    • 4. 发明授权
    • Aromatic polyester and manufacturing process thereof
    • 芳香族聚酯及其制造方法
    • US07884173B2
    • 2011-02-08
    • US12374538
    • 2007-07-19
    • Kazuteru KohnoEiji KinoshitaTomoyuki Kishino
    • Kazuteru KohnoEiji KinoshitaTomoyuki Kishino
    • C08G63/06C08G63/12
    • C08J5/18C08G63/189C08G63/672C08G63/78C08J2367/02
    • To provide an aromatic polyester which is formed into a film having excellent heat resistance, color, mechanical properties, dimensional stability and gas barrier properties and a manufacturing process thereof; the aromatic polyester comprises a dicabroxylic acid component and a diol component, wherein (i) the dicarboxylic acid component contains 50 to 100 mol % of a recurring unit represented by the following formula (A):  wherein R is an alkylene group having 2 to 10 carbon atoms, (ii) the aromatic polyester has an intrinsic viscosity measured at 35° C. by using a mixed solvent of P-chlorophenol and 1,1,2,2-tetrachloroethane (weight ratio of 40/60) of 0.4 to 3.0; (iii) the aromatic polyester has a content of a recurring unit represented by the following formula (D) of less than 10 mol %: —O—CH2CH2—O—CH2CH2—O—  (D) (iv) the aromatic polyester has a terminal carboxyl group concentration of 200 eq/ton or less; and (v) the aromatic polyester has an alkali metal content of 300 ppm or less.
    • 提供一种形成为具有优异的耐热性,颜色,机械性能,尺寸稳定性和阻气性的薄膜的芳族聚酯及其制造方法; 芳族聚酯包括二硬脂酸组分和二醇组分,其中(i)二羧酸组分含有50至100摩尔%的由下式(A)表示的重复单元:其中R是具有2至10个的亚烷基 碳原子,(ii)芳族聚酯在35℃下通过使用对氯苯酚和1,1,2,2-四氯乙烷(重量比40/60)的混合溶剂测得的特性粘度为0.4〜3.0 ; (iii)芳族聚酯具有由下式(D)表示的小于10mol%的重复单元的含量:-O-CH 2 CH 2 -O-CH 2 CH 2 -O-(D)(iv)芳族聚酯具有 末端羧基浓度为200当量/吨以下; 和(v)芳族聚酯的碱金属含量为300ppm以下。
    • 7. 发明申请
    • AROMATIC POLYESTER AND MANUFACTURING PROCESS THEREOF
    • 芳香聚酯及其制造方法
    • US20100016539A1
    • 2010-01-21
    • US12374538
    • 2007-07-19
    • Kazuteru KohnoEiji KinoshitaTomoyuki Kishino
    • Kazuteru KohnoEiji KinoshitaTomoyuki Kishino
    • C08G63/12
    • C08J5/18C08G63/189C08G63/672C08G63/78C08J2367/02
    • To provide an aromatic polyester which is formed into a film having excellent heat resistance, color, mechanical properties, dimensional stability and gas barrier properties and a manufacturing process thereof; the aromatic polyester comprises a dicarboxylic acid component and a diol component, wherein (i) the dicarboxylic acid component contains 50 to 100 mol % of a recurring unit represented by the following formula (A): wherein R is an alkylene group having 2 to 10 carbon atoms, (ii) the aromatic polyester has an intrinsic viscosity measured at 35° C. by using a mixed solvent of P-chlorophenol and 1,1,2,2-tetrachloroethane (weight ratio of 40/60) of 0.4 to 3.0; (iii) the aromatic polyester has a content of a recurring unit represented by the following formula (D) of less than 10 mol %: —O—CH2CH2—O—CH2CH2—O—  (D) (iv) the aromatic polyester has a terminal carboxyl group concentration of 200 eq/ton or less; and (v) the aromatic polyester has an alkali metal content of 300 ppm or less.
    • 提供一种形成为具有优异的耐热性,颜色,机械性能,尺寸稳定性和阻气性的薄膜的芳族聚酯及其制造方法; 芳族聚酯包含二羧酸成分和二醇成分,其中(i)二羧酸成分含有50〜100摩尔%的下述式(A)表示的重复单元,式中,R为2〜10的亚烷基 碳原子,(ii)芳族聚酯在35℃下通过使用对氯苯酚和1,1,2,2-四氯乙烷(重量比40/60)的混合溶剂测得的特性粘度为0.4〜3.0 ; (iii)芳族聚酯具有由下式(D)表示的小于10mol%的重复单元的含量:-O-CH 2 CH 2 -O-CH 2 CH 2 -O-(D)(iv)芳族聚酯具有 末端羧基浓度为200当量/吨以下; 和(v)芳族聚酯的碱金属含量为300ppm以下。