热词
    • 6. 发明专利
    • Member resistant to biodiesel fuel
    • 耐生物柴油燃料的会员
    • JP2013173930A
    • 2013-09-05
    • JP2013033596
    • 2013-02-22
    • Daikin Industries Ltdダイキン工業株式会社
    • OTA DAISUKEUEDA AKINORIKADOWAKI YUTAEDA MAYUKOKITAICHI MASAKIDOI MICHIKOYAMAMURA KAZUHIROFUKUOKA SHOJI
    • C08J3/24
    • PROBLEM TO BE SOLVED: To provide a member resistant to biodiesel fuel, the member being excellent in resistance to biodiesel fuel and having excellent tensile properties and cracking resistance at high temperatures.SOLUTION: A member resistant to biodiesel fuel can be obtained by crosslinking a fluororubber composition including a fluororubber (A) and a carbon black (B). In the member resistant to the biodiesel fuel, the crosslinked fluororubber has a loss elastic modulus E'' of ≥400 kPa and ≤6,000 kPa, in a dynamic viscoelasticity test carried out in a condition that: measurement temperature is 160°C; tensile strain is 1%; a static tension value when a static load condition at distortion variance is made constant is 157 cN; and frequency is 10 Hz.
    • 要解决的问题:提供耐生物柴油燃料的构件,其耐生物柴油燃料性能优异,并且在高温下具有优异的拉伸性能和抗开裂性。解决方案:可通过将氟橡胶交联而获得耐生物柴油燃料的构件 组合物,其包含氟橡胶(A)和炭黑(B)。 在耐生物柴油燃料的构件中,在测定温度为160℃的条件下进行的动态粘弹性试验中,交联氟橡胶的损失弹性模量E“≥400kPa,≤6000kPa。 拉伸应变为1%; 当变形方差的静态负载条件为常数时的静态张力值为157 cN; 频率为10 Hz。
    • 9. 发明专利
    • Laminate
    • 层压板
    • JP2012061644A
    • 2012-03-29
    • JP2010206138
    • 2010-09-14
    • Daikin Industries LtdDaiso Co Ltdダイキン工業株式会社ダイソー株式会社
    • HAMAGUCHI KOSHIROKITAGAWA NORIKIMASUI TOSHIAKIINABA TSUYOSHIKUWASHIMA MASAMITAEDA MAYUKO
    • B32B25/08B32B1/08C08G65/24C08K3/22C08K3/36C08K5/42C08L63/00C08L71/03F16L11/04
    • PROBLEM TO BE SOLVED: To provide a vulcanized laminate with a rubber layer and a fluororesin layer firmly bonded together without treating their surfaces and using an adhesive.SOLUTION: This laminate includes the rubber layer (A) and the fluororesin layer (B) laminated on the former. In addition, the rubber layer (A) is formed of a rubber composition for vulcanization, and contains epichlorohydrin rubber (a1), at least one kind of a chemical compound (a2) selected from a group composed of p-toluenesulfonate of 1,8-diazabicyclo(5.4.0)undecene-7 or 1,5-diazabicyclo(4.3.0)-nonene-5, a phenol salt, phenol resinate, orthophthalate, formate and octylate, a magnesium oxide (a3), silica (a4) and epoxy resin (a5). The fluororesin layer (B) contains a fluoropolymer (b1) with a copolymerization unit derived from chlorotrifluoroethylene.
    • 要解决的问题:提供具有橡胶层和氟树脂层的硫化层压板,其不用处理它们的表面并使用粘合剂牢固地结合在一起。 解决方案:该层压体包括层压在前者上的橡胶层(A)和氟树脂层(B)。 另外,橡胶层(A)由硫化用橡胶组合物形成,并含有表氯醇橡胶(a1),选自由对甲苯磺酸盐组成的组中的至少一种化合物(a2) 苯酚盐,苯酚树脂酸盐,邻苯二甲酸盐,甲酸盐和辛酸盐,氧化镁(a3),二氧化硅(a4),二氧化硅(a4),二氯甲烷 和环氧树脂(a5)。 氟树脂层(B)含有具有来自三氟氯乙烯的共聚单元的含氟聚合物(b1)。 版权所有(C)2012,JPO&INPIT