    • Biodegradable polyestreramide and a process of preparing
    • 可生物降解的聚甲基丙烯酰胺和一种制备方法
    • US06353084B1
    • 2002-03-05
    • US08860755
    • 1997-07-07
    • Volker WarzelhanGunnar SchornickEdwin BaumannUrsula SeeligerMotonori YamamotoGerhard Ramlow
    • Volker WarzelhanGunnar SchornickEdwin BaumannUrsula SeeligerMotonori YamamotoGerhard Ramlow
    • C08G6944
    • C08G69/44C08G18/606Y02W30/43
    • Biodegradable polyesteramides as defined in the specification are obtained by reacting a mixture consisting essentially of a1) a mixture consisting essentially of 35 to 95 mol % of adipic acid or ester-forming derivatives thereof, 5 to 65 mol % of terephthalic acid or ester-forming derivatives thereof, and 0 to 5 mol % of a compound containing sulfonate groups, a2) a mixture consisting essentially of 95.5 to 0.5 mol % of a dihydroxy compound, 0.5 to 99.5 mol % of an amino-C2-C12-alkanol or an amino-C5-C10-cycloalkanol, 0 to 50 mol % of a diamino-C1-C8-alkane, and 0 to 50 mol % of a 2,2′-bisoxazoline of the formula I  wherein R1 is as set forth in the specification, and a3) 0 to 5 mol %, based on a1), of a compound D as set forth in the specification; and other biodegradable polymers and thermoplastic molding compositions, their manufacture and their use for producing biodegradable moldings, adhesives, foams, and coatings.
    • 通过使基本上由以下组成的混合物,将主要由35〜95摩尔%的己二酸或其成酯性衍生物组成的混合物,5〜65摩尔%的对苯二甲酸或其成酯衍生物 ,和0〜5摩尔%的含有磺酸酯基的化合物,a2)基本上由95.5〜0.5摩尔%的二羟基化合物组成的混合物,0.5〜99.5摩尔%的氨基-C2-C12烷醇或氨基-C5 -C 10 - 环烷醇,0〜50摩尔%的二氨基-C 1 -C 8烷烃和0〜50摩尔%的式I的2,2'-双恶唑啉,其中R1如说明书所述,和a3)0 至5摩尔%,基于a1)制备的化合物D;以及其它可生物降解的聚合物和热塑性模塑组合物,其制造及其用于生产可生物降解的模制品,粘合剂,泡沫和涂料的用途。
    • 9. 发明授权
    • Biodegradable polymers, preparation thereof and use thereof for producing biodegradable moldings
    • 生物可降解聚合物,其制备方法及其生产可降解模塑制品的用途
    • US06303677B1
    • 2001-10-16
    • US09611555
    • 2000-07-07
    • Volker WarzelhanGunnar SchornickBernd BruchmannUrsula SeeligerMotonori YamamotoPeter Bauer
    • Volker WarzelhanGunnar SchornickBernd BruchmannUrsula SeeligerMotonori YamamotoPeter Bauer
    • C08K5092
    • C08L3/02C08G18/4216C08G18/4219C08G18/4277C08G18/428C08G18/4286C08G18/4676C08G18/6659C08G63/20C08G63/60C08G2230/00C08L75/06C09D167/00C09K17/52Y02A40/284Y10S525/938Y10T428/31547Y10T428/31786Y10T428/31794C08L2666/02C08L2666/26C08L2666/36
    • Biodegradable polyesters P1 obtainable by reaction of a mixture consisting essentially of (a1) a mixture consisting essentially of from 35 to 95 mol % of adipic acid or ester-forming derivatives thereof or mixtures thereof, from 5 to 65 mol % of terephthalic acid or ester-forming derivatives thereof or mixtures thereof, and from 0 to 5 mol % of a sulfonate compound, the sum of the individual mole percentages being 100 mol %, and (a2) a dihydroxy compound selected from the group consisting of C2-C6-alkanediols and CS-C10-cycloalkanediols, the molar ratio of (a1) to (a2) being chosen within the range from 0.4:1 to 1.5:1, with the proviso that the polyesters P1 have a molecular weight (Mn) within the range from 5000 to 50,000 g/mol, a viscosity number within the range from 30 to 350 g/ml (measured in 50:50 w/w o-dichlorobenzene/phenol at a concentration of 0.5% by weight of polyester P1 at 25° C.) and a melting point within the range from 50 to 170° C. and with the further proviso that the polyesters P1 are prepared using from 0.01 to mol %, based on the molar quantity used of component (a1), of a compound D having at least three groups capable of ester formation, and further biodegradable polymers and thermoplastic molding compositions, processes for the preparation thereof, use thereof for producing biodegradable moldings, and adhesives, biodegradable moldings, foams and blends with starch obtainable from the polymers or molding compositions of the present invention.
