    • Method for preparing a vehicle interior material
    • 车辆内部材料的制备方法
    • US07923074B2
    • 2011-04-12
    • US12832807
    • 2010-07-08
    • Harukazu OkudaIchiro TaniiNorio NakamuraKazuyuki MatsumuraAkira YamamotoToshiaki Ihara
    • Harukazu OkudaIchiro TaniiNorio NakamuraKazuyuki MatsumuraAkira YamamotoToshiaki Ihara
    • B05D3/00
    • C08K3/32C08K3/016C08K5/31C08K5/34928C08K9/02C09D5/18
    • A method for preparing a vehicle interior material comprises the steps of feeding 100 parts by weight of phosphorus and nitrogen-containing non-halogen flame retardant particles and 0.1 to 20 parts by weight of hydrophobic inorganic oxide fine particles having hydrophobic groups and having an average particle size of 0.001 to 5 μm to a mixer equipped with a high-speed agitation means having a revolution capability of about 100 to 5,000 rpm, agitating and mixing the phosphorus and nitrogen-containing non-halogen flame retardant particles and the hydrophobic inorganic oxide fine particles to produce the phosphorus and nitrogen-containing non-halogen flame retardant particles coated with the hydrophobic inorganic oxide fine particles, mixing 100 parts by weight as solids of a synthetic resin emulsion and 1 to 300 parts by weight of the phosphorus and nitrogen-containing non-halogen flame retardant particles coated with the hydrophobic inorganic oxide fine particles to produce a coating composition, coating the coating composition onto the vehicle interior material, and drying the coated vehicle interior material.
    • 一种制备车辆内部材料的方法包括以下步骤:将100重量份的磷和含氮非卤素阻燃剂颗粒和0.1至20重量份具有疏水基团并具有平均颗粒的疏水性无机氧化物细颗粒 尺寸为0.001〜5μm,配备有具有约100〜5,000rpm的转速的高速搅拌装置的混合机,搅拌并混合含磷的含氮无卤阻燃粒子和疏水性无机氧化物微粒 制备涂覆有疏水性无机氧化物细颗粒的含磷和氮的非卤素阻燃剂颗粒,将100重量份的固体合成合成树脂乳液和1至300重量份的含磷和不含氮的非卤素阻燃剂颗粒混合, - 卤素阻燃颗粒涂覆有疏水性无机氧化物细颗粒以产生涂层c 将涂料组合物涂覆到车辆内部材料上,并干燥涂覆的车辆内部材料。
    • 6. 发明授权
    • Acrylic rubber composition
    • 丙烯酸橡胶组合物
    • US5134170A
    • 1992-07-28
    • US792598
    • 1991-11-15
    • Hiroyuki OhataHarukazu OkudaSatoshi TerasakiMasaharu Takahashi
    • Hiroyuki OhataHarukazu OkudaSatoshi TerasakiMasaharu Takahashi
    • C08L33/04C08J9/10
    • C08J9/10C08J2333/06
    • An acrylic rubber composition is proposed which is improved in respect of the extrusion-moldability as well as the surface slipperiness of the vulcanized article obtained therefrom. The composition comprises (a) an acrylic rubbery cooplymer which is a copolymer of a (meth)acrylic ester and a coolymerizable organosilicon compound having a silicon-bonded vinyl group in a molecule, (b) a reinforcing filler, (c) a powder of spherical particles having a specified average particle diameter and (d) an organic peroxide as a vulcanizing agent. The composition can be compounded further with a blowing agent to give a foamable rubber composition capable of being vulcanized into a spongy rubber body exhibiting excellent feeling on touch and slipperiness in contact with human skin to be useful, for example, as a material of cosmetic puffs.
