    • 1. 发明申请
    • APPARATUS AND METHOD FOR FORMING A GLASS SHEET
    • 用于形成玻璃片的装置和方法
    • US20160272528A1
    • 2016-09-22
    • US15033259
    • 2014-10-29
    • CORNING INCORPORATED
    • Charles Michael Darcangelo
    • C03B17/06C03B17/02
    • C03B17/065C03B17/02C03B17/064C03B17/068C03B33/0215
    • A method includes forming a continuous ribbon of glass. The continuous ribbon includes a first surface, a second surface opposite the first surface, a first edge region, a second edge region opposite the first edge region, and a central region extending between the first edge region and the second edge region. Each of the first edge region and the second edge region has a greater thickness than the central region of the continuous ribbon. An indented pattern is formed longitudinally along the first edge region of the continuous ribbon by forming a first series of indentations in the first surface of the continuous ribbon and forming a second series of indentations in the second surface of the continuous ribbon. The indented pattern includes intermediate segments interconnected with one another by web by webs. Each intermediate segment is thicker than adjacent webs.
    • 一种方法包括形成连续的玻璃带。 连续带包括第一表面,与第一表面相对的第二表面,第一边缘区域,与第一边缘区域相对的第二边缘区域以及在第一边缘区域和第二边缘区域之间延伸的中心区域。 第一边缘区域和第二边缘区域中的每一个具有比连续带材的中心区域更大的厚度。 通过在连续带的第一表面中形成第一系列凹陷并在连续带的第二表面中形成第二系列凹陷,沿着连续带的第一边缘区域纵向地形成凹入图案。 缩进图案包括通过腹板彼此互相连接的中间片段。 每个中间段比相邻腹板厚。
    • 4. 发明申请
    • METHODS OF FINISHING AN EDGE OF A GLASS SHEET
    • 完成玻璃片边缘的方法
    • US20150190898A1
    • 2015-07-09
    • US14661421
    • 2015-03-18
    • CORNING INCORPORATED
    • Charles Michael DarcangeloAric Bruce ShoreyDaniel Duane StrongDavid Alan Tammaro
    • B24B9/10B24B21/00
    • B24B9/10B24B9/08B24B21/002
    • Methods of finishing an edge of a glass sheet comprise the step of machining the edge of the glass sheet into a predetermined cross-sectional profile along a plane taken transverse to the edge of the glass sheet with an initial average edge strength ESi. The methods also include the step of finishing the edge with at least one finishing member, such as an endless belt, without substantially changing a shape of the predetermined cross-sectional profile. In one example, a wet slurry including an abrasive can be applied to at least one of a finishing member and the edge of the glass sheet. After finishing the edge, example finished average edge strengths ESf can be at least about 250 MPa. In addition or alternatively, in another example, the ratio ESf/ESi can be within a range of from about 1.6 to about 5.6.
    • 完成玻璃板的边缘的方法包括将玻璃板的边缘沿着具有初始平均边缘强度ESi的横向于玻璃板的边缘的平面加工成预定的横截面轮廓的步骤。 该方法还包括用至少一个精加工构件(例如环形带)来完成边缘的步骤,而基本上不改变预定横截面轮廓的形状。 在一个实例中,包括研磨剂的湿浆料可以施加到精加工构件和玻璃板的边缘中的至少一个。 完成边缘后,实例成品的平均边缘强度ESf可以至少为250MPa。 另外或者在另一个实施例中,ESf / ESi比可以在约1.6至约5.6的范围内。