热词
    • 1. 发明授权
    • Low temperature fired dielectric ceramic composition with flat TC
characteristic and method of making
    • 具有扁平TC特性的低温烧结介电陶瓷组合物及其制备方法
    • US4540676A
    • 1985-09-10
    • US613250
    • 1984-05-23
    • Mike S. H. ChuCharles E. HodgkinsDaniel C. Rose
    • Mike S. H. ChuCharles E. HodgkinsDaniel C. Rose
    • C04B35/46C04B35/468H01B3/12H01G4/12
    • H01G4/1227C04B35/4684
    • A low temperature fired ceramic dielectric composition in which the dielectric constant does not vary from its base value of over 2400 by more than 15 percent over a wide temperature range. A base ceramic preparation (a) and a ceramic flux (b), each consisting essentially of metal oxides or precursors thereof to provide in oxide form (a) 98.0 to 99 weight percent barium titanate, from about 0.97 to about 1.54 weight percent niobium pentoxide and from about 0.19 to about 0.32 weight percent cobalt oxide; (b) from about 16 to about 60 weight percent bismuth titanate, about 8 to about 52 weight percent lead titanate, about 18 to about 35 weight percent zinc oxide and about 5 to about 11 weight percent boron oxide. Manganese dioxide or precursor thereof in amount of from about 0 to 0.114 percent of the combined weight of the base ceramic preparation and ceramic flux is added to the metal oxides or precursors of the base ceramic preparation and ceramic flux and the mixture is fired at a temperature less than about 1150.degree. C.
    • 一种低温烧制陶瓷电介质组合物,其中介电常数在宽的温度范围内,其基值超过2400的值不会超过15%。 一种基础陶瓷制剂(a)和一种陶瓷助熔剂(b),各自主要由金属氧化物或其前体组成,以氧化物形式(a)98.0至99重量%的钛酸钡,约0.97至约1.54重量%的五氧化二铌 和约0.19至约0.32重量%的氧化钴; (b)约16至约60重量%的钛酸铋,约8至约52重量%的钛酸铅,约18至约35重量%的氧化锌和约5至约11重量%的氧化硼。 将二氧化锰或其前体的量占基础陶瓷制剂和陶瓷助熔剂的总重量的约0至1.114%加入到基础陶瓷制剂和陶瓷助熔剂的金属氧化物或前体中,并将​​混合物在温度 小于约1150℃