    • 提出了丙烯酸橡胶组合物,其在挤出成型性以及由其获得的硫化制品的表面光滑性方面得到改进。 该组合物包含(a)丙烯酸橡胶状共聚物,其是分子中具有硅键合乙烯基的(甲基)丙烯酸酯和可共聚有机硅化合物的共聚物,(b)增强填料,(c) 具有指定平均粒径的球形颗粒和(d)作为硫化剂的有机过氧化物。 该组合物可以与发泡剂进一步混合,得到能够硫化成海绵状橡胶体的发泡性橡胶组合物,其表现出良好的触感和与人体皮肤接触的滑爽性,例如可用作化妆气泡的材料 。
    • 7. 发明申请
    • METHOD FOR PREPARING A VEHICLE INTERIOR MATERIAL
    • 制备车辆内部材料的方法
    • US20100272911A1
    • 2010-10-28
    • US12832807
    • 2010-07-08
    • Harukazu OKUDAIchiro TaniiNorio NakamuraKazuyuki MatsumuraAkira YamamotoToshiaki Ihara
    • Harukazu OKUDAIchiro TaniiNorio NakamuraKazuyuki MatsumuraAkira YamamotoToshiaki Ihara
    • B05D3/00
    • C08K3/32C08K3/016C08K5/31C08K5/34928C08K9/02C09D5/18
    • A method for preparing a vehicle interior material comprises the steps of feeding 100 parts by weight of phosphorus and nitrogen-containing non-halogen flame retardant particles and 0.1 to 20 parts by weight of hydrophobic inorganic oxide fine particles having hydrophobic groups and having an average particle size of 0.001 to 5 μm to a mixer equipped with a high-speed agitation means having a revolution capability of about 100 to 5,000 rpm, agitating and mixing the phosphorus and nitrogen-containing non-halogen flame retardant particles and the hydrophobic inorganic oxide fine particles to produce the phosphorus and nitrogen-containing non-halogen flame retardant particles coated with the hydrophobic inorganic oxide fine particles, mixing 100 parts by weight as solids of a synthetic resin emulsion and 1 to 300 parts by weight of the phosphorus and nitrogen-containing non-halogen flame retardant particles coated with the hydrophobic inorganic oxide fine particles to produce a coating composition, coating the coating composition onto the vehicle interior material, and drying the coated vehicle interior material.
    • 一种制备车辆内部材料的方法包括以下步骤:将100重量份的磷和含氮非卤素阻燃剂颗粒和0.1至20重量份具有疏水基团并具有平均颗粒的疏水性无机氧化物细颗粒 尺寸为0.001〜5μm,配备有具有约100〜5,000rpm的转速的高速搅拌装置的混合机,搅拌并混合含磷的含氮无卤阻燃粒子和疏水性无机氧化物微粒 制备涂覆有疏水性无机氧化物细颗粒的含磷和氮的非卤素阻燃剂颗粒,将100重量份的固体合成合成树脂乳液和1至300重量份的含磷和不含氮的非卤素阻燃剂颗粒混合, - 卤素阻燃颗粒涂覆有疏水性无机氧化物细颗粒以产生涂层c 将涂料组合物涂覆到车辆内部材料上,并干燥涂覆的车辆内部材料。
    • 9. 发明授权
    • Crosslinkable copolymer composition and a method for the preparation
thereof
    • 可交联共聚物组合物及其制备方法
    • US4722975A
    • 1988-02-02
    • US800433
    • 1985-11-21
    • Kunio ItohYasuo TarumiTsutomu NakamuraHiroyuki OhataTsutomu MatsuoHarukazu Okuda
    • Kunio ItohYasuo TarumiTsutomu NakamuraHiroyuki OhataTsutomu MatsuoHarukazu Okuda
    • C08F8/42
    • C08F8/42
    • The inventive copolymer composition is satisfactorily curable or vulcanizable into, for example, a rubbery elastomer even by an organic peroxide contained therein as a crosslinking agent. The crosslinkable copolymer comprised therein is a polymer having, in a molecule, at least two monomeric units each having a vinyl-containing organosilicon pendant group represented by the general formula (Vi.sub.m R.sup.1.sub.n SiO).sub.a Vi.sub.b R.sup.2.sub.c Si--, in which Vi is a vinyl group, R.sup.1 is a hydrogen atom or a group selected from the class consisting of monovalent hydrocarbon groups free from aliphatic unsaturation, hydroxy group and hydrolyzable groups excepting halogen atoms, R.sup.2 is a hydrogen atom or a monovalent hydrocarbon group, m is 1, 2 or 3, n is zero, 1 or 2, a is 1, 2 or 3, b is zero, 1 or 2 and c is zero, 1 or 2 with the proviso that a+b=1, 2 or 3 and a+b+c=3. Such a copolymer can be prepared by the copolymerization of a first ordinary ethylenically unsaturated monomer and a second monomer having, simultaneously in a molecule, an ethylenically unsaturated linkage copolymerizable with the first monomer and the vinyl-containing organosilicon group of the above given formula.
    • 本发明的共聚物组合物甚至可以通过其中含有的有机过氧化物作为交联剂令人满意地固化或硫化成例如橡胶弹性体。 包含在其中的可交联共聚物是分子中具有至少两个单体单元的聚合物,每个单体单元具有由通式(VimR1nSiO)aVibR2cSi-表示的含乙烯基的有机硅侧基,其中Vi是乙烯基,R1是 氢原子或选自不含脂肪族不饱和键的一价烃基,羟基和除卤素原子外的可水解基团的基团,R 2为氢原子或一价烃基,m为1,2或3,n为0 ,1或2,a为1,2或3,b为0,1或2,c为0,1或2,条件是a + b = 1,2或3,a + b + c = 3。 这种共聚物可以通过共聚第一普通烯键式不饱和单体和第二单体来制备,该单体在分子中同时具有可与上述给定式的第一单体和含乙烯基的有机硅基团共聚的烯属不饱和键。