    • 1. 发明申请
    • Repairing damage to low-k dielectric materials using silylating agents
    • 使用硅烷化剂修复对低k电介质材料的损坏
    • US20050095840A1
    • 2005-05-05
    • US10940682
    • 2004-09-15
    • Anil BhanapTeresa RamosNancy IwamotoRoger LeungAnanth Naman
    • Anil BhanapTeresa RamosNancy IwamotoRoger LeungAnanth Naman
    • H01L21/4763
    • H01L21/31058H01L21/02203H01L21/02216H01L21/02282H01L21/3122H01L21/76801
    • A method for restoring hydrophobicity to the surfaces of organosilicate glass dielectric films which have been subjected to an etchant or ashing treatment. These films are used as insulating materials in the manufacture of integrated circuits to ensure low and stable dielectric properties in these films. The method deters the formation of stress-induced voids in these films. An organosilicate glass dielectric film is patterned to form vias and trenches by subjecting it to an etchant or ashing reagent in such a way as to remove at least a portion of previously existing carbon containing moieties and reduce hydrophobicity of said organosilicate glass dielectric film. The vias and trenches are thereafter filled with a metal and subjected to an annealing treatment. After the film is subjected to the etchant or ashing reagent, but before being subjected to an annealing treatment, the film is contacted with a toughening agent composition to restore some of the carbon containing moieties and increase the hydrophobicity of the organosilicate glass dielectric film.
    • 用于恢复已进行蚀刻剂或灰化处理的有机硅酸盐玻璃介电膜表面的疏水性的方法。 这些膜在集成电路的制造中用作绝缘材料,以确保这些膜中的低和稳定的介电性能。 该方法阻止了这些膜中应力诱发的空隙的形成。 通过使有机硅酸盐玻璃电介质膜经受蚀刻剂或灰化试剂以形成通孔和沟槽,以除去至少一部分先前存在的含碳部分并降低所述有机硅酸盐玻璃电介质膜的疏水性。 之后通过通孔和沟槽填充金属并进行退火处理。 在将薄膜进行蚀刻剂或灰化试剂之后,但在进行退火处理之前,使膜与增韧剂组合物接触以还原一些含碳部分并增加有机硅酸盐玻璃电介质膜的疏水性。
    • 6. 发明授权
    • Antireflective coatings for via fill and photolithography applications and methods of preparation thereof
    • 用于通孔填充和光刻应用的抗反射涂层及其制备方法
    • US08992806B2
    • 2015-03-31
    • US13217706
    • 2011-08-25
    • Bo LiJoseph KennedyNancy IwamotoMark A. FradkinMakarem A. HusseinMichael D. GoodnerVictor LuRoger Leung
    • Bo LiJoseph KennedyNancy IwamotoMark A. FradkinMakarem A. HusseinMichael D. GoodnerVictor LuRoger Leung
    • C09K3/00G03F7/11C09D183/04G03F7/075C09D183/08G03F7/09
    • C09D183/04C09D183/08G03F7/0751G03F7/0752G03F7/091
    • An absorbing composition is described herein that includes at least one inorganic-based compound, at least one absorbing compound, and at least one material modification agent. In addition, methods of making an absorbing composition are also described that includes: a) combining at least one inorganic-based compound, at least one absorbing compound, at least one material modification agent, an acid/water mixture, and one or more solvents to form a reaction mixture; and b) allowing the reaction mixture to form the absorbing composition at room temperature. Another method of making an absorbing composition includes: a) combining at least one inorganic-based compound, at least one absorbing compound, at least one material modification agent, an acid/water mixture, and one or more solvents to form a reaction mixture; and b) heating the reaction mixture to form the absorbing composition. Yet another method of making an absorbing composition is described that includes: a) combining at least one inorganic-based compound, at least one absorbing compound, at least one material modification agent, and one or more solvents to form a reaction mixture, wherein the at least one material modification agent comprises at least one acid and water; and b) heating the reaction mixture to form an absorbing material, a coating or a film. In other methods of making an absorbing composition described herein, those methods include: a) combining at least one inorganic-based compound, at least one absorbing compound, at least one material modification agent, and one or more solvents to form a reaction mixture, wherein the at least one material modification agent comprises at least one acid and water; and b) allowing the reaction mixture to form an absorbing material, a coating or a film.
