    • 1. 发明授权
    • Method for producing polylactic acid block copolymer
    • 聚乳酸嵌段共聚物的制备方法
    • US08211986B2
    • 2012-07-03
    • US12521725
    • 2007-08-10
    • Yuka KomazawaZhen Tang
    • Yuka KomazawaZhen Tang
    • C08G63/91
    • C08G63/08C08L2666/02C08L2666/14C09J153/00
    • It is an object of the present invention to provide a method for producing a polylactic acid block copolymer having high molecular weight, and in lower cost, wherein only a stereo-complex crystal is capable of growing, even when heat melting process is repeated. The present invention relates to a method for producing a polylactic acid block copolymer characterized in that (i) ring-opening polymerization of D-lactide (D component) is carried out in the presence of poly-L-lactic acid (L component), or (ii) ring-opening polymerization of L-lactide (L component) is carried out in the presence of poly-D-lactic acid (D component), and mass ratio of the D component and the L component is the D component/the L component=60/40 to 91/9, or the L component/the D component=60/40 to 91/9.
    • 本发明的目的是提供一种制备具有高分子量的聚乳酸嵌段共聚物的方法,并且即使在重复加热熔融过程时,也只需立体络合物晶体即可生长。 聚乳酸嵌段共聚物的制造方法技术领域本发明涉及聚乳酸嵌段共聚物的制造方法,其特征在于,(I)D-乳酸(D成分)的开环聚合在聚-L-乳酸(L成分)的存在下进行, 或(ii)在聚-D-乳酸(D成分)的存在下进行L-丙交酯(L成分)的开环聚合,D成分和L成分的质量比为D成分/ L成分= 60/40〜91/9,L成分/ D成分= 60/40〜91/9。
    • 4. 发明申请
    • METHOD FOR PRODUCING POLYLACTIC ACID BLOCK COPOLYMER
    • 制备聚酸嵌段共聚物的方法
    • US20100324229A1
    • 2010-12-23
    • US12521725
    • 2004-08-10
    • Yuka KomazawaZhen Tang
    • Yuka KomazawaZhen Tang
    • C08G63/08
    • C08G63/08C08L2666/02C08L2666/14C09J153/00
    • It is an object of the present invention to provide a method for producing a polylactic acid block copolymer having high molecular weight, and in lower cost, wherein only a stereo-complex crystal is capable of growing, even when heat melting process is repeated. The present invention relates to a method for producing a polylactic acid block copolymer characterized in that (i) ring-opening polymerization of D-lactide (D component) is carried out in the presence of poly-L-lactic acid (L component), or (ii) ring-opening polymerization of L-lactide (L component) is carried out in the presence of poly-D-lactic acid (D component), and mass ratio of the D component and the L component is the D component/the L component=60/40 to 91/9, or the L component/the D component=60/40 to 91/9.
    • 本发明的目的是提供一种制备具有高分子量的聚乳酸嵌段共聚物的方法,并且即使在重复加热熔融过程时,也只需立体络合物晶体即可生长。 聚乳酸嵌段共聚物的制造方法技术领域本发明涉及聚乳酸嵌段共聚物的制造方法,其特征在于,(I)D-乳酸(D成分)的开环聚合在聚-L-乳酸(L成分)的存在下进行, 或(ii)在聚-D-乳酸(D成分)的存在下进行L-丙交酯(L成分)的开环聚合,D成分和L成分的质量比为D成分/ L成分= 60/40〜91/9,L成分/ D成分= 60/40〜91/9。