thereof, and whereinR'" is chosen from the group consisting of hydrogen, alkyl groups, aryl alkyl, aryl groups and the like,q ranges from 0-50,m ranges from -24,n ranges from 0-24, provided that the sum of m plus n is at least 1.Processes for achieving modified polymers having the above functional group is also disclosed.
    • 可以以这样的方式修饰含酰胺的聚合物,以实现由以下结构描述的取代的侧酰胺基团:其中:R选自氢和低级烷基(C 1 -C 4)基团,R 1是 含有1-20个碳原子的多价烃基桥接基团,X是叔胺或季铵盐官能团,Y选自-OR“和”IMAGE“及其混合物,其中R “选自氢,烷基,芳基烷基,芳基等,q范围为0-50,m的范围为-24,n的范围为0-24,条件是m的和 加上n至少为1.还公开了获得具有上述官能团的改性聚合物的方法。
    • 9. 发明授权
    • Cooling water corrosion inhibition method
    • 冷却水腐蚀抑制方法
    • US4923634A
    • 1990-05-08
    • US155393
    • 1988-02-12
    • John E. HootsDonald A. JohnsonDodd W. FongJames F. Kneller
    • John E. HootsDonald A. JohnsonDodd W. FongJames F. Kneller
    • C23F11/08
    • C23F11/08
    • A method for inhibiting corrosion in industrial cooling waters which contain hardness and a pH of at least 6.5, by dosing the water with a composition which comprises a water-soluble inorganic phosphate capable of inhibiting corrosion in an aqueous alkaline environment and a hydrocarbon polymer containing an N-substituted acrylamide polymers with an amide structure as follows: ##STR1## where R.sub.2 is hydrogen or methyl, where R.sub.1 is a hydrogen or an alkyl and R is alkylene or phenylene, and X is sulfonate, (poly)hydroxyl, (poly)carboxyl or carbonyl, and combinations thereof; or containing derivatized maleic anhydride homo-, co- and terpolymers having N-substituted maleamic acid units, N-substituted maleimide units and maleic acid (and salts) units having a structure as follows: ##STR2## where R.sub.1, R.sub.2 and R.sub.3 are each independently chosen from the group consisting of hydrogen, hydroxyl, carboxyalkyl, carboxyamide, phenyl, substituted phenyl, linear or branched alkyl of from one to ten carbon atoms,and substituted alkyl of from one to ten carbon atoms, where the substituent is phosphonic acid; phosphinic acid; phosphate ester; sulfonic acid; sulfate ester, carboxyamide, (poly)carboxy and (poly)hydroxy, alkoxy and carboxylate ester groups; and combinations thereof.
    • 一种通过用含有能够在碱性水溶液中抑制腐蚀的水溶性无机磷酸盐的组合物给予水,并且含有至少为6.5的烃聚合物的含有硬度和pH至少为6.5的工业冷却水中的腐蚀的方法 具有酰胺结构的N-取代丙烯酰胺聚合物如下:其中R 2是氢或甲基,其中R 1是氢或烷基,R是亚烷基或亚苯基,X是磺酸根,(多)羟基,(聚) 羧基或羰基,及其组合; 或含有具有N-取代的马来酰胺酸单元,N-取代的马来酰亚胺单元和具有如下结构的马来酸(和盐)单元的衍生化马来酸酐均聚物,共聚物和三元共聚物:其中R 1,R 2和R 3各自为 独立地选自氢,羟基,羧基烷基,羧基酰胺,苯基,取代的苯基,1至10个碳原子的直链或支链烷基和1至10个碳原子的取代烷基,其中取代基是膦酸; 次膦酸 磷酸酯; 磺酸 硫酸酯,羧酰胺,(多)羧基和(多)羟基,烷氧基和羧酸酯基团; 及其组合。
    • 10. 发明授权
    • Process for preparing high molecular weight hydrophobic acrylamide
polymers
    • 制备高分子量疏水性丙烯酰胺聚合物的方法
    • US4921903A
    • 1990-05-01
    • US256339
    • 1988-10-11
    • Dodd W. Fong
    • Dodd W. Fong
    • C08F8/32
    • C08F8/32
    • A process of making a water-in-oil emulsion which contains from 5-60% by weight of a hydrophobic acrylamide terpolymer composed of the random repeating units: ##STR1## where: R is methyl or hydrogen,M is hydrogen, alkali metal, ammonia, or amine,R.sup.1 is a hydrophobic radical,with the mol ratio of A:B:C being A(2-50):B(50-98):C(0.1-15), which comprises reacting a 5-60% by weight water-in-oil emulsion of an acrylamide polymer with a hydrophobic amine at a temperature above 120.degree. C. for a period of time sufficient to transamidate the acrylamide groups in the acrylamide polymer with the hydrophobic amine.
    • 一种制备油包水乳液的方法,其包含5-60重量%的由无规重复单元组成的疏水丙烯酰胺三元共聚物:其中:R是甲基或氢,M是氢,碱金属, 氨或胺,R1是疏水基团,A:B:C的摩尔比为A(2-50):B(50-98):C(0.1-15),其包括使5-60 重量%的丙烯酰胺聚合物与疏水性胺在温度高于120℃下的油包水乳液一段足以使丙烯酰胺聚合物中的丙烯酰胺基团与疏水胺转酰胺化的时间。