    • 本文描述的吸收组合物包括至少一种无机基化合物,至少一种吸收化合物和至少一种材料改性剂。 此外,还描述了制备吸收组合物的方法,其包括:a)将至少一种无机基化合物,至少一种吸收化合物,至少一种材料改性剂,酸/水混合物和一种或多种溶剂 形成反应混合物; 和b)使反应混合物在室温下形成吸收组合物。 制备吸收组合物的另一种方法包括:a)将至少一种无机基化合物,至少一种吸收化合物,至少一种材料改性剂,酸/水混合物和一种或多种溶剂组合以形成反应混合物; 和b)加热反应混合物以形成吸收组合物。 描述了制备吸收组合物的另一种方法,其包括:a)将至少一种无机基化合物,至少一种吸收化合物,至少一种材料改性剂和一种或多种溶剂组合以形成反应混合物,其中 至少一种材料改性剂包含至少一种酸和水; 和b)加热反应混合物以形成吸收材料,涂层或膜。 在制备本文所述的吸收组合物的其它方法中,这些方法包括:a)将至少一种无机基化合物,至少一种吸收化合物,至少一种材料改性剂和一种或多种溶剂组合以形成反应混合物, 其中所述至少一种材料改性剂包含至少一种酸和水; 和b)使反应混合物形成吸收材料,涂层或膜。
    • 7. 发明申请
    • Antireflective Coatings for Via Fill and Photolithography Applications and Methods of Preparation Thereof
    • 用于通孔填充和光刻的抗反射涂层及其制备方法
    • US20120001135A1
    • 2012-01-05
    • US13217706
    • 2011-08-25
    • Bo LiJoseph KennedyNancy IwamotoMark A. FradkinMakarem A. HusseinMichael D. GoodinVictor LuRoger Leung
    • Bo LiJoseph KennedyNancy IwamotoMark A. FradkinMakarem A. HusseinMichael D. GoodinVictor LuRoger Leung
    • C09K3/00
    • C09D183/04C09D183/08G03F7/0751G03F7/0752G03F7/091
    • An absorbing composition is described herein that includes at least one inorganic-based compound, at least one absorbing compound, and at least one material modification agent. In addition, methods of making an absorbing composition are also described that includes: a) combining at least one inorganic-based compound, at least one absorbing compound, at least one material modification agent, an acid/water mixture, and one or more solvents to form a reaction mixture; and b) allowing the reaction mixture to form the absorbing composition at room temperature. Another method of making an absorbing composition includes: a) combining at least one inorganic-based compound, at least one absorbing compound, at least one material modification agent, an acid/water mixture, and one or more solvents to form a reaction mixture; and b) heating the reaction mixture to form the absorbing composition. Yet another method of making an absorbing composition is described that includes: a) combining at least one inorganic-based compound, at least one absorbing compound, at least one material modification agent, and one or more solvents to form a reaction mixture, wherein the at least one material modification agent comprises at least one acid and water; and b) heating the reaction mixture to form an absorbing material, a coating or a film. In other methods of making an absorbing composition described herein, those methods include: a) combining at least one inorganic-based compound, at least one absorbing compound, at least one material modification agent, and one or more solvents to form a reaction mixture, wherein the at least one material modification agent comprises at least one acid and water; and b) allowing the reaction mixture to form an absorbing material, a coating or a film.
    • 本文描述的吸收组合物包括至少一种无机基化合物,至少一种吸收化合物和至少一种材料改性剂。 此外,还描述了制备吸收组合物的方法,其包括:a)将至少一种无机基化合物,至少一种吸收化合物,至少一种材料改性剂,酸/水混合物和一种或多种溶剂 形成反应混合物; 和b)使反应混合物在室温下形成吸收组合物。 制备吸收组合物的另一种方法包括:a)将至少一种无机基化合物,至少一种吸收化合物,至少一种材料改性剂,酸/水混合物和一种或多种溶剂组合以形成反应混合物; 和b)加热反应混合物以形成吸收组合物。 描述了制备吸收组合物的另一种方法,其包括:a)将至少一种无机基化合物,至少一种吸收化合物,至少一种材料改性剂和一种或多种溶剂组合以形成反应混合物,其中 至少一种材料改性剂包含至少一种酸和水; 和b)加热反应混合物以形成吸收材料,涂层或膜。 在制备本文所述的吸收组合物的其它方法中,这些方法包括:a)将至少一种无机基化合物,至少一种吸收化合物,至少一种材料改性剂和一种或多种溶剂组合以形成反应混合物, 其中所述至少一种材料改性剂包含至少一种酸和水; 和b)使反应混合物形成吸收材料,涂层或膜。
    • 8. 发明申请
    • Antireflective coatings for via fill and photolithography applications and methods of preparation thereof
    • 用于通孔填充和光刻应用的抗反射涂层及其制备方法
    • US20050171277A1
    • 2005-08-04
    • US10717028
    • 2003-11-18
    • Bo LiJoseph KennedyNancy IwamotoVictor LuRoger LeungMark FradkinMakarem HusseinMichael Goodner
    • Bo LiJoseph KennedyNancy IwamotoVictor LuRoger LeungMark FradkinMakarem HusseinMichael Goodner
    • C08G20060101C08L83/04C09D183/04C09D183/08G03F7/09
    • C09D183/04C09D183/08G03F7/0751G03F7/0752G03F7/091
    • An absorbing composition is described herein that includes at least one inorganic-based compound, at least one absorbing compound, and at least one material modification agent. In addition, methods of making an absorbing composition are also described that includes: a) combining at least one inorganic-based compound, at least one absorbing compound, at least one material modification agent, an acid/water mixture, and one or more solvents to form a reaction mixture; and b) allowing the reaction mixture to form the absorbing composition at room temperature. Another method of making an absorbing composition includes: a) combining at least one inorganic-based compound, at least one absorbing compound, at least one material modification agent, an acid/water mixture, and one or more solvents to form a reaction mixture; and b) heating the reaction mixture to form the absorbing composition. Yet another method of making an absorbing composition is described that includes: a) combining at least one inorganic-based compound, at least one absorbing compound, at least one material modification agent, and one or more solvents to form a reaction mixture, wherein the at least one material modification agent comprises at least one acid and water; and b) heating the reaction mixture to form an absorbing material, a coating or a film. In other methods of making an absorbing composition described herein, those methods include: a) combining at least one inorganic-based compound, at least one absorbing compound, at least one material modification agent, and one or more solvents to form a reaction mixture, wherein the at least one material modification agent comprises at least one acid and water; and b) allowing the reaction mixture to form an absorbing material, a coating or a film.
