    • 1. 发明申请
    • INTERLACED SERIES PARALLEL CONFIGURATION FOR METAL SOLVENT EXTRACTION PLANTS
    • 用于金属溶剂萃取植物的互连系列并行配置
    • WO2004096400A2
    • 2004-11-11
    • PCT/US2004/010706
    • 2004-04-08
    • COGNIS CORPORATIONHEIN, Hans, C.ARAYA, Gabriel
    • HEIN, Hans, C.ARAYA, Gabriel
    • B01D
    • C22B3/0005C22B3/02C22B15/0063C22B23/04Y02P10/234Y02P10/236
    • An interlaced series parallel configuration for the extraction of metal values from an metal value containing aqueous is a special series parallel configuration wherein the stripped organic is first contacted in a second 5 extraction stage with the partially copper depleted aqueous stream exiting from a first extraction stage. This partially loaded organic then advances to a parallel extraction stage where it is contacted with a fresh volume of PLS and extracts additional copper. The organic then advances to the first extraction stage where it contacts a second stream of PLS. This approach 10 results in an overall higher recovery of copper than in the conventional modified series parallel configuration. An increase of 4% overall recovery of copper is achieved relative to that realized with the conventional series parallel . configuration.
    • 用于从含有金属含量的金属值提取金属值的交错串联并联构型是特殊的串联并行配置,其中剥离的有机物在第二个萃取阶段首先与部分贫铜的含水物流从第一提取阶段排出。 然后将该部分负载的有机物进入平行萃取阶段,在其中与新鲜体积的PLS接触并提取另外的铜。 然后有机物前进到其接触第二个PLS流的第一提取阶段。 这种方法10导致铜的总体回收率高于常规改进的串联并联配置。 相对于传统的串联平行实现的,铜的总回收率增加了4%。 组态。
    • 2. 发明申请
    • IMPROVED METHOD FOR METAL HEAP AND DUMP LEACHING COUPLED WITH METAL SOLVENT EXTRACTION
    • 与金属溶剂萃取相结合的金属热浸和浸出浸出的改进方法
    • WO2006041695A3
    • 2006-09-08
    • PCT/US2005034889
    • 2005-09-27
    • COGNIS IP MAN GMBHKORDOSKY GARY ANISBETT ANDREWHEIN HANS C
    • KORDOSKY GARY ANISBETT ANDREWHEIN HANS C
    • C22B15/00B01D11/00C22B19/00C22B23/00
    • C22B19/22C22B3/0005C22B3/04C22B15/0067C22B15/0089Y02P10/234Y02P10/236
    • The disclosed invention provides a process for enhanced recovery of one or more metal values from heap and/or dump leaching of ores containing the metal values, the process comprising: (a) providing a high grade leach solution obtained by heap or dump leaching of fresh high grade ore containing a first metal value; (b) subjecting the high grade leach solution to a first solvent extraction of the first metal value and applying the resulting first aqueous raffinate to leach fresh high grade ore; (c) providing a low grade leach solution obtained by heap or dump leaching of partially leached ore or fresh low grade ore of the first metal value; and (d) subjecting the low grade leach solution to a second solvent extraction of the first metal value, separate from the first solvent extraction of the first metal value, and applying the resulting separate, second aqueous to leach partially leached ore or fresh low grade ore, wherein the first and second aqueous raffinates are not intermixed prior to being applied to their respective ores for leaching. Alternatively, the first and second raffinates may be intermixed prior to being applied to their respective ores for leaching, providing that the aqueous raffinate applied to fresh high grade ore comprises at least 60% by volume of the first aqueous raffinate and the aqueous raffinate applied to partially leached ore or fresh low grade ore comprises at least 60% by volume of the second aqueous raffinate.
    • 所公开的发明提供了一种用于从含有金属值的矿石的堆和/或堆浸浸出中增加一种或多种金属值的回收的方法,所述方法包括:(a)提供通过堆积或堆浸浸出新鲜 含有第一金属价值的高品位矿石; (b)使高品位浸出溶液经第一溶剂萃取第一金属值,并将得到的第一含水萃余液浸出新鲜的高品位矿石; (c)提供通过对第一金属价值的部分浸出的矿石或新鲜低品位矿石进行堆浸或倾倒浸出获得的低品位浸出溶液; 和(d)使低级浸出溶液对第一金属值进行第二溶剂萃取,与第一金属值的第一溶剂萃取分离,并将所得到的分离的第二水溶液浸出部分浸出的矿石或新鲜低级 矿石,其中第一和第二含水残液在施加到它们各自的矿石之前不混合浸出。 或者,第一和第二残液可以在施加到它们各自的矿石之前混合用于浸出,条件是应用于新鲜高品位矿石的含水萃余液包含至少60体积%的第一含水萃余液和施用于 部分浸出的矿石或新鲜的低等级矿石包含至少60体积%的第二含水萃余液。
    • 3. 发明申请
    • IMPROVED METHOD FOR METAL HEAP AND DUMP LEACHING COUPLED WITH METAL SOLVENT EXTRACTION
    • 改进的金属堆浸和金属溶剂萃取耦合的方法
    • WO2006041695A2
    • 2006-04-20
    • PCT/US2005/034889
    • 2005-09-27
    • COGNIS IP MANAGEMENT GMBHKORDOSKY, Gary, A.NISBETT, AndrewHEIN, Hans, C.