    • 可生物降解的聚酯P1可通过基本上由(a1)基本上由35至95摩尔%的己二酸或其酯形成衍生物或其混合物组成的混合物,混合物,5-65摩尔%的对苯二甲酸或酯 - 形成其衍生物或其混合物,和0-5mol%的磺酸盐化合物,各摩尔百分比的总和为100mol%,和(a2)选自C2-C6-烷二醇和CS的二羟基化合物 -C1-环烷二醇,(a1)与(a2)的摩尔比选择在0.4:1至1.5:1的范围内,条件是聚酯P1的分子量(Mn)在5000至 50,000g / mol,粘度数在30-350g / ml的范围内(在25℃下在50:50w / w邻二氯苯/苯酚中的浓度为聚酯P1的0.5重量%测量)和 熔点在50至170℃的范围内,进一步的条件是, 基于组分(a1)使用的摩尔量,具有至少三个能够进行酯形成的基团的化合物D和其它可生物降解的聚合物和热塑性模塑组合物,制备P1的制备方法 其可用于生产可生物降解的成型品,以及可从本发明的聚合物或模塑组合物获得的粘合剂,可生物降解的模制品,泡沫和与淀粉的共混物。
    • 10. 发明授权
    • Process for preparing rubber-modified moulding compounds
    • 制备橡胶改性模塑料的方法
    • US06211297B1
    • 2001-04-03
    • US09319596
    • 1999-06-08
    • Graham Edmund Mc KeeStephan JünglingVolker WarzelhanHermann Gausepohl
    • Graham Edmund Mc KeeStephan JünglingVolker WarzelhanHermann Gausepohl
    • C08L2300
    • C08F20/12
    • Preparation of rubber-modified molding compositions comprises a1) anionic polymerization of a mixture (A) comprising acrylate derivatives or methacrylate derivatives or acrylate derivatives and methacrylate derivatives and a solvent, if desired comprising olefinically unsaturated compounds which are not an acrylate derivative or a methacrylate derivative, or a2) sequential anionic polymerization of acrylate derivatives or methacrylate derivatives or acrylate derivatives and methacrylate derivatives in the presence of a solvent which, if desired, comprises olefinically unsaturated compounds to give block copolymers, and b) subjecting the reaction mixture obtained in a1) or a2) or a1) and a2) to a free-radical-initiated polymerization, if desired after the addition of unsaturated compounds.
    • 橡胶改性成型组合物的制备包括a)如果需要,包含丙烯酸酯衍生物或甲基丙烯酸酯衍生物或丙烯酸酯衍生物和甲基丙烯酸酯衍生物的混合物(A)的阴离子聚合和包含不是丙烯酸酯衍生物或甲基丙烯酸酯衍生物的烯属不饱和化合物的溶剂, ora2)在溶剂存在下丙烯酸酯衍生物或甲基丙烯酸酯衍生物或丙烯酸酯衍生物和甲基丙烯酸酯衍生物的顺序阴离子聚合,如果需要,其包含烯属不饱和化合物以产生嵌段共聚物,和b)使得在a1)或a2)中获得的反应混合物, 或a1)和a2)进行自由基引发的聚合,如果需要,在加入不饱和化合物之后。