    • 本文描述的吸收组合物包括至少一种无机基化合物,至少一种吸收化合物和至少一种材料改性剂。 此外,还描述了制备吸收组合物的方法,其包括:a)将至少一种无机基化合物,至少一种吸收化合物,至少一种材料改性剂,酸/水混合物和一种或多种溶剂 形成反应混合物; 和b)使反应混合物在室温下形成吸收组合物。 制备吸收组合物的另一种方法包括:a)将至少一种无机基化合物,至少一种吸收化合物,至少一种材料改性剂,酸/水混合物和一种或多种溶剂组合以形成反应混合物; 和b)加热反应混合物以形成吸收组合物。 描述了制备吸收组合物的另一种方法,其包括:a)将至少一种无机基化合物,至少一种吸收化合物,至少一种材料改性剂和一种或多种溶剂组合以形成反应混合物,其中 至少一种材料改性剂包含至少一种酸和水; 和b)加热反应混合物以形成吸收材料,涂层或膜。 在制备本文所述的吸收组合物的其它方法中,这些方法包括:a)将至少一种无机基化合物,至少一种吸收化合物,至少一种材料改性剂和一种或多种溶剂组合以形成反应混合物, 其中所述至少一种材料改性剂包含至少一种酸和水; 和b)使反应混合物形成吸收材料,涂层或膜。
    • 10. 发明授权
    • Nanoporous polymers crosslinked via cyclic structures
    • 通过环状结构交联的纳米多孔聚合物
    • US06172128B2
    • 2001-01-09
    • US09544722
    • 2000-04-06
    • Kreisler LauTian-An ChenRoger Leung
    • Kreisler LauTian-An ChenRoger Leung
    • C08J902
    • C08J3/246C08J9/26C08J2201/046
    • Nanoporous polymeric materials are fabricated in which polymeric strands are crosslinked via ring structures. Preferred ring structures are formed de novo during crosslinking, and at least some of the ring structures are preferably included in the backbones of the strands. At least one of the ring structures may advantageously comprise an aromatic structure, and may more advantageously comprise a benzyl moiety. Especially preferred polymers comprise a poly(arylene ether) synthesized from a difluoroaromatic portion and an aromatic bisphenolic portion. In another preferred aspect, the difluoroaromatic portions of the poly(arylene ether) carry at least two different crosslinking functionalities. In an even more preferred aspect, the crosslinking functionalities comprise an ethynyl and a tetracyclone. Nanoporosity is preferably introduced by thermolyzing one or more thermolabile portions in the crosslinked polymer. An especially preferred thermolabile portion comprises ethylene glycol-poly(caprolactone).
    • 制造纳米多孔聚合材料,其中聚合物链通过环结构交联。 优选的环结构在交联期间从头形成,并且至少一些环结构优选包含在该链的主链中。 至少一个环结构可以有利地包含芳族结构,并且可以更有利地包含苄基部分。 特别优选的聚合物包括由二氟芳族部分和芳族双酚部分合成的聚(亚芳基醚)。 在另一个优选的方面,聚(亚芳基醚)的二氟芳香族部分携带至少两种不同的交联官能团。 在更优选的方面,交联官能团包括乙炔基和四环。 优选通过热交换聚合物中的一个或多个热不稳定部分来引入纳米孔。 特别优选的耐热不稳定部分包括乙二醇 - 聚(己内酯)。