    • KORDOSKY, Gary, A.NISBETT, AndrewHEIN, Hans, C.
    • C22B15/00
    • C22B19/22C22B3/0005C22B3/04C22B15/0067C22B15/0089Y02P10/234Y02P10/236
    • The disclosed invention provides a process for enhanced recovery of one or more metal values from heap and/or dump leaching of ores containing the metal values, the process comprising: (a) providing a high grade leach solution obtained by heap or dump leaching of fresh high grade ore containing a first metal value; (b) subjecting the high grade leach solution to a first solvent extraction of the first metal value and applying the resulting first aqueous raffinate to leach fresh high grade ore; (c) providing a low grade leach solution obtained by heap or dump leaching of partially leached ore or fresh low grade ore of the first metal value; and (d) subjecting the low grade leach solution to a second solvent extraction of the first metal value, separate from the first solvent extraction of the first metal value, and applying the resulting separate, second aqueous to leach partially leached ore or fresh low grade ore, wherein the first and second aqueous raffinates are not intermixed prior to being applied to their respective ores for leaching. Alternatively, the first and second raffinates may be intermixed prior to being applied to their respective ores for leaching, providing that the aqueous raffinate applied to fresh high grade ore comprises at least 60% by volume of the first aqueous raffinate and the aqueous raffinate applied to partially leached ore or fresh low grade ore comprises at least 60% by volume of the second aqueous raffinate.
    • 所公开的发明提供了一种用于从含有金属值的矿石的堆积和/或倾倒浸出中强化回收一种或多种金属价值的方法,所述方法包括:(a)提供高品位浸出溶液 通过对含有第一金属价值的新鲜高品位矿石进行堆积或倾倒浸出获得; (b)使高品位浸取溶液经受第一金属值的第一溶剂萃取并施加所得的第一含水萃余液以浸出新鲜的高品位矿石; (c)提供通过堆浸或倾倒浸出部分浸出的矿石或具有第一金属价值的新鲜低品位矿石获得的低品位浸取溶液; 和(d)使低品位浸出溶液进行第一金属值的第二溶剂萃取,与第一金属值的第一溶剂萃取分开,并将所得分离的第二水溶液施用以浸出部分浸出的矿石或新鲜的低品位 矿石,其中第一和第二含水提余液在被施用到它们各自的矿石之前不混合以进行浸出。 或者,第一和第二提余液可以在被施加到它们各自的矿石之前被混合以进行浸出,条件是施加到新鲜高品位矿石的含水提余液包含至少60体积%的第一含水提余液和提供的含水提余液 部分浸出的矿石或新鲜的低品位矿石包含至少60体积%的第二含水提余液。
    • 4. 发明申请
    • INTERLACED SERIES PARALLEL CONFIGURATION FOR METAL SOLVENT EXTRACTION PLANTS
    • 用于金属溶剂萃取植物的互连系列并行配置
    • WO2005108630A1
    • 2005-11-17
    • PCT/US2005/015517
    • 2005-05-04
    • COGNIS CORPORATIONHEIN, Hans, C.ARAYA, Gabriel
    • HEIN, Hans, C.ARAYA, Gabriel
    • C22B15/00
    • C22B23/04C22B3/0005C22B3/02C22B15/0063Y02P10/234Y02P10/236
    • An interlaced series parallel configuration for the extraction of metal values from an metal value containing aqueous is a special series parallel configuration wherein the stripped organic is first contacted in a second extraction stage (E2) with a partially copper depleted aqueous stream exiting from a first extraction stage (E1). This partially loaded organic then advances to a parallel extraction stage (EP) where it is contacted with a fresh volume of PLS and extracts additional copper. The organic then advances to the first extraction stage (E1) where it contacts a second stream of PLS. This approach results in an overall higher recovery of copper than in the conventional modified series parallel configuration. An increase of 4% overall recovery of copper is achieved relative to that realized with the conventional series parallel configuration.
    • 用于从含有金属含量的金属值中提取金属值的交错串联并行配置是特殊的串联并行配置,其中汽提的有机物在第二提取阶段(E2)中首先与部分贫铜的水流从第一提取物 舞台(E1)。 然后将该部分负载的有机物前进到平行萃取阶段(EP),其中其与新鲜体积的PLS接触并提取另外的铜。 然后,有机物进入第一提取阶段(E1),其中它接触第二个PLS流。 这种方法导致铜的总体回收率高于传统的改进型串联配置。 相对于传统的串联并联配置实现的,铜的总回收率增加了4%。