    • 4. 发明申请
    • BLENDS OF POLYARYLENE ETHERS AND POLYARYLENE SULFIDES
    • 聚乙烯醚和聚亚烷基硫化物的混合物
    • US20120252962A1
    • 2012-10-04
    • US13515905
    • 2010-12-14
    • Martin WeberChristian MaletzkoSusanne ZeiherMark VölkelNorbert GüntherbergRüdiger Bluhm
    • Martin WeberChristian MaletzkoSusanne ZeiherMark VölkelNorbert GüntherbergRüdiger Bluhm
    • C08L81/06C08L81/04
    • C08L81/06C08G2650/40C08L2205/02C08L81/02C08L71/00
    • The present invention relates to thermoplastic molding materials comprising the following components: (A) at least one polyarylene ether, (B) at least one polyarylene sulfide, (C) at least one functionalized polyarylene ether comprising carboxyl groups having a viscosity number according to DIN EN ISO 1628-1 of 45 to 65 ml/g measured in 1% strength by weight solution in N-methyl-2-pyrrolidone at 25° C., (D) at least one fibrous or particulate filler and (E) optionally further additives and/or processing assistants. In addition, the present invention relates to a process for the preparation of the thermoplastic molding materials according to the invention, the use thereof for the production of shaped articles and the use of functionalized polyarylene ethers comprising carboxyl groups having a viscosity number according to DIN EN ISO 1628-1 of 45 to 65 ml/g measured in 1% strength by weight solution in N-methyl-2-pyrrolidone at 25° C. for increasing the elongation at break and for improving the impact strength.
    • 本发明涉及包含以下组分的热塑性模塑材料:(A)至少一种聚亚芳基醚,(B)至少一种聚芳硫醚,(C)至少一种官能化聚亚芳基醚,其含有根据DIN 在25℃下,在N-甲基-2-吡咯烷酮中的1重量%的重量溶液中测量的EN ISO 1628-1为45至65ml / g,(D)至少一种纤维或颗粒填料和(E)任选进一步 添加剂和/或加工助剂。 此外,本发明涉及一种制备本发明的热塑性成型材料的方法,其用于生产成型制品的用途,以及使用包含羧基的官能化聚亚芳基醚,其粘度值根据DIN EN 在25℃下在1-甲基-2-吡咯烷酮中的1重量%溶液中测量的ISO 1628-1为45至65ml / g,用于增加断裂伸长率和改善冲击强度。
    • 5. 发明申请
    • METHOD FOR PRODUCING A COMPOSITE COMPONENT BY MULTI-COMPONENT INJECTION MOLDING
    • 通过多组分注射成型生产复合组分的方法
    • US20110318524A1
    • 2011-12-29
    • US13141012
    • 2009-12-07
    • Reinhard JakobiJürgen BartlKamil Fischer-JerdonekCecile GibonHarald KrögerSusanne Zeiher
    • Reinhard JakobiJürgen BartlKamil Fischer-JerdonekCecile GibonHarald KrögerSusanne Zeiher
    • B32B5/20B32B27/00B29C33/40
    • B29C45/1671B29C44/086B29C44/18B29C44/3415B29C45/0005B29C45/1676B29K2077/00B29K2105/04B29K2105/12Y10T428/233Y10T428/249992Y10T428/31725
    • The invention relates to processes for the production of a composite component via multicomponent injection molding, where the composite component comprises a main body composed of a thermoplastic A) and an external layer composed of a foamed thermoplastic B), where the main body is produced in a first process step a) via injection molding of the thermoplastic A) and subsequent hardening of the same in an injection mold, and an external layer is injected on to the main body in a second process step b) which follows directly, via injection molding of a mixture comprising the thermoplastic B) and comprising a chemical blowing agent, and the mixture is subsequently hardened in the same injection mold, with somewhat extended cavity, and the external layer injected on to the main body is foamed in a further process step d) via introduction of heat, and the composite component is solidified via cooling in a final process step e), where an essential feature of the invention is that it comprises using, as thermoplastic B) in the mixture used in process step b), at least one polyamide whose modulus of elasticity derived from the tensile test (tensile modulus) Et is from 1 MPa to 250 MPa (determined to DIN EN ISO 527 of April 1996) in the entire temperature range from 70° C. to 180° C., and using, as chemical blowing agent in the mixture used in process step b), one or more substances present in non-polymerized form.The invention further relates to composite components and to reinforced load-bearing elements, where these can be produced by said processes, and also to mixtures, and to the use of said mixtures for the production of composite components.
    • 本发明涉及通过多组分注射成型生产复合部件的方法,其中复合部件包括由热塑性A)构成的主体和由发泡热塑性B)组成的外层,其中主体被制成 第一工艺步骤a)通过注塑成型热塑性塑料A),然后在注模中随后硬化,并且在通过注塑成型的第二工艺步骤b)中将外层注入到主体上 的包含热塑性B)并且包含化学发泡剂的混合物,然后将该混合物在相同的注塑模具中硬化,具有稍微延伸的空腔,并且在另外的工艺步骤d中喷射注入主体的外层 ),并且通过最终工艺步骤e)中的冷却将复合组分固化,其中本发明的基本特征是其包含 在工艺步骤b)中使用的混合物中使用至少一种由拉伸试验(拉伸模量)Et得到的弹性模量为1MPa至250MPa(根据DIN EN ISO 527确定的聚酰胺) 在整个温度范围为70℃至180℃的范围内,并且使用在工艺步骤b)中使用的混合物中的化学发泡剂,以非聚合形式存在的一种或多种物质。 本发明还涉及复合部件和增强的承载元件,其中这些元件可以通过所述方法生产,并且还涉及混合物,以及所述混合物用于生产复合部件